Effect of shot peening on microstructure, nanocrystallization and microhardness of Ti–10V–2Fe–3Al alloy surface

被引:0
|
作者
Hai-zhong Zheng
Sheng-hua Guo
Qin-hao Luo
Xiao-yong Shu
Gui-fa Li
机构
[1] Nanchang Hangkong University,National Defense Key Disciplines Laboratory of Light Alloy Processing Science and Technology
关键词
Ti–10V–2Fe–3Al alloy; Shot peening treatment; Surface nanocrystallization; Martensitic transformation; Microhardness;
D O I
暂无
中图分类号
学科分类号
摘要
Severe plastic deformation of Ti–10V–2Fe–3Al alloy in the surface region was caused by shot peening at air pressure of 0.6 MPa with processing time ranging from 1 to 45 min. The results showed that the thickness of surface deformation layer was proportional to the processing time, the microhardness of the shot-peened surface increased from 280 to 385 HV, and the depth of highly hardening layers arrived at 200 μm. It was worth noting that a grain size gradient from nanocrystalline on the surface toward coarse grain in the matrix was obtained during the shot peening process and the minimum grain size in the top surface after shot peening was about 100–200 nm.
引用
收藏
页码:52 / 58
页数:6
相关论文
共 50 条
  • [41] EFFECT OF β-FLECKS ON MECHANICAL PROPERTIES OF Ti-10V-2Fe-3Al ALLOY
    ZHOU Yigang YU Hanqing ZENG Weidong Northwestern Polytechnical University
    Acta Metallurgica Sinica(English Edition), 1993, (03) : 197 - 201
  • [42] EFFECT OF THE SHOT PEENING ON SURFACE PROPERTIES OF Ti-6Al-4V ALLOY PRODUCED BY MEANS OF DMLS TECHNOLOGY
    Zebrowski, Remigiusz
    Walczak, Mariusz
    Klepka, Tomasz
    Pasierbiewicz, Kamil
    EKSPLOATACJA I NIEZAWODNOSC-MAINTENANCE AND RELIABILITY, 2019, 21 (01): : 46 - 53
  • [43] Effect of ultrasonic shot peening on LCF behavior of the Ti-6Al-4V alloy
    Kumar, Sanjeev
    Chattopadhyay, K.
    Singh, Vakil
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 724 : 187 - 197
  • [44] Effect of cryogenic quenching on microstructure and microhardness of Ti-6Al-4V alloy
    Shukla, Shashank
    Bajpai, Vivek
    MATERIALS LETTERS, 2020, 267
  • [45] Influence of hot rolling deformation on microstructure and properties of Ti-10V-2Fe-3Al alloy
    Shang, Guo-Qiang
    Zhu, Zhi-Shou
    Kou, Hong-Chao
    Wang, Xin-Nan
    Fei, Yue
    Chang, Hui
    Li, Jin-Shan
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2013, 34 (03): : 108 - 113
  • [46] AN INFLUENCE OF TITANIUM ALLOY Ti10V2Fe3Al MICROSTRUCTURE ON THE ELECTRODISCHARGE PROCESS EFFICIENCY
    Zyra, A.
    Bogucki, R.
    Skoczypiec, S.
    ARCHIVES OF METALLURGY AND MATERIALS, 2019, 64 (03) : 1005 - 1010
  • [47] Microstructural evolution in the surface of Ti-10V-2Fe-3Al alloy by solution treatments
    Lichun Qi
    Xaichao Zhang
    Xueliang Qiao
    Lijun Huang
    Xu Huang
    Xinqing Zhao
    Progress in Natural Science:Materials International, 2020, 30 (01) : 106 - 109
  • [48] Influence of aging processing on microstructure and mechanical properties of ti-10v-2fe-3al alloy
    Shang, Guoqiang
    Kou, Hongchao
    Fei, Yue
    Chang, Hui
    Zhu, Zhishou
    Wang, Xinnan
    Zhang, Fengshou
    Li, Jinshan
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2010, 39 (06): : 1061 - 1065
  • [49] MICROSTRUCTURE REFINEMENT OF TI-10V-2FE-3AL ALLOY BY LOW-TEMPERATURE EXTRUSION
    MAHAJAN, YR
    MARTORELL, IA
    EYLON, D
    BRODERICK, TF
    FROES, FH
    JOURNAL OF METALS, 1984, 36 (12): : 56 - 56
  • [50] Microstructural evolution in the surface of Ti-10V-2Fe-3Al alloy by solution treatments
    Qi, Lichun
    Zhang, Kaichao
    Qiao, Xueliang
    Huang, Lijun
    Huang, Xu
    Zhao, Xinqing
    PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2020, 30 (01) : 106 - 109