SiC fibre by chemical vapour deposition on tungsten filament

被引:0
|
作者
R. V. Krishnarao
J. Subrahmanyam
S. Subbarao
机构
[1] Defence Metallurgical Research Laboratory,
来源
关键词
SiC; CVD; continuous fibre; composite; deposition;
D O I
暂无
中图分类号
学科分类号
摘要
A CVD system for the production of continuous SiC fibre was set up. The process of SiC coating on 19 µ m diameter tungsten substrate was studied. Methyl trichloro silane (CH3SiCl3) and hydrogen reactants were used. Effect of substrate temperature (1300–1500°C) and concentration of reactants on the formation of SiC coating were studied. SiC coatings of negligible thickness were formed at very low flow rates of hydrogen (5 × 10−5 m3/min) and CH3SiCl3 (1.0 × 10−4 m3/min of Ar). Uneven coatings and brittle fibres were formed atvery high concentrations of CH3SiCl3 (6 × 10−4 m3/min of Ar). The flow rates of CH3SiCl3 and hydrogen were adjusted to get SiC fibre with smooth surface. The structure and morphology of SiC fibres were evaluated.
引用
收藏
页码:273 / 279
页数:6
相关论文
共 50 条
  • [41] Hot-filament chemical vapour deposition of nanodiamond on silicon nitride substrates
    Amaral, M
    Oliveira, F
    Belmonte, M
    Fernandes, AJS
    Costa, FM
    Silva, RF
    DIAMOND AND RELATED MATERIALS, 2004, 13 (4-8) : 643 - 647
  • [42] Pulsed biased growth of nanocrystalline diamond by hot filament chemical vapour deposition
    Jones, AN
    Ahmed, W
    Hassan, IU
    Sein, H
    Rego, CA
    SURFACE ENGINEERING, 2004, 20 (03) : 181 - 185
  • [43] Nucleation and initial growth of diamond by biased hot filament chemical vapour deposition
    Wang, WL
    Sanchez, G
    Polo, MC
    Zhang, RQ
    Esteve, J
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 1997, 65 (03): : 241 - 249
  • [44] A Study of Diamond Synthesis by Hot Filament Chemical Vapour Deposition on Nanocomposite Coatings
    Polini, R.
    Kumashiro, S.
    Jackson, M. J.
    Amar, M.
    Ahmed, W.
    Sein, H.
    SURFACE ENGINEERING, PROCEEDINGS, 2006, : 256 - +
  • [45] Paramagnetic defects in diamond films synthesized by the hot filament chemical vapour deposition
    Banaszak, A.
    Fabisiak, K.
    Kaczmarski, M.
    Kozanecki, M.
    CRYSTAL RESEARCH AND TECHNOLOGY, 2006, 41 (06) : 535 - 540
  • [46] Nucleation and initial growth of diamond by biased hot filament chemical vapour deposition
    W.L. Wang
    G. Sánchez
    M.C. Polo
    R.Q. Zhang
    J. Esteve
    Applied Physics A, 1997, 65 : 241 - 249
  • [47] CHEMICAL VAPOR-DEPOSITION OF TUNGSTEN AND TIN ON SIC FIBERS
    HWAN, L
    KMETZ, M
    SUIB, SL
    GALASSO, FS
    JOURNAL OF MATERIALS SCIENCE, 1992, 27 (11) : 2873 - 2876
  • [48] Liquid polycarbosilane as a potential chemical liquid vapour deposition precursor for SiC
    Nair, Sandhya G.
    Siva, M. Subramania
    Thomas, Deepthi
    Sreejith, K. J.
    Prabhakaran, P., V
    Devasia, Renjith
    CERAMICS INTERNATIONAL, 2019, 45 (14) : 17442 - 17446
  • [49] Aerosol Assisted Chemical Vapour Deposition Control Parameters for Selective Deposition of Tungsten Oxide Nanostructures
    Vallejos, S.
    Umek, P.
    Blackman, C.
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2011, 11 (09) : 8214 - 8220
  • [50] Chemical vapour deposition
    Kareh, Kristina Maria
    NATURE REVIEWS METHODS PRIMERS, 2021, 1 (01):