Room Temperature Photocatalytic Oxidation of Carbon Monoxide Over Pd/TiO2–SiO2 Catalysts

被引:1
|
作者
Gurkan Karakas
Pelin Yetisemiyen
机构
[1] Middle East Technical University,Department of Chemical Engineering
来源
Topics in Catalysis | 2013年 / 56卷
关键词
Photocatalysis; TiO; SiO; Pd; CO oxidation;
D O I
暂无
中图分类号
学科分类号
摘要
The photocatalytic oxidation of carbon monoxide over TiO2–SiO2 and Pd/TiO2–SiO2 catalysts was studied. The catalyst samples were synthesized by using sol–gel technique coupled with hydrothermal treatment and all samples were hydrothermally treated before calcination in air. The catalyst samples were characterized by XRD, BET and DRIFTS techniques. The photocatalytic activity of the samples was determined by using circulated batch photoreactor coupled with in line gas transmission FTIR cell charged with 2,000 ppm carbon monoxide in air initially over 0.5 g of catalyst sample under 33 W (254 nm) irradiation power. XRD and BET results confirmed the presence of anatase phase and the decrease on the crystallite size of TiO2 with SiO2 addition which yield higher surface area and better dispersion of TiO2 over mesoporous SiO2. DRIFTS results indicated the presence of surface hydroxyls coordinated to Ti4+ and Si–O–Ti sites. All samples containing 10–90 % TiO2 over SiO2 exhibited significant photo oxidation activity at room temperature. The photocatalytic oxidation rate of carbon monoxide is favored by SiO2 addition due to high surface area, better dispersion of TiO2 particles and higher surface defects. The addition of PdO improves the photocatalytic activity significantly and the synergy between the TiO2 and PdO phases.
引用
收藏
页码:1883 / 1891
页数:8
相关论文
共 50 条
  • [21] Role of PdAg Interface in Pd-Ag/SiO2 Bimetallic Catalysts in Low-Temperature Oxidation of Carbon Monoxide
    Bondarchuk, I. S.
    Mamontov, G. V.
    KINETICS AND CATALYSIS, 2015, 56 (03) : 379 - 385
  • [22] Coupling system application in photocatalytic degradation of methylorange by TiO2, TiO2/SiO2 and TiO2/SiO2/Ag
    Hossein Ghasemi Mobtaker
    Seyed Javad Ahmadi
    Shahram Moradi Dehaghi
    Taher Yousefi
    Rare Metals, 2015, 34 (12) : 851 - 858
  • [23] Coupling system application in photocatalytic degradation of methylorange by TiO2, TiO2/SiO2 and TiO2/SiO2/Ag
    Hossein Ghasemi Mobtaker
    Seyed Javad Ahmadi
    Shahram Moradi Dehaghi
    Taher Yousefi
    Rare Metals, 2015, 34 : 851 - 858
  • [24] Coupling system application in photocatalytic degradation of methylorange by TiO2, TiO2/SiO2 and TiO2/SiO2/Ag
    Mobtaker, Hossein Ghasemi
    Ahmadi, Seyed Javad
    Dehaghi, Shahram Moradi
    Yousefi, Taher
    RARE METALS, 2015, 34 (12) : 851 - 858
  • [25] ADSORPTION AND CATALYTIC PROPERTIES OF PD/SIO2, CU/SIO2, AND PD-CU/SIO2 SYSTEMS .3. CARBON-MONOXIDE AND BENZENE HYDROGENATION OVER PD-CU/SIO2 CATALYSTS
    LEON Y LEON, CA
    VANNICE, MA
    APPLIED CATALYSIS, 1991, 69 (02): : 305 - 321
  • [26] Characterization of Au/MnOx/TiO2 for photocatalytic oxidation of carbon monoxide
    Kim, Hyun-Jong
    Han, Myung-Keun
    Lee, Sang-Min
    Hwang, Duck Kun
    Shul, Yong-Gun
    TOPICS IN CATALYSIS, 2008, 47 (3-4) : 109 - 115
  • [27] Characterization of Au/MnOx/TiO2 for Photocatalytic Oxidation of Carbon Monoxide
    Hyun-Jong Kim
    Myung-Keun Han
    Sang-Min Lee
    Duck Kun Hwang
    Yong-Gun Shul
    Topics in Catalysis, 2008, 47 : 109 - 115
  • [28] Formaldehyde Oxidation on Pd/TiO2 Catalysts at Room Temperature: The Effects of Surface Oxygen Vacancies
    Yaobin Li
    Chunying Wang
    Changbin Zhang
    Hong He
    Topics in Catalysis, 2020, 63 : 810 - 816
  • [29] Influence of alkali metals on Pd/TiO2 catalysts for catalytic oxidation of formaldehyde at room temperature
    Li, Yaobin
    Zhang, Changbin
    He, Hong
    Zhang, Jianghao
    Chen, Min
    CATALYSIS SCIENCE & TECHNOLOGY, 2016, 6 (07) : 2289 - 2295
  • [30] Rhodium catalysts on SiO2, TiO2, and SiO2-TiO2 for the reforming of methane with carbon dioxide
    Józwiak, WK
    Ignaczak, W
    Fedorov, R
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY, 2005, 79 (07): : 1047 - 1053