Effect of Cr Content on Microstructure and Growth of External Al2O3 Scale Formed on Fe–Cr–Al Alloys

被引:0
|
作者
Suzue Yoneda
Shigenari Hayashi
机构
[1] Tokyo Institute of Technology,Department of Metallurgy and Ceramics Science, Graduate School of Science and Engineering
[2] Hokkaido University,Division of Materials Science and Engineering, Faculty of Engineering
来源
Oxidation of Metals | 2022年 / 97卷
关键词
Al; O; scale; Microstructure; Fe–Cr–Al alloy;
D O I
暂无
中图分类号
学科分类号
摘要
The effect of Cr on the microstructure and growth of Al2O3 scale that forms on Fe–4Cr–6Al and Fe–24Cr–6Al alloys during long-term oxidation at 1000 °C was investigated. The Al2O3 scale that formed on both alloys consisted of a duplex layer comprising columnar grains. The grain size of Al2O3 scale was found to be smaller for the Fe–24Cr–6Al alloy. The smaller grain size of Al2O3 scale formed on the alloy with higher Cr content was inferred to be due to the formation of an initial transient Cr-rich oxide scale with finer grain structure for the outer layer, and that a higher number density of internal Al2O3 precipitates formed during the initial stage of oxidation for the inner layer in the alloy with higher Cr content. The columnar grains grew larger laterally accompanying the growth of both the outer and inner layers at the gas/scale and scale/substrate interface during the steady-state oxidation period. Differences in the growth rate of Al2O3 scale formed on Fe–4Cr–6Al and Fe–24Cr–6Al can be explained by differences in the Al2O3-scale grain size, which indicates that the initial transient oxidation behavior strongly affects the microstructure and, therefore, the growth rate of Al2O3 scale.
引用
收藏
页码:195 / 208
页数:13
相关论文
共 50 条
  • [31] THE EFFECT OF AN AL2O3 DISPERSION ON THE ADHESION OF AL2O3 SCALES ON ALUMINIZED CO-10-DEGREES CR ALLOYS
    KINGSLEY, LM
    STRINGER, J
    OXIDATION OF METALS, 1989, 32 (5-6): : 371 - 378
  • [32] The Effects of Al2O3 Amount on the Microstructure and Properties of Fe-Cr Matrix Composites
    Shamsuddin, Saidatulakmar
    Jamaludin, Shamsul Baharin
    Hussain, Zuhailawati
    Ahmad, Zainal Arifin
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (13): : 3452 - 3457
  • [33] The Effects of Al2O3 Amount on the Microstructure and Properties of Fe-Cr Matrix Composites
    Saidatulakmar Shamsuddin
    Shamsul Baharin Jamaludin
    Zuhailawati Hussain
    Zainal Arifin Ahmad
    Metallurgical and Materials Transactions A, 2010, 41 : 3452 - 3457
  • [34] On the in situ synthesis of (Fe,Cr)Al and (Fe,Cr)Al-Al2O3 nanostructured materials
    Sourani, F.
    Enayati, M. H.
    Ngan, A. H. W.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [35] Effects of Cr2O3 Content on Microstructure and Mechanical Properties of Al2O3 Matrix Composites
    Cui, Kunkun
    Zhang, Yingyi
    Fu, Tao
    Hussain, Shahid
    Saad Algarni, Tahani
    Wang, Jie
    Zhang, Xu
    Ali, Shafaqat
    COATINGS, 2021, 11 (02) : 1 - 17
  • [36] Effect of Al2O3 content on the viscosity and structure of CaO–SiO2–Cr2O3–Al2O3 slags
    Fang Yuan
    Zheng Zhao
    Yanling Zhang
    Tuo Wu
    InternationalJournalofMinerals,MetallurgyandMaterials, 2022, (08) : 1522 - 1531
  • [37] Effect of Al2O3 Content in Top Slag on Cleanness of Stainless Steel Fe-13Cr
    Wang, Qi
    Wang, Lijun
    Chou, Kuochih
    ADVANCES IN MOLTEN SLAGS, FLUXES, AND SALTS, 2016, : 155 - 163
  • [38] The Transition from Transient Oxide to Protective Al2O3 Scale on Fe-Cr-Al Alloys During Heating to 1000 A°C
    Yoneda, Suzue
    Hayashi, Shigenari
    Ukai, Shigeharu
    OXIDATION OF METALS, 2018, 89 (1-2): : 81 - 97
  • [39] Measuring adhesion of Cr2O3 and Al2O3 scales on Fe-based alloys
    Galerie, A
    Toscan, F
    N'Dah, E
    Przybylski, K
    Wouters, Y
    Dupeux, M
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 631 - 638
  • [40] ADHESION STUDIES OF CU-CR ALLOYS ON AL2O3
    CHAN, CJ
    CHANG, CA
    FARRELL, CE
    SCHROTT, AG
    APPLIED PHYSICS LETTERS, 1993, 62 (06) : 654 - 656