共 50 条
- [21] THRESHOLD STRESS FOR THE SUPERPLASTIC ELASTIC AFTER-EFFECT IN THE SN-PB EUTECTIC SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (03): : 407 - 409
- [22] Superplastic indentation creep of Sn-Pb-Sb peritectic MATERIALS LETTERS, 2005, 59 (13) : 1705 - 1708
- [23] Indentation creep of lead-free Sn-Bi solder alloys as replacements of Sn-Pb used in microelectronic packaging IEMT 2006: 31ST INTERNATIONAL CONFERENCE ON ELECTRONICS MANUFACTURING AND TECHNOLOGY, 2006, : 443 - +
- [24] Effect of microalloying on the creep strength and microstructure of eutectic Sn-Pb solders CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, 2000, 171-1 : 663 - 667
- [27] Determination of supercooling and latent heat of Sn-Pb and Sn-Zn alloys Metallic Materials (English translation of Kovove Materialy) (Cambridge, Engl), 1991, 29 (02): : 87 - 93
- [30] The columnar to equiaxed transition during solidification of Sn-Pb alloys Journal of Alloys and Compounds, 2003, 351 (1-2): : 126 - 134