Microstructure and Abrasive Wear Resistance of 18Cr-4Ni-2.5Mo Cast Steel

被引:2
|
作者
Kalandyk, B. [1 ]
机构
[1] AGH Univ Sci & Technol, Fac Foundry Engn, Dept Cast Alloys & Composites Engn, 30 Mickiewicza Av, PL-30059 Krakow, Poland
关键词
Highly alloyed Cr-Ni cast steel; Microstructure; Equivalent Cr and Ni; CCT diagrams; Abrasive wear;
D O I
10.2478/v10266-012-0111-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
An influence of a decreased Cr content on the microstructure of the highly alloyed Cr-Ni cast steel, duplex type, melted under laboratory conditions, was characterized in the paper. The microstructure investigations were performed in the initial state and after the heat treatment (solution annealing) at 1060 degrees C as well as the phase transformation kinetics at continuous cooling was measured. The wear resistance of the investigated cast steel was tested and compared with the 24% Cr-5%Ni-2.5% Mo cast steel. The Cr content decrease, in ferritic-austenitic cast steels (duplex), from 24-26% Cr to 18% leads to the changes of the castings microstructure and eliminating of a brittle sigma phase. In dependence of the casting cooling rate, apart from ferrite and austenite, also fine martensite precipitates occur in the casting structure. It was shown that the investigated cast steel is characterised by a slightly lower wear resistance than the typical cast steel duplex grades.
引用
收藏
页码:81 / 84
页数:4
相关论文
共 50 条
  • [21] Microstructure and abrasive wear resistance of Cr3C2/Ni3Al composite
    Gu, Guo-Rong
    Luo, He-Li
    Li, Shang-Ping
    Liu, Pei-Ying
    Feng, Di
    Hangkong Cailiao Xuebao/Journal of Aeronautical Materials, 2007, 27 (04): : 50 - 53
  • [22] Microstructure and Abrasive Wear Resistance of Deposited Materials of the Ni–Cr–B–Si System with Inclusions of Dispersed Phases
    S. О. Luzan
    А. S. Luzan
    Materials Science, 2020, 56 : 381 - 388
  • [23] Study on the microstructure and wear resistance of laser cladding layer of Ni and Cr on the surface of stainless steel
    Wu, Yunxin
    Wang, Kunlin
    Zhu, Runming
    Zhu, Zhangxiao
    Ding, Lianzhen
    Zhongguo Jiguang/Chinese Journal of Lasers, 1994, 21 (07): : 603 - 608
  • [24] Microstructure, Mechanical Properties, and Abrasive Wear Behaviour of Si-Mn-Cr-B Cast Steel as a Function of Carbon Concentration
    Fu, Hanguang
    Kuang, Jiacai
    Wang, Lintao
    STEEL RESEARCH INTERNATIONAL, 2008, 79 (09) : 721 - 728
  • [25] Influence of microstructure on impact and wear behaviour of sintered Cr and Mo steel
    Molinari, A
    Straffelini, G
    Campestrini, P
    POWDER METALLURGY, 1999, 42 (03) : 235 - 241
  • [26] Development of Cr-Mo-Nb wear-resistant cast steel
    Dai, Duncai
    Lin, Huaitao
    Zhao, Siyong
    Zeng, Yaodong
    Wu, Guoyi
    Chen, Hexing
    Lu, Jincai
    Chang, Zhechuan
    Li, Wei
    Zhuzao/Foundry, 1996, (11): : 11 - 15
  • [27] Effect of TiBAl inoculation on abrasive wear resistance of high Cr white cast iron
    Teker, Tanju
    Yilmaz, S. Osman
    Kerkut, Erhan
    MATERIALS TESTING, 2019, 61 (07) : 690 - 694
  • [28] Effect of Ni on microstructure and wear behaviour of 13Cr-W-Mo-2C white cast iron
    Teker, Tanju
    Yilmaz, S. Osman
    REVISTA DE METALURGIA, 2023, 59 (02)
  • [29] Microstructure and Abrasive Wear Resistance of Deposited Materials of the Ni-Cr-B-Si System with Inclusions of Dispersed Phases
    Luzan, S. O.
    Luzan, A. S.
    MATERIALS SCIENCE, 2020, 56 (03) : 381 - 388
  • [30] Influence of As-Cast Microstructure on the Impact Wear Resistance of 27 mass%Cr Cast Iron
    Ngo Huynh Kinh Luan
    Koizumi, Koreaki
    Mizuno, Kuniaki
    Yamada, Yutaka
    Okuyama, Tetsuya
    MATERIALS TRANSACTIONS, 2019, 60 (11) : 2475 - 2480