DEOXIDATION EQUILIBRIUM OF SILICON IN LIQUID NICKEL COPPER AND NICKEL COBALT ALLOYS

被引:12
|
作者
ISHII, F
BANYA, S
机构
[1] Tohoku Univ, Sendai, Japan
关键词
DEOXIDATION EQUILIBRIUM; SI; NI-CU ALLOY; NI-CO ALLOYS; CO; EQUILIBRIUM CONSTANT; DEOXIDATION PRODUCT; INTERACTION PARAMETER; SUPERALLOY;
D O I
10.2355/isijinternational.33.245
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The deoxidation of liquid nickel-copper and nickel-cobalt binary alloys with silicon has been measured at temperatures ranging from 1 450 to 1 650-degrees-C by the use of quartz crucibles. On the nickel basis in nickel-copper binary, the deoxidation product, log K'Si(Ni-Cu), which increased with the addition of copper up to 40 mass% containing 0.5 mass% silicon, was expressed to be: log K'Si(Ni-Cu)=log K(Si(Ni)+0.0342[%Cu]-0.0004[%Cu]2 The effect of temperature on the equilibrium constants of the deoxidation reaction in copper, obtained by the extrapolation, was estimated as follows: log K(Si(Cu)=-15 680/T + 2.16 while log K'Si(Ni-Cu) on the copper basis was given by the expression: log K'Si(Ni-Cu)=log K(Si(Cu)+0.012[%Ni]-0.0001[%Ni]2 up to 40 mass% of nickel. On the nickel basis in nickel-cobalt binary containing 0.55 mass% silicon, log K'Si(Ni-Co) up to 20 mass% of cobalt was represented to be as follows: log K'Si(Ni-Co)=log K(Si(Ni)+0.005[%Co] The temperature dependence of the equilibrium constants at temperatures between 1 550 and 1 650-degrees-C for the deoxidation of pure cobalt was expressed to be: log K'Si(Co)=-15 270/T + 1.81 whereas logK'Si(Ni-Co) on the cobalt basis was found to be: log K'Si(Ni-Co)=log K'Si(Co)-0.001[%Ni] up to 60 mass% of nickel. Using these values of the deoxidation product, the interaction parameters for the effect of these elements on the activity coefficient of oxygen in metals have been established.
引用
收藏
页码:245 / 250
页数:6
相关论文
共 50 条
  • [21] Preparation of pure nickel, cobalt, nickel-cobalt and nickel-copper alloys by hydrothermal reduction
    Li, YD
    Li, LQ
    Liao, HW
    Wang, HR
    JOURNAL OF MATERIALS CHEMISTRY, 1999, 9 (10) : 2675 - 2677
  • [22] STUDY OF DISPERSED PARTICLES IN AGING COPPER-NICKEL-SILICON AND COPPER-COBALT-SILICON ALLOYS
    TEPLITSKII, MD
    NIKOLAEV, AK
    REVINA, NI
    ROZENBERG, VM
    FIZIKA METALLOV I METALLOVEDENIE, 1975, 40 (06): : 1240 - &
  • [23] DEOXIDATION OF IRON NICKEL AND COBALT MELTS
    SAMARIN, AM
    JERNKONTORETS ANNALER, 1967, 151 (03): : 181 - &
  • [24] MAGNETOSTRICTION CONSTANTS OF NICKEL-COPPER AND NICKEL-COBALT ALLOYS
    YAMAMOTO, M
    NAKAMICHI, T
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 1958, 13 (02) : 228 - 229
  • [25] Enthalpies of formation of liquid binary (copper plus iron, cobalt, and nickel) alloys
    Nikolaenko, IV
    Turchanin, MA
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1997, 28 (06): : 1119 - 1130
  • [26] Deoxidation equilibrium of aluminum in liquid cobalt
    Ishihara, I
    Takahashi, K
    Kawaguchi, M
    Ishii, F
    Hino, M
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1997, 61 (10) : 1064 - 1069
  • [27] FORGING COPPER-NICKEL-SILICON ALLOYS
    SCHOCH, H
    METALL, 1984, 38 (04): : 306 - 311
  • [28] MAGNETIC-PROPERTIES OF NICKEL-COPPER AND NICKEL-COBALT ALLOYS
    JILES, DC
    CHANG, TT
    HOUGEN, DR
    RANJAN, R
    JOURNAL DE PHYSIQUE, 1988, 49 (C-8): : 1937 - 1938
  • [29] EQUILIBRIUM SEGREGATION OF SILICON AT GRAIN BOUNDARIES IN NICKEL-IRON-COPPER-MOLYBDENUM ALLOYS
    WALTERS, RES
    ACTA METALLURGICA, 1954, 2 (06): : 890 - &
  • [30] On the magnetisation of nickel, cobalt and of alloys of nickel and cobalt.
    Weiss, P
    Bloch, O
    COMPTES RENDUS HEBDOMADAIRES DES SEANCES DE L ACADEMIE DES SCIENCES, 1911, 153 : 941 - 943