Role of microstructural degradation in the heat-affected zone of 2.25Cr-1Mo steel weldments on subscale features during steam oxidation and their role in weld failures

被引:0
|
作者
R. K. Singh Raman
机构
[1] Royal Melbourne Institute of Technology (RMIT),the Department of Communication and Electronic Engineering
关键词
Material Transaction; Base Metal; Weld Metal; Oxide Scale; Alloy Matrix;
D O I
暂无
中图分类号
学科分类号
摘要
Microstructural degradations in the base metal adjacent to the weld pool, i.e., the heat-affected zone (HAZ), caused during welding of 2.25Cr-1Mo steel, were characterized by electron and optical microscopy of different regions of the weldments. In order to study the influence of the microstructural degradations on scaling kinetics in steam and the resulting subscale features, samples of the base metal, the HAZ, and weld metal specimens were extracted from the weldment and oxidized in an environment of 35 pct steam+nitrogen at 873 K for 10 hours. Oxide scales formed in the three regions and the underlying subscales were characterized using scanning electron microscopy (SEM) and electron probe microanalysis (EPMA). Influence of the “free” chromium content in the three weldment regions on protective scale formation and on the subscale features has been investigated. As the principal achievement, this study has clearly shown the occurrence of oxidation-induced void formation in the subscale zone and grain boundary cavitation in the neighboring area during steam oxidation of the HAZ. This article also discusses the possible role of oxidation-induced void formation and grain boundary cavitation in the inferior service life of welds in 2.25Cr-1Mo steel components.
引用
收藏
页码:577 / 586
页数:9
相关论文
共 50 条
  • [41] Acoustic emission studies during the high temperature oxidation of 2.25Cr-1Mo steel at 1173 K
    Jha, B. B.
    Mishra, B. K.
    Mohapatra, B. K.
    Ojha, S. N.
    MATERIALS AT HIGH TEMPERATURES, 2011, 27 (04) : 301 - 311
  • [42] On the Heat-Affected Zone Role for Mechanical Properties of Structural-Steel MIG and CMT-MIG Weldments
    Khajuria, Akhil
    Misra, Anurag
    Shiva, S.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2024, 77 (11) : 3905 - 3913
  • [43] Role of gaseous environment and secondary precipitation in microstructural degradation of Cr-Mo steel weldments at high temperatures
    R. K. Singh Raman
    Metallurgical and Materials Transactions A, 1999, 30 : 2103 - 2113
  • [44] Role of gaseous environment and secondary precipitation in microstructural degradation of Cr-Mo steel weldments at high temperatures
    Raman, RKS
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1999, 30 (08): : 2103 - 2113
  • [45] Evaluation of Post-Weld Heat-Treated 2.25Cr-1Mo Steel Joint Behaviors by Electromagnetic NDE Parameters
    Roy, Rajat K.
    Murugaiyan, Premkumar
    Panda, Ashis K.
    JOURNAL OF SUPERCONDUCTIVITY AND NOVEL MAGNETISM, 2024, 37 (8-10) : 1677 - 1687
  • [46] COMBINED EFFECTS OF POST-WELD HEAT-TREATMENT AND AGING ON ALLOY 800/2.25CR-1MO STEEL JOINT
    BHADURI, AK
    VENKADESAN, S
    RODRIGUEZ, P
    MUKUNDA, PG
    MATERIALS SCIENCE AND TECHNOLOGY, 1991, 7 (11) : 1051 - 1056
  • [47] Characterization of Microstructures across the Heat-Affected Zone of the Modified 9Cr-1Mo Weld Joint to Understand Its Role in Promoting Type IV Cracking
    K. LAHA
    K.S. CHANDRAVATHI
    P. PARAMESWARAN
    K. BHANU SANKARA RAO
    S.L. MANNAN
    Metallurgical and Materials Transactions A, 2007, 38 : 58 - 68
  • [48] Characterization of microstructures across the heat-affected zone of the modified 9Cr-1 Mo weld joint to understand its role in promoting type IV cracking
    Laha, K.
    Chandravathi, K. S.
    Parameswaran, P.
    Rao, K. Bhanu Sankara
    Mannan, S. L.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (01): : 58 - 68
  • [49] Thermal simulation experiments of welding heat affected zone of 2.25Cr-1Mo-0.25V heat resistance steel
    Key Laboratory of Metastable Materials Science and Technology, College of Materials Science and Engineering, Yanshan University, Qinhuangdao 066004, China
    不详
    Cailiao Rechuli Xuebao, 2007, 1 (66-70+74):
  • [50] Finite element analysis of residual stress in 2.25Cr-1Mo steel pipe during welding and heat treatment process
    Ren, Sendong
    Li, Suo
    Wang, Yifeng
    Deng, Dean
    Ma, Ninshu
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 47 (110-118) : 110 - 118