Microstructure and Abrasive Wear Performance of Ni-Wc Composite Microwave Clad

被引:0
|
作者
Amit Bansal
Sunny Zafar
Apurbba Kumar Sharma
机构
[1] Indian Institute of Technology Roorkee,Mechanical and Industrial Engineering Department
关键词
cermet; cladding; composite; electron microscopy; microhardness; microwave; wear;
D O I
暂无
中图分类号
学科分类号
摘要
In the present work, Ni-WC powder was deposited on mild steel substrate to develop clads through microwave hybrid heating technique. The cladding trials were carried out in an industrial microwave applicator at 1.1 kW for 540 s. The Ni-WC composite clads were characterized for microstructure and abrasive wear performance through combination of x-ray diffraction, electron and optical microscopy, microhardness, and wear tests. Phase analysis of the Ni-WC clad indicated the presence of stable carbides such as WC, W2C, Ni2W4C, and Fe6W6C. The microstructure study of the clad layer revealed the presence of a uniformly distributed interlocked WC-based reinforcement embedded in the Ni-based matrix. The average Vicker’s microhardness in the clad layer was observed to be 1028 ± 90 HV, which was approximately three times the microhardness of the substrate. Abrasive wear resistance of the microwave clads was superior to the MS substrate. Abrasion was the main wear mechanism in the Ni-WC clads and the substrate samples. However, the presence of WC-based reinforcement in the composite clads reduced microcutting, resulting in enhanced wear resistance.
引用
收藏
页码:3708 / 3716
页数:8
相关论文
共 50 条
  • [21] Pulse Electrocodeposited Ni-WC Composite Coating
    Gupta, R. N.
    Das, A. K.
    Nagahanumaiah
    Henal, Shah
    MATERIALS AND MANUFACTURING PROCESSES, 2016, 31 (01) : 42 - 47
  • [22] Microstructure and wear resistance of a Ni-WC composite coating on titanium grade 2 obtained by electroplating and electron beam remelting
    Li, Yulong
    Song, Peng
    Wang, Wenqin
    Lei, Min
    Li, Xuewen
    MATERIALS CHARACTERIZATION, 2020, 170
  • [23] Microstructure and Abrasive-wear Behavior Under High Temperature of Laser Clad Ni-based WC Ceramic Coating
    Kuang Jian-xin
    Wang Xin-heng
    Liu An-min
    MANUFACTURING ENGINEERING AND AUTOMATION II, PTS 1-3, 2012, 591-593 : 891 - 895
  • [24] Microstructure and Abrasive-wear Behavior Under High Temperature of Laser Clad Ni-based WC Ceramic Coating
    Wang, X. H.
    Liu, A. M.
    INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING (20TH CONGRESS), 2013, 50 : 145 - 149
  • [25] Effect of WC morphology on dry sliding wear behavior of cold-sprayed Ni-WC composite coatings
    Alidokht, Sima A.
    Yue, Stephen
    Chromik, Richard R.
    SURFACE & COATINGS TECHNOLOGY, 2019, 357 : 849 - 863
  • [26] Effect of microstructure and micromechanics on wear/ wear-corrosion mechanism of laser-repaired Ni-WC coating
    Zhang, Xingshou
    Wang, Qinying
    Deng, Yuhang
    Chai, Hui
    Hu, Shaoyan
    Feng, Yuhang
    Xi, Yuchen
    Dong, Lijin
    Lin, Li
    Lin, Yuanhua
    Zeng, Dezhi
    ENGINEERING FAILURE ANALYSIS, 2024, 162
  • [27] On processing of Ni-WC based functionally graded composite clads through microwave heating
    Kaushal, Sarbjeet
    Gupta, Dheeraj
    Bhowmick, Hiralal
    MATERIALS AND MANUFACTURING PROCESSES, 2018, 33 (08) : 822 - 828
  • [28] Effect of Microstructure and Properties of Ni-WC Composite Coatings on Their Solid Particle Erosion Behavior
    Alidokht, Sima A.
    Lengaigne, Jacques
    Klemberg-Sapieha, Jolanta E.
    Yue, Steve
    Chromik, Richard R.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (03) : 1532 - 1543
  • [29] Effect of Microstructure and Properties of Ni-WC Composite Coatings on Their Solid Particle Erosion Behavior
    Sima A. Alidokht
    Jacques Lengaigne
    Jolanta E. Klemberg-Sapieha
    Steve Yue
    Richard R. Chromik
    Journal of Materials Engineering and Performance, 2019, 28 : 1532 - 1543
  • [30] Cold spray deposition of a Ni-WC composite coating and its dry sliding wear behavior
    Alidokht, S. A.
    Manimunda, P.
    Vo, P.
    Yue, S.
    Chromik, R. R.
    SURFACE & COATINGS TECHNOLOGY, 2016, 308 : 424 - 434