High-Temperature Phases in the Fe–Mo–Cr–C System

被引:0
|
作者
T. A. Velikanova
A. M. Zaslavskii
M. V. Kindrachuk
机构
[1] National Academy of Sciences of Ukraine,Frantsevich Institute for Problems of Materials Science
[2] State Reserve Agency of Ukraine,Research Institute ‘Resurs’
[3] National Aviation University,undefined
来源
关键词
Fe; Mo; Cr; C system; high-temperature phase equilibria; manganese-like phases; linear thermal expansion coefficients;
D O I
暂无
中图分类号
学科分类号
摘要
Phase equilibria involving the stable high-temperature quaternary χFe,Cr,Mo,C phase were established in the Fe–Mo–Cr–C phase diagram. The arc-melted alloys were annealed at subsolidus temperatures for 52 h and then quenched in liquid gallium. The solidus temperature of the alloys was determined with the Pirani–Alterthum method. High-temperature X-ray diffractometry was employed to monitor the sequence of changes in the alloy phase composition from room temperature to the solidus temperature. The χ + η + α, χ + η, and χ + σ phase equilibria were directly observed at 973 K < T < 1373 K, 1273 K < T < 1530 K, and 1523 K < T < 1530 K, respectively, in the Fe52.5Mo23.5Cr18.7C5.3 (at.%) alloy. The χ + M23C6 + α and χ + σ phase equilibria were directly observed at 973 K ≤ T < 1523 K and 1473 K < T < 1525 K in the Fe55.5Mo11.8Cr28.2C4.5 (at.%) alloy. It was shown that the two-phase χ + σ equilibrium could be preceded by three-phase χ + η + σ equilibria or a single-phase χ Fe,Cr,Mo,C equilibrium region (for the Fe52.5Mo23.5Cr18.7C5.3 alloy in the 1523 K < T < 1530 K temperature range). The quaternary χ Fe,Cr,Mo,C phase was found in the (51.9–64.9) Fe, (5.4–23.5) Mo, (14.5–35.4) Cr, and (1–10.7) C at.% composition ranges. Primary crystallization regions of the σ Fe,Cr,Mo,C and αFe,Cr,Mo,C phases with solidus temperatures of approximately 1530 K (for the Fe52.5Mo23.5Cr18.7C5.3 alloy) and 1525 K (for the Fe55.5Mo11.8Cr28.2C4.5 alloy) were revealed. The linear thermal expansion coefficients for the χ Fe,Cr,Mo,C, η Fe,Cr,Mo,C, and αFe,Cr,Mo,C phases of different composition observed for different temperature ranges were determined.
引用
收藏
页码:613 / 624
页数:11
相关论文
共 50 条
  • [31] FERRITIC Fe-Cr-Ti-Mo ALLOYS WITH A STRENGTHENING INTERMETALLIC PHASE FOR HIGH-TEMPERATURE APPLICATIONS.
    Schumacher, Manfred
    Sauthoff, Gerhard
    Zeitschrift fuer Metallkunde/Materials Research and Advanced Techniques, 1987, 78 (08): : 582 - 589
  • [32] HIGH-TEMPERATURE CREEP DEFORMATION OF A CR-MO-V STEEL
    KIMURA, K
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1986, 72 (05): : S487 - S487
  • [33] High-temperature oxidation of Fe-Cr alloys in air
    Goncharov, O. Yu.
    Kanunnikova, O. M.
    INORGANIC MATERIALS, 2007, 43 (05) : 515 - 519
  • [34] High-temperature oxidation of Fe-Cr alloys in air
    O. Yu. Goncharov
    O. M. Kanunnikova
    Inorganic Materials, 2007, 43 : 515 - 519
  • [35] High-temperature relaxation in a Fe-Cr-Al alloy
    Zhou, ZC
    Han, FS
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 2003, 199 (02): : 202 - 206
  • [36] HIGH-TEMPERATURE SULFIDATION OF FE-MN-CR ALLOYS
    SOUTHWELL, G
    YOUNG, DJ
    OXIDATION OF METALS, 1991, 36 (5-6): : 409 - 421
  • [37] HIGH-TEMPERATURE OXIDATION OF FE-CR-NI ALLOYS
    NIZHELSKIY, PE
    KOZYAVKIN, AA
    RUSSIAN METALLURGY, 1974, (05): : 48 - 51
  • [38] Microstructure and high-temperature properties of Fe-Ti-Cr-Mo-B-C-Y2O3 laser cladding coating
    Zhang, Min
    Wang, Xinhong
    Liu, Shushuai
    Qu, Kaili
    JOURNAL OF RARE EARTHS, 2020, 38 (06) : 683 - 688
  • [39] Microstructure and high-temperature properties of Fe-Ti-Cr-Mo-B-C-Y2O3 laser cladding coating
    Min Zhang
    Xinhong Wang
    Shushuai Liu
    Kaili Qu
    Journal of Rare Earths, 2020, 38 (06) : 683 - 688
  • [40] HIGH-TEMPERATURE PROPERTIES OF LOW C-3CR-1MO-V-NB STEELS
    NAGAE, M
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1376 - 1376