- [32] MICROSTRUCTURAL FEATURES PRODUCED BY THE REDUCTION OF WUSTITE IN H2/H2O GAS-MIXTURES METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1982, 13 (01): : 117 - 124
- [33] THE CORROSION BEHAVIOR OF CO-MO ALLOYS IN H2-H2O-H2S ENVIRONMENTS OXIDATION OF METALS, 1992, 37 (5-6): : 441 - 461
- [34] The solubility of Au in H2O-H2S gas mixtures GEOCHIMICA ET COSMOCHIMICA ACTA, 2008, 72 (12) : A1076 - A1076
- [36] REDUCTION OF SOLID WUSTITE IN H2/H2O/CO/CO2 GAS-MIXTURES METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1990, 21 (01): : 135 - 139
- [38] CORROSION OF FERRITIC STEELS (FE-CR-AL) IN SULFUR VAPOR AND H2S-H2 MIXTURES OXIDATION OF METALS, 1977, 11 (06): : 335 - 354
- [39] DISUSSION OF CONCERNING SULFIDATION OF PURE IRON IN H2/H2S GAS MIXTURES - REPLY METALLURGICAL TRANSACTIONS, 1970, 1 (01): : 300 - &
- [40] Sulphidation of the Fe-40 at% Al alloy in H-2/H2S mixtures at high temperatures MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1997, 48 (05): : 298 - 302