Impact-sliding fretting tribocorrosion behavior of 316L stainless steel in solution with different halide concentrations

被引:0
|
作者
Xu Ma
Wei Tan
Remy Bonzom
Xue Mi
Guorui Zhu
机构
[1] Tianjin University,School of Chemical Engineering and Technology
[2] Zhejiang Institute of Tianjin University,Materials and Mechanics of Components Department
[3] Electricité de France R&D,undefined
[4] Nuclear Power Institute of China,undefined
来源
Friction | 2023年 / 11卷
关键词
impact-sliding; fretting wear; tribocorrosion; halide concentration; 316L stainless steel;
D O I
暂无
中图分类号
学科分类号
摘要
Impact-sliding caused by random vibrations between tubes and supports can affect the operation of heat exchangers. In addition, a corrosive environment can cause damage, accelerating the synergism of corrosion and wear. Therefore, the focus of this work was the impact-sliding fretting tribocorrosion behavior of 316L heat exchanger tubes at different halide concentrations. A device system incorporating the in situ electrochemical measurements of impact-sliding fretting corrosion wear was constructed, and experiments on 316L heat exchanger tubes in sodium chloride (NaCl) solution with different concentrations (0.0, 0.1, 0.5, 1.0, 3.5, and 5.0 wt%) were carried out. The synergism between wear and corrosion was also calculated and analyzed. The wear and damage mechanisms were elucidated by correlating the corrosion-wear synergism, morphologies, and material loss rates. The results indicated that the stable wear stage occurred at approximately 9–12 h, after which the corrosion current increased with the expansion of the wear area. As the halide concentration increased, the scale of damage on the wear scars gradually decreased, changing from being dominated by cracks, delaminations, and grooves to being dominated by scratches, microgrooves, and holes. There was an obvious positive synergism between wear and corrosion. The material loss was dominated by pure mechanical wear and wear enhanced by corrosion, but corrosion enhanced by wear contributed more than tangential sliding fretting corrosion. The total mass loss increased gradually in the range of 0.0–0.5 wt% and decreased in the range of 0.5–5.0 wt%. Large-scale damage enhanced by corrosivity and small-scale damage reduced by lubricity dominated the material loss at low and high concentrations, respectively.
引用
收藏
页码:2310 / 2328
页数:18
相关论文
共 50 条
  • [21] Accelerated deterioration mechanism of 316L stainless steel in NaCl solution under the intermittent tribocorrosion process
    Liu, Yingrui
    Liu, Linlin
    Li, Shuyu
    Wang, Rujia
    Guo, Peng
    Wang, Aiying
    Ke, Peiling
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 121 : 67 - 79
  • [22] Accelerated deterioration mechanism of 316L stainless steel in NaCl solution under the intermittent tribocorrosion process
    Yingrui Liu
    Linlin Liu
    Shuyu Li
    Rujia Wang
    Peng Guo
    Aiying Wang
    Peiling Ke
    Journal of Materials Science & Technology, 2022, 121 (26) : 67 - 79
  • [23] Accelerated deterioration mechanism of 316L stainless steel in NaCl solution under the intermittent tribocorrosion process
    Liu, Yingrui
    Liu, Linlin
    Li, Shuyu
    Wang, Rujia
    Guo, Peng
    Wang, Aiying
    Ke, Peiling
    Journal of Materials Science and Technology, 2022, 121 : 67 - 79
  • [24] Effect of applied potential on the fretting corrosion-wear behavior of 316L stainless steel
    Yan, J.Z.
    Wu, Y.S.
    Li, J.Q.
    Zhang, L.
    Mocaxue Xuebao/Tribology, 2001, 21 (01): : 19 - 23
  • [25] Corrosion Behavior of Eutectic Molten Salt solution on Stainless Steel 316L
    Subari, Fuzieah
    Maksom, Hafizul Faiz
    Zawawi, Aiman
    WORLD CONFERENCE ON TECHNOLOGY, INNOVATION AND ENTREPRENEURSHIP, 2015, : 2699 - 2708
  • [26] Cavitation Erosion Behavior of 316L Stainless Steel
    Guiyan Gao
    Zheng Zhang
    Tribology Letters, 2019, 67
  • [27] The mechanochemical behavior of type 316L stainless steel
    Gutman, EM
    Solovioff, G
    Eliezer, D
    CORROSION SCIENCE, 1996, 38 (07) : 1141 - 1145
  • [28] THE BEHAVIOR OF 316L STAINLESS-STEEL IN HYDROGEN
    ELIEZER, D
    JOURNAL OF MATERIALS SCIENCE, 1984, 19 (05) : 1540 - 1547
  • [29] Cavitation Erosion Behavior of 316L Stainless Steel
    Gao, Guiyan
    Zhang, Zheng
    TRIBOLOGY LETTERS, 2019, 67 (04)
  • [30] Tribocorrosion behaviour of low temperature plasma carburised 316L stainless steel in 0.5 M NaCl solution
    Sun, Y.