共 50 条
- [41] REACTIONS BETWEEN LOW ALLOYED STEEL AND INITIALLY PURE AS WELL AS IRON-SATURATED ALUMINUM MELTS BETWEEN 670 AND 800-DEGREES-C ZEITSCHRIFT FUR METALLKUNDE, 1986, 77 (04): : 239 - 244
- [42] DECOMPOSITION OF AN FE-CR 38-WT-PERCENT CHROMIUM STAINLESS-STEEL AT 475-DEGREES-C HYPERFINE INTERACTIONS, 1994, 94 (1-4): : 2355 - 2360
- [45] EFFECT OF ALLOYING ELEMENTS ON THE 1ST STEPS OF OXIDATION OF A LOW-ALLOY STEEL BETWEEN 600 AND 800-DEGREES-C REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 1994, 91 (12): : 1805 - 1813
- [46] HIGH TEMPERATURE OXIDATION OF NI-CR OR MODIFIED NI-CR ALLOYS AT 1 ATMOSPHERE OF OXYGEN BETWEEN 800 DEGREES AND 1300 DEGREES C. TIDSSKRIFT FOR KJEMI BERGVESENOG METALLURGI, 1969, 29 (12): : 215 - &
- [48] CARBIDE FORMATION IN A LOW-FERRITE AUSTENITIC STAINLESS-STEEL WELD METAL AT 649-DEGREES-C METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (01): : 173 - 174
- [49] CREEP-FATIGUE DAMAGE IN 316-L AUSTENITIC STAINLESS-STEEL AT 600-DEGREES-C ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 1981, 6 (02): : 197 - 208