Directional solidification casting technology of heavy-duty gas turbine blade with liquid metal cooling (LMC) process

被引:0
|
作者
Xiao-fu Liu
Yan-chun Lou
Bo Yu
Gui-qiao Su
Chang-chun Li
Xin-li Guo
Biao Li
Guo-yan Shui
机构
[1] Shenyang Research Institute of Foundry Co.,State Key Laboratory of Light Alloy Casting Technology for High
[2] Ltd.,end Equipment
来源
China Foundry | 2019年 / 16卷
关键词
liquid metal cooling (LMC); heavy-duty gas turbine; large-size blade; directional solidification; microstructure; TG132.3; 3; A;
D O I
暂无
中图分类号
学科分类号
摘要
In this work, some important factors such as ceramic shell strength, heat preservation temperature, standing time and withdrawal rate, which influence the formability of directionally solidified large-size blades of heavy-duty gas turbine with the liquid metal cooling (LMC) process, were studied through the method of microstructure analysis combining. The results show that the ceramic shell with medium strength (the high temperature flexural strength is 8 MPa, the flexural strength after thermal shock resistance is 12 MPa and the residual flexural strength is 20 MPa) can prevent the rupture and runout of the blade. The appropriate temperature (1,520 °C for upper region and 1,500 °C for lower region) of the heating furnace can eliminate the wide-angle grain boundary, the deviation of grain and the run-out caused by the shell crack. The holding time after pouring (3-5 min) can promote the growth of competitive grains and avoid a great deviation of columnar grains along the crystal orientation <001>, resulting in a straight and uniform grain structure. In addition, to avoid the formation of wrinkles and to ensure a smooth blade surface, the withdrawal rate should be no greater than the growth rate of grain. It is also found that the dendritic space of the blade decreases with the rise of solidification rate, and increases with the enlarging distance between the solidification position and the chill plate.