Gallium-Suboxide Attack of Stainless Steel and Nickel Alloys at 800–1200°C

被引:1
|
作者
D. G. Kolman
T. N. Taylor
Y. S. Park
M. Stan
D. P. Butt
C. J. Maggiore
J. R. Tesmer
G. J. Havrilla
机构
[1] Los Alamos National Laboratory,
来源
Oxidation of Metals | 2001年 / 55卷
关键词
gallium oxide; gallium suboxide; 304 stainless steel; 316 stainless steel; Hastelloy C-276;
D O I
暂无
中图分类号
学科分类号
摘要
Failure of furnace parts composed of stainless steel or nickel-base alloys has been observed following treatment of gallium-containing compounds at 800 to 1200°C. This work examines the effect of gallium suboxide (Ga2O) and gallium oxide (Ga2O3) on the chemical and mechanical properties of 304 SS, 316 SS, and Hastelloy C-276 in an effort to elucidate a failure mechanism. Results indicate that all three materials are subject to attack by gallium compounds. Elemental segregation, oxidation, and Ga uptake all occur following exposure. Ga2O gas appears to play the dominant role in alloy attack under reducing conditions. Increasing temperature is shown to increase the magnitude of attack, as measured by oxide thickness and gallium-metal uptake. Calculations of the system thermodynamics suggest that Cr, Mn, Si, and V alloying components are responsible for metal oxidation and concurrent gallium absorption. A homogeneous, large (>30 wt.%) gallium uptake resulted in brittle failure of 304 SS. Therefore, exposure to gallium compounds can result in premature failure of iron- and nickel-base structural alloys.
引用
收藏
页码:437 / 470
页数:33
相关论文
共 50 条
  • [1] Gallium-suboxide attack of stainless steel and nickel alloys at 800-1200°C
    Kolman, DG
    Taylor, TN
    Park, YS
    Stan, M
    Butt, DP
    Maggiore, CJ
    Tesmer, JR
    Havrilla, GJ
    OXIDATION OF METALS, 2001, 55 (5-6): : 437 - 470
  • [2] Gallium suboxide vapor attack of chromium, cobalt, molybdenum, tungsten, and their alloys at 1200°C
    Kolman, DG
    Taylor, TN
    Park, YS
    Stan, M
    Butt, DP
    Maggiore, CJ
    Tesmer, JR
    Havrilla, GJ
    OXIDATION OF METALS, 2001, 56 (3-4): : 347 - 374
  • [3] Gallium Suboxide Vapor Attack of Chromium, Cobalt, Molybdenum, Tungsten, and Their Alloys at 1200°C
    D. G. Kolman
    T. N. Taylor
    Y. S. Park
    M. Stan
    D. P. Butt
    C. J. Maggiore
    J. R. Tesmer
    G. J. Havrilla
    Oxidation of Metals, 2001, 56 : 347 - 374
  • [4] Environmentally-assisted cracking of 316 L stainless steel exposed to gallium suboxide
    Kolman, DG
    Havrilla, GJ
    CHEMISTRY AND ELECTROCHEMISTRY OF CORROSION AND STRESS CORROSION CRACKING: A SYMPOSIUM HONORING THE CONTRIBUTIONS OF R.W. STAEHLE, 2001, : 635 - 648
  • [5] CHARACTERISTIC SCALES ON PURE NICKEL-CHROMIUM ALLOYS AT 800 DEGREES-1200 DEGREES C
    WOOD, GC
    HODGKIESS, T
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1966, 113 (04) : 319 - +
  • [6] Tensile tests on stainless steels in temperature range 800 to 1200 °C
    Tehovnik, F.
    Arzensek, B.
    Arh, B.
    METALURGIJA, 2008, 47 (02): : 75 - 79
  • [7] Materials of Construction: Stainless Steel Versus Nickel Alloys
    Signorelli, Rodrigo
    Li, Jan
    Chemical Engineering (United States), 2022, 129 (07): : 31 - 36
  • [8] STRIP CLADDING OF STEEL WITH STAINLESS AND NICKEL BASED ALLOYS
    HORSFIELD, AM
    ALMQVIST, G
    ROSENDAH.CH
    BRITISH WELDING JOURNAL, 1966, 13 (05): : 315 - +
  • [9] Fume generation rates for stainless steel, nickel and aluminum alloys
    Castner, HR
    WELDING JOURNAL, 1996, 75 (12) : S393 - S401
  • [10] On the α+γ⇆γ-phase boundary in nickel and in manganese containing stainless steel alloys
    Schüle, W
    EFFECTS OF RADIATION ON MATERIALS: 20TH INTERNATIONAL SYMPOSIUM, 2001, 1045 : 704 - 721