Physical Modeling of Metallurgical Slag Foaming Induced by Chemical Reaction

被引:0
|
作者
Bo Zhang
Ruifang Wang
Chengjun Liu
Peiyang Shi
Maofa Jiang
机构
[1] Northeastern University,Key Laboratory for Ecological Metallurgy of Multimetallic Ores (Ministry of Education)
[2] Northeastern University,School of Metallurgy
[3] Baotou Research Institute of Rare Earths,State Key Laboratory of Baiyunobo Rare Earth Resource Researches and Comprehensive Utilization
[4] Northeastern University,National Frontiers Science Center for Industrial Intelligence and Systems Optimization
[5] Ministry of Education,Key Laboratory of Data Analytics and Optimization for Smart Industry (Northeastern University)
来源
JOM | 2022年 / 74卷
关键词
D O I
暂无
中图分类号
学科分类号
摘要
Control of slag foaming induced by chemical reactions is vital for efficient and safe production of metallurgical processes. Through physical modeling, this paper investigates the effects of amount of gas generated, viscosity, and surface tension of the slag on the slag foaming induced by chemical reaction. The research outcomes indicate that the maximum volume fraction of gas increases and spherical-cell foam gradually evolves into polyhedral-cell foam with increasing generation of gas. The evolution of the foam structure is prevented by an increase in the viscosity of the slag. As the viscosity of the slag increases, the maximum volume fraction of gas increases first and consequently marginally decreases. With decreasing the surface tension, the maximum volume fraction of gas increases and the decaying rate of foam decreases. The increase in the maximum volume fraction of gas arising from decreasing surface tension is reduced with increasing generation of gas.
引用
收藏
页码:4930 / 4937
页数:7
相关论文
共 50 条
  • [21] Micro insight into foaming behavior of CaO-SiO2-FexO-MgO-based slag induced by slag/metal reaction
    Wang, Ruifang
    Zhang, Bo
    Liang, Yudong
    Liu, Chengjun
    Jiang, Maofa
    CERAMICS INTERNATIONAL, 2023, 49 (11) : 17185 - 17193
  • [22] Foaming and the Rate of the Carbon-Iron Oxide Reaction in Slag
    Corbari, Rodrigo
    Matsuura, Hiroyuki
    Halder, Sabuj
    Walker, Matthew
    Fruehan, Richard J.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2009, 40 (06): : 940 - 948
  • [23] Foaming and the Rate of the Carbon-Iron Oxide Reaction in Slag
    Rodrigo Corbari
    Hiroyuki Matsuura
    Sabuj Halder
    Matthew Walker
    Richard J. Fruehan
    Metallurgical and Materials Transactions B, 2009, 40 : 940 - 948
  • [24] Physical modelling of slag-foaming phenomenon resulted from inside-origin gas formation reaction
    Qiu, G.
    Shan, C.
    Zhang, X.
    Lv, X.
    IRONMAKING & STEELMAKING, 2017, 44 (04) : 246 - 254
  • [25] Sinter-crystallization kinetics and foaming of glass from metallurgical slag in air and inert atmosphere
    Jordanov, N. B.
    Kukeva, R.
    Stoyanova, R.
    Karamanov, A.
    THERMOCHIMICA ACTA, 2023, 723
  • [26] Progress in Slag Foaming in Metallurgical Processes (vol 43B, pg 751, 2012)
    Zhu, Tai Xi
    King, Matthew Peter
    Coley, K. S.
    Irons, G. A.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2013, 44 (02): : 478 - 478
  • [27] Physical Modeling of Metallurgical Processes.
    Mundim, Marcos Jose
    de S. Costa, Sergio Luiz
    Costa de Andrade, Sidmei O.
    Metalurgia ABM, 1987, 43 (353): : 208 - 212
  • [28] Study on the properties of physical and chemical foaming concrete
    Li, Qijin
    Li, Guozhong
    Jiang, Congcong
    CHEMICAL ENGINEERING AND MATERIAL PROPERTIES II, 2012, 549 : 741 - 744
  • [29] METALLURGICAL MEASURES AND CONDITIONS FOR DESULFURIZATION OF STEEL BY THE SLAG REACTION METHOD
    GRUNER, H
    WIEMER, HE
    BARDENHEUER, F
    FIX, W
    STAHL UND EISEN, 1979, 99 (14): : 725 - 737
  • [30] EFFECT OF THE BUBBLE-SIZE AND CHEMICAL-REACTIONS ON SLAG FOAMING
    ZHANG, Y
    FRUEHAN, RJ
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1995, 26 (04): : 803 - 812