Surface-modified WE43 magnesium alloys for reduced degradation and superior biocompatibility

被引:6
|
作者
Manivasagam, Vignesh K. [1 ,2 ]
Sankar, Magesh [3 ,4 ,5 ]
Garcia, Caterina Bartomeu [1 ]
Vishnu, Jithin [3 ]
Chatterjee, Kaushik [6 ]
Suwas, Satyam [6 ]
Manivasagam, Geetha [3 ]
Webster, Thomas J. [1 ,7 ]
机构
[1] Northeastern Univ, Dept Chem Engn, Boston, MA USA
[2] Colorado State Univ, Dept Mech Engn, Ft Collins, CO USA
[3] Vellore Inst Technol, Ctr Biomat Cellular & Mol Theranost CBCMT, Vellore, India
[4] Natl Univ Ireland Galway, Sch Engn & Informat, Galway, Ireland
[5] Natl Univ Ireland Galway, Ctr Res Med Devices CURAM, Galway, Ireland
[6] Indian Inst Sci, Dept Mat Engn, Bangalore 560012, India
[7] Interstellar Therapeut, Boston, MA USA
来源
IN VITRO MODELS | 2022年 / 1卷 / 03期
关键词
Magnesium; WE43; Surface mechanical attrition treatment; In vitro studies; Surface modification; Calcium deposition; Antibacterial; MECHANICAL ATTRITION TREATMENT; IN-VITRO DEGRADATION; AZ31 MG ALLOY; CORROSION BEHAVIOR; STAPHYLOCOCCUS-AUREUS; TEXTURE EVOLUTION; GRAIN-REFINEMENT; ELECTRODEPOSITION; HYDROXYAPATITE; LAYER;
D O I
10.1007/s44164-022-00016-x
中图分类号
Q813 [细胞工程];
学科分类号
摘要
WE43 magnesium alloy was modified using surface mechanical attrition treatment (SMAT) and characterized to evaluate the influence of sub-micron surface modification on degradation rate and in vitro behavior. Modified surface was characterized for wettability, hardness, roughness, degradation rate, in vitro biocompatibility, and antibacterial activity as per the ASTM standards. The treated substrates proved to have a significant decrease in the degradation profile by creating micro pockets of oxidation channels and reducing the total delamination in comparison to the conventional heterogeneous oxide layer formed on the untreated substrate surface. Biocompatibility studies showed that this modification did not induce any toxicity to human fetal osteoblast (hFOB) cells as demonstrated by cell proliferation and enhanced calcium deposition. In fact, results showed that between the 7th day and 14th day of culture, there was an eight time increase in calcium deposition for the surface-treated magnesium alloy. Bacterial adhesion and toxicity studies were carried out using Staphylococcus aureus and methicillin-resistant Staphylococcus aureus. Bacterial toxicity studies showed that both treated and control samples were toxic to the bacteria with more dead cells. Hence, this treatment has developed a highly potential orthopedic surface with decreased biodegradability rate of WE43 and simultaneously enhanced antibacterial properties with good osteoblast cell growth and calcium deposition for faster in vitro bone growth.
引用
收藏
页码:273 / 288
页数:16
相关论文
共 50 条
  • [41] Microstructure and kinetics of hot deformation WE43 magnesium alloy
    Gao Jiacheng
    Wang Qiang
    Wang Yong
    Li Wei
    Niu Wenjuan
    RARE METALS, 2008, 27 (04) : 405 - 409
  • [42] Characterization of continuous dynamic recrystallization in WE43 magnesium alloy
    Fatemi, S. M.
    Paul, H.
    MATERIALS CHEMISTRY AND PHYSICS, 2021, 257
  • [43] Plasticity damage behavior caused by compression twins and double twins in rolled WE43 magnesium alloys
    Liu, Boshu
    Xue, Likai
    Li, Rongguang
    Zong, Lin
    Zhang, Hang
    Li, Jingren
    Li, Shanshan
    Wu, Di
    MATERIALS LETTERS, 2023, 350
  • [44] STRUCTURE AND PROPERTIES OF ADDITIVELY MANUFACTURED WE43 MAGNESIUM ALLOY
    Kristofova, Patricia
    Kubasek, Jiri
    Roudnicka, Michaela
    Michalcova, Alena
    Suchy, Jan
    Palousek, David
    Vojtech, Dalibor
    28TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2019), 2019, : 1578 - 1582
  • [45] HIGH STRAIN RATE SUPERPLASTICITY OF WE43 MAGNESIUM ALLOY
    Vavra, Tomas
    Kral, Robert
    Kubasek, Jiri
    Zemkova, Maria
    Minarik, Peter
    28TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2019), 2019, : 1297 - 1301
  • [46] Improvement in corrosion resistance of WE43 magnesium alloy by the electrophoretic formation of a ZnO surface coating
    J. E. Qu
    M. Ascencio
    L. M. Jiang
    S. Omanovic
    L. X. Yang
    Journal of Coatings Technology and Research, 2019, 16 : 1559 - 1570
  • [47] Microstructure and kinetics of hot deformation WE43 magnesium alloy
    GAO Jiacheng
    RareMetals, 2008, (04) : 405 - 409
  • [48] Superplastic behavior in ingot metallurgy WE43 magnesium alloy
    Watanabe, H
    Mukai, T
    Ishikawa, K
    Mohri, T
    Mabuchi, M
    Higashi, K
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 2043 - 2046
  • [49] Improvement in corrosion resistance of WE43 magnesium alloy by the electrophoretic formation of a ZnO surface coating
    Qu, J. E.
    Ascencio, M.
    Jiang, L. M.
    Omanovic, S.
    Yang, L. X.
    JOURNAL OF COATINGS TECHNOLOGY AND RESEARCH, 2019, 16 (06) : 1559 - 1570
  • [50] Low-cycle fatigue behavior of solutionized and aged WE43 magnesium alloys at room temperature
    Cai, Yong
    Wei, Jianxiong
    Yan, Hong
    Chen, Yipeng
    Chen, Rongshi
    JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (06) : 2284 - 2297