Structure and mechanical properties of iron subjected to surface severe plastic deformation by attrition: II. Mechanical properties of nano- and submicrocrystalline iron

被引:8
|
作者
Yurkova A.I. [1 ,2 ]
Milman Y.V. [2 ]
Byakova A.V. [1 ,2 ]
机构
[1] Kiev Polytechnical Institute, National Technical University of Ukraine, Kiev 03056
[2] Institute of Problems of Materials Science, National Academy of Sciences of Ukraine
关键词
Severe Plastic Deformation; RUSSIAN Metallurgy; Triple Junction; Grain Boundary Slide; Armco Iron;
D O I
10.1134/S0036029510040026
中图分类号
学科分类号
摘要
Depth-sensing indentation is used to study the effect of grain refinement to submicro- and nanograins on the mechanical properties (hardness, plasticity, Young's modulus) of armco iron subjected to severe plastic deformation by attrition in argon. In contrast to fcc metals, where the hardness increases and the plasticity decreases as the grain size decreases to 20 nm, the hardness of bcc iron decreases from 5.8 to 3.7 GPa and plasticity δA increases from 0.82 to 0.87 as the grain size decreases from 50 to 20 nm. © 2010 Pleiades Publishing, Ltd.
引用
收藏
页码:258 / 263
页数:5
相关论文
共 50 条
  • [1] Structure and mechanical properties of iron after surface severe plastic deformation under friction with simultaneous nitrogen saturation: II. The mechanical properties of nano- and submicrocrystalline iron saturated with nitrogen during deformation
    Yurkova A.I.
    Mil'man Y.V.
    Byakova A.V.
    Russian Metallurgy (Metally), 2012, 2012 (4) : 282 - 289
  • [2] Structure and mechanical properties of iron subjected to surface severe plastic deformation by friction: I. Structure formation
    Yurkova A.I.
    Milman Y.V.
    Byakova A.V.
    Russian Metallurgy (Metally), 2010, 2010 (4) : 249 - 257
  • [3] Mechanical properties of iron processed by severe plastic deformation
    Han, BQ
    Lavernia, EJ
    Mohamed, FA
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34 (01): : 71 - 83
  • [4] Mechanical properties of iron processed by severe plastic deformation
    Bing Q. Han
    Farghalli A. Mohamed
    Enrique J. Lavernia
    Metallurgical and Materials Transactions A, 2003, 34 : 71 - 83
  • [5] The structural features and mechanical properties of submicrocrystalline nickel produced by severe plastic deformation
    Kolobov Yu.R.
    Girsova N.V.
    Ivanov K.V.
    Grabovetskaya G.P.
    Perevalova O.B.
    Russian Physics Journal, 2002, 45 (6) : 547 - 552
  • [6] Mechanical properties of nanostructured iron obtained by various methods of severe plastic deformation
    Sus-Ryszkowska, M
    Pakiela, Z
    Valiev, RZ
    Wyrzykowski, JW
    Kurzydlowski, KJ
    BULK AND GRADED NANOMETALS, 2005, 101-102 : 85 - 90
  • [7] Mechanical properties of submicrocrystalline aluminum alloys after severe plastic deformation by angular pressing
    Markushev, MV
    Murashkin, MY
    PHYSICS OF METALS AND METALLOGRAPHY, 2000, 90 (05): : 506 - 515
  • [8] DEPENDENCE OF THE DISLOCATION STRUCTURE AND MECHANICAL PROPERTIES OF IRON ON CONDITIONS OF PLASTIC DEFORMATION.
    Pavlov, V.A.
    Filippov, Yu.I.
    Ketova, V.P.
    Pecherkina, N.L.
    Physics of Metals and Metallography, 1982, 53 (03): : 152 - 157
  • [9] Grain refinement and mechanical properties of nickel subjected to severe plastic deformation
    Krasilnikov, NA
    Pakiela, Z
    Lojkowski, W
    Valiev, RZ
    INTERFACIAL EFFECTS AND NOVEL PROPERTIES OF NANOMATERIALS, 2003, 94 : 51 - 54
  • [10] Interfacial structure and mechanical properties of surface iron-nickel alloying layer in pure iron fabricated by surface mechanical attrition alloy treatment
    An, Yan-li
    Du, Hua-yun
    Wei, Ying-hui
    Wang, Ning
    Hou, Li-feng
    Lin, Wan-ming
    MATERIALS & DESIGN, 2013, 46 : 627 - 633