Nanometer-scale chip formation and surface integrity of pure titanium in diamond turning

被引:1
|
作者
Mehdi Heidari
Jiwang Yan
机构
[1] Keio University,Department of Mechanical Engineering
关键词
Pure titanium; Ultraprecision cutting; Diamond turning; Chip formation; Surface roughness; Tool wear;
D O I
暂无
中图分类号
学科分类号
摘要
Titanium is attracting great attentions in aerospace and medical applications where high surface quality plays an important role in improving the product performance. For developing nano-precision machining technology for titanium, clarification of the nanometer-scale chip formation mechanism is essential. In this study, the surface formation mechanism of pure titanium in ultraprecision cutting tests using single-crystal diamond tools was investigated. The results demonstrated that decreasing undeformed chip thickness from the micrometer scale down to the nanometer scale had profound impacts on the shear angle, specific cutting force, and chip morphology. Chip tearing phenomenon occurred when undeformed chip thickness is smaller than a critical value (~ 100 nm), which significantly affected the chip morphology and machined surface integrity. In nanometer-scale cutting, tool feed mark is no longer a major reason of surface roughness; instead, material plucking, debris, scratches, and chip adhesion influenced the surface integrity. The high pressure generated in the nanometer-scale cutting caused a hardness increase in workpiece material and promoted workpiece material adhesion to the tool surface, as well as tool wear.
引用
收藏
页码:479 / 492
页数:13
相关论文
共 50 条
  • [21] SURFACE MODIFICATION OF NANOMETER-SCALE SILVER PARTICLES BY IMIDAZOLE
    VUKOVIC, VV
    NEDELJKOVIC, JM
    LANGMUIR, 1993, 9 (04) : 980 - 983
  • [22] Effect of titanyl sulfate concentration on growth of nanometer-scale rutile rod arrays on the surface of titanium substrate
    Liu, Xing-zhu
    Yoshioka, Tomohiko
    Hayakawa, Satoshi
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2019, 127 (08) : 545 - 550
  • [23] FORMATION OF NANOMETER-SCALE GROOVES IN SILICON WITH A SCANNING TUNNELING MICROSCOPE
    KOBAYASHI, A
    GREY, F
    WILLIAMS, RS
    AONO, M
    SCIENCE, 1993, 259 (5102) : 1724 - 1726
  • [24] Preparation and characterization of nanometer-scale polycarbonate fibers: Bead formation
    Shawon, J
    Sung, C
    ELECTRONICS ON UNCONVENTIONAL SUBSTRATES-ELECTROTEXTILES AND GIANT-AREA FLEXIBLE CIRCUITS, 2003, 736 : 115 - 120
  • [25] Formation of nanometer-scale structures using conventional optical lithography
    Kim, Kyoung S.
    Lee, Kyoung Nam
    Roh, Yonghan
    THIN SOLID FILMS, 2008, 516 (07) : 1489 - 1492
  • [26] Nanometer-scale hydrogen 'portals' for the control of magnesium hydride formation
    Chung, Chia-Jung
    Nivargi, Chinmay
    Clemens, Bruce
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2015, 17 (43) : 28977 - 28984
  • [28] PECULIARITIES OF COBALT NANOMETER-SCALE PARTICLE NUCLEATION ON AN ALUMINA SURFACE
    VASILKOV, AY
    OLENIN, AY
    TITOVA, EF
    SERGEEV, VA
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1995, 169 (02) : 356 - 360
  • [29] HARDNESS DEMONSTRATION OF DIAMOND TIPS BY NANOMETER-SCALE CONTROLLED SCRATCHING ON METALLIC SURFACES
    CHU, X
    MA, Z
    LIU, N
    CHANG, ZP
    HU, TM
    XUE, ZQ
    PANG, SJ
    APPLIED PHYSICS LETTERS, 1993, 63 (25) : 3446 - 3448
  • [30] Nanometer-scale ordered arrangement of diamond nanoparticles on substrates via electrostatic deposition
    Yoshikawa, Taro
    Liu, Ming
    Miyake, Hiroto
    Ieki, Ryosuke
    Kojima, Ryouta
    Makino, Yuto
    Tsurui, Akihiko
    Mahiko, Tomoaki
    Nishikawa, Masahiro
    APPLIED PHYSICS EXPRESS, 2021, 14 (05)