Investigation of dissolution and precipitation behaviours of precipitates in welded joints of high Cr ferritic heat resistant steels

被引:0
|
作者
Li D.J. [1 ,2 ]
Shinozaki K. [1 ]
机构
[1] Department of Mechanical System Engineering, Graduate School of Engineering, Hiroshima University
[2] Institute for Materials Science, Welding and Forming, Technical University Graz
关键词
Ageing; Coarse grained heat affected zone; Comparisons; Heat affected zone; Heat resisting materials; Heat treatment; Parent material; Post weld heat treatment; Practical investigations; Radiation; Simulating; Thermal cycling; Weld zone; X rays;
D O I
10.1007/BF03263417
中图分类号
学科分类号
摘要
This paper is aimed at investigating dissolution and precipitation behaviour in fine grained heat-affected zones (FGHAZ), coarse grained heat-affected zones (CGHAZ), and base metals for the welded joints of high Cr ferrite heat resistant steels. The simulated HAZ (SHAZ) specimens were used, whose thermal cycles were controlled to be the same as those in the actual welded joint with peak temperatures of 1 173 and 1 523 K to represent FGHAZ and CGHAZ, respectively. The behaviours of dissolution and precipitation during welding, PWHT and ageing processes were observed. SEM observation showed that after long time ageing the precipitates in FGHAZ specimens (1 173 K) were fewer and larger than those in CGHAZ (1 523 K) specimens and base metal specimens. This phenomenon implied that growth and coarsening of precipitates in FGHAZ may play a role in the deterioration of creep property and Type IV cracking, which was observed in previous creep tests. X-ray diffraction analysis for the electrolytic extraction showed that the types of precipitates were M 23C6, M7C3, MX, Laves phase, and μ phase. By using software of Thermo-Calc and Dictra, a 3-D model was performed to simulate the dissolution process of M23C6 during welding. It was found that the dissolution of M23C6 can lead to high Cr and high W concentration in a local region. On the other hand, the precipitation behaviour of M23C6 was simulated, and it was found that the growth of M23C6 was fast and in the period of PWHT and creep process it can reach to the equilibrium concentration in a short time of about 2 000 seconds. At last, the growth of Laves phase was simulated and it was found that it grew very slowly and it reached the equilibrium concentration in about 3 000 hours. As an important point, the simulation result showed that Laves phase was easy to grow in the region where M23C6 had dissolved due to the high residual concentration of Cr and W.
引用
收藏
页码:7 / 15
页数:8
相关论文
共 50 条
  • [41] ON THE FRACTURE RESISTANCE OF WELDED JOINTS IN HEAT-RESISTANT STEELS IN CONDITIONS OF CREEP.
    Shron, R.Z.
    Welding Production (English translation of Svarochnoe Proizvodstvo), 1976, 23 (07): : 10 - 13
  • [42] FRACTURE RESISTANCE OF WELDED-JOINTS IN HEAT-RESISTANT STEELS IN CONDITIONS OF CREEP
    SHRON, RZ
    WELDING PRODUCTION, 1976, 23 (07): : 10 - 13
  • [43] Formation Mechanism of Type IV Failure in High Cr Ferritic Heat-Resistant Steel-Welded Joint
    Y. Liu
    S. Tsukamoto
    T. Shirane
    F. Abe
    Metallurgical and Materials Transactions A, 2013, 44 : 4626 - 4633
  • [44] Formation Mechanism of Type IV Failure in High Cr Ferritic Heat-Resistant Steel-Welded Joint
    Liu, Y.
    Tsukamoto, S.
    Shirane, T.
    Abe, F.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2013, 44A (10): : 4626 - 4633
  • [45] Effect of Co on creep deformation and precipitation behavior of high-Cr ferritic steels
    Kadoya, Y
    Shimizu, E
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2002, 88 (09): : 539 - 546
  • [46] Effects of W and Co on long-term creep strength of precipitation strengthened 15Cr ferritic heat resistant steels
    Toda, Y
    Seki, K
    Kimura, K
    Abe, F
    ISIJ INTERNATIONAL, 2003, 43 (01) : 112 - 118
  • [47] Effect of microstructure on elastic property at high temperatures in ferritic heat resistant steels
    Sawada, K
    Ohba, T
    Kushima, H
    Kimura, K
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 394 (1-2): : 36 - 42
  • [48] METHODS OF IMPROVING THE EFFICIENCY OF WELDED-JOINTS MADE OF HEAT-RESISTANT AND HIGH-TEMPERATURE STEELS AND ALLOYS
    ZEMZIN, VN
    AUTOMATIC WELDING USSR, 1985, 38 (07): : 32 - 35
  • [49] INFLUENCE OF HIGH-TEMPERATURE SOAKING AND MECHANICAL LOADING ON PROPERTIES OF WELDED-JOINTS IN HEAT-RESISTANT STEELS
    SHTRIKMAN, MM
    WELDING PRODUCTION, 1976, 23 (10): : 29 - 33
  • [50] Thermodynamic modelling of the microstructure of high Cr ferritic creep resistant steam pipe steels
    Hald, J