Effect of Air Abrasion and Erbium-Doped Yttrium Aluminum Garnet (Er: YAG) laser preparation on Shear Bond Strength of Composite to Dentin

被引:0
|
作者
Pahlavan, Ayoub [1 ]
Mehmanchi, Mobin [2 ]
Omrani, Ladan Ranjbar [3 ,4 ]
Chiniforush, Nasim [5 ]
机构
[1] Univ Tehran Med Sci, Sch Dent, Dept Operat Dent, Tehran, Iran
[2] Univ Tehran Med Sci, Dent Students Res Ctr, Sch Dent, Tehran, Iran
[3] Univ Tehran Med Sci, Sch Dent, Dept Operat Dent, North Amirabad St, Tehran, Iran
[4] Univ Tehran Med Sci, Dent Res Ctr, Sch Dent, Tehran, Iran
[5] Univ Tehran Med Sci, Laser Res Ctr Dent, Sch Dent, Tehran, Iran
关键词
Er-YAG laser; dental air abrasion; dentin;
D O I
暂无
中图分类号
R8 [特种医学]; R445 [影像诊断学];
学科分类号
1002 ; 100207 ; 1009 ;
摘要
Introduction: The aim of this study was to assess shear bond strength of composite to dentin after air abrasion and laser treatment. Methods: 40 human extracted molars divided into 4 groups (n=10) received the following treatments. Group 1: carbide bur, Group 2: air abrasion with aluminum oxide 50 mu m, Group 3: irradiated with Erbium-Doped Yttrium Aluminum Garnet (Er: YAG) laser (150 mJ/20Hz), Group 4: irradiated with Er: YAG laser (150 mJ/20Hz)+ air. Specimens in all groups were chemically etched with phosphoric acid 37% and treated with bonding agent (single bond 3M). Then, composite build-up was performed by tygon tube. After storage in distilled water at 37 degrees c for one week, all specimens were subjected to a shear bond strength test with universal testing machine. Data were analyzed with ANOVA and T-Test. Results: The mean and standard deviation of shear bond strength of the 4 groups were 20.8 +/- 6.76, 14.98 +/- 3.98, 11.43 +/- 4.36 and 14.95 +/- 3.18 MPa, respectively. Conclusion: Air abrasion after laser treatment improved the shear bond strength.