Helium embrittlement resistance of Fe-25% Ni-15% Cr austenitic alloys with various MX (M = V, Ti, Nb, Zr; X = C, N) stabilizers was compared through post helium implantation creep testing at 923 K. While significant deterioration by helium in terms of creep rupture time and elongation occurred for all materials investigated, the suppression of the deterioration, especially in rupture time, was discerned for the materials in which semi-coherent MC (M = Ti, Ti + Nb, V + Ti) particles were distributed at high density. The material which contains the incoherent M,C, as predominant precipitates seems to be less degraded by helium than those containing the MXs (M = Zr, V; X = C, N), if compared at the same number density of precipitates. Therefore, it is suggested that the high density dispersion of incoherent M(23)C(6) as well as semi-coherent Ti containing MC particles would be beneficial in reducing the detrimental helium influences on mechanical properties.
引用
收藏
页码:185 / 196
页数:12
相关论文
共 50 条