Thermal Parameters, Microstructure, and Mechanical Properties of Directionally Solidified Sn-0.7 wt.%Cu Solder Alloys Containing 0 ppm to 1000 ppm Ni

被引:0
|
作者
Bismarck Luiz Silva
Noé Cheung
Amauri Garcia
José Eduardo Spinelli
机构
[1] Federal University of São Carlos—UFSCar,Department of Materials Engineering
[2] Federal Institute of Education,Department of Materials Engineering
[3] Science and Technology of São Paulo—IFSP,undefined
[4] University of Campinas—UNICAMP,undefined
来源
关键词
Solidification; microstructure; thermal parameters; mechanical properties; solder alloys;
D O I
暂无
中图分类号
学科分类号
摘要
Environmental concerns over the toxicity of Pb are resulting in the progressive ban of Pb-based solders as part of electrical and electronic devices. Sn-Cu alloys are becoming interesting Pb-free solder alternatives. In the case of hypoeutectic Sn-Cu alloys (<0.7 wt.% Cu), small alloying additions of Ni can prevent the growth of coarse and deleterious Cu6Sn5 particles. Solidification thermal parameters such as the growth rate, cooling rate, and interfacial heat transfer coefficient (hi) determine the morphology and scale of the phases forming the resulting microstructure. In the present study, directional solidification experiments were carried out with Sn-0.7 wt.%Cu, Sn-0.7 wt.% Cu-0.05 wt.%Ni, and Sn-0.7 wt.%Cu-0.1 wt.%Ni alloys and interrelations of solidification thermal parameters, microstructure, and tensile properties have been established. The highest time-dependent hi profile was found for the Sn-0.7 wt.%Cu-0.1 wt.%Ni alloy, which is an indication that this alloy has the highest fluidity. Constrained dendritic arrangements were observed for all alloys experimentally examined. This morphology has been associated with high cooling rates and growth rates. Cellular regions, characterized by aligned eutectic colonies, were also observed to occur for cooling rates lower than 0.9 K/s and 6.0 K/s for the unmodified Sn-0.7 wt.%Cu alloy and for both Ni-modified Sn-Cu alloys, respectively. Experimental Hall–Petch-type equations correlating the ultimate tensile strength and elongation with cell/dendritic spacings are proposed.
引用
收藏
页码:179 / 191
页数:12
相关论文
共 50 条
  • [31] The effectiveness of Ni microalloying on the microstructure and mechanical properties of low temperature In-35 wt%Sn/Cu solder joint
    Chang, M. S.
    Salleh, M. A. A. Mohd
    Somidin, F.
    Halin, D. S. C.
    Yasuda, H.
    Nogita, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 882
  • [32] Effects of antimony on the microstructure, thermal properties, mechanical performance, and interfacial behavior of Sn–0.7Cu–0.05Ni–xSb/Cu solder joints
    Suchart Chantaramanee
    Phairote Sungkhaphaitoon
    Journal of Materials Science: Materials in Electronics, 2021, 32 : 27607 - 27624
  • [33] Interfacial Microstructure and Mechanical Properties of Sn2.5Ag0.7Cu0.1RE0.05Ni/Cu Solder Joint under Thermal Shock
    Zhang Keke
    Guo Xingdong
    Wang Huigai
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (05) : 1353 - 1358
  • [34] Effect of 0.05 wt.% Pr Addition on Microstructure and Shear Strength of Sn-0.3Ag-0.7Cu/Cu Solder Joint during the Thermal Aging Process
    Wu, Jie
    Xue, Songbai
    Wang, Jingwen
    Huang, Guoqiang
    APPLIED SCIENCES-BASEL, 2019, 9 (17):
  • [35] Influence of 0.05 wt% Pr addition on interfacial microstructure and mechanical properties of Sn–0.3Ag–0.7Cu/Cu solder joint during thermal shocking
    Peng Zhang
    Songbai Xue
    Cheng Qian
    Jianhao Wang
    Lu Liu
    Jie Wu
    Journal of Materials Science: Materials in Electronics, 2022, 33 : 7099 - 7108
  • [36] Microstructure and mechanical properties of rapidly solidified Al-20Si-xFe-3Cu-lMg (x=0 and 5 wt.%) Extradates
    T. S. Kim
    K. H. Kim
    W. T. Kim
    C. W. Won
    S. S. Cho
    B. S. Chun
    Metals and Materials, 1998, 4 : 1163 - 1169
  • [37] The bulk alloy microstructure and tensile properties of Sn-1Ag-0.5Cu-xAl lead-free solder alloys (x=0, 1, 1.5 and 2 wt.%)
    Shnawah, Dhafer Abdul-Ameer
    Sabri, Mohd Faizul Mohd
    Badruddin, Irfan Anjum
    Che, Fa Xing
    MICROELECTRONICS INTERNATIONAL, 2012, 29 (02) : 108 - 116
  • [38] Evolution of microstructure, thermal and creep properties of Ni-doped Sn-0.5Ag-0.7Cu low-Ag solder alloys for electronic applications
    Hammad, A. E.
    MATERIALS & DESIGN, 2013, 52 : 663 - 670
  • [39] Microstructure and mechanical properties of rapidly solidified Al-20Si-xFe-3Cu-1Mg (x=0 and 5 wt.%) extrudates
    Kim, T.S.
    Kim, K.H.
    Kim, W.T.
    Won, C.W.
    Cho, S.S.
    Chun, B.S.
    Metals and Materials International, 1998, 4 (06): : 1163 - 1169
  • [40] Microstructure and mechanical properties of rapidly solidified Al-20Si-xFe-3Cu-1Mg (x=0 and 5 wt.%) extrudates
    Kim, TS
    Kim, KH
    Kim, WT
    Won, CW
    Cho, SS
    Chun, BS
    METALS AND MATERIALS-KOREA, 1998, 4 (06): : 1163 - 1169