Hot cracking behaviour of an autogenously laser welded Al-Cu-Li alloy

被引:0
|
作者
J. Enz
C. Carrarin
S. Riekehr
V. Ventzke
N. Kashaev
机构
[1] Institute of Materials Research,Helmholtz
[2] Materials Mechanics,Zentrum Geesthacht
关键词
Al-Li alloy; Laser welding; Autogenous welding; Hot cracking; Mechanical properties;
D O I
暂无
中图分类号
学科分类号
摘要
AA2198 is a relatively new light-weight and high-performance Al-Cu-Li alloy considered for aviation and space applications. However, Al-Cu-Li alloys generally exhibit severe weldability problems for all fusion-welding techniques, such as laser-beam welding. In particular, porosity formation and hot cracking are observed for the laser-beam welding of these alloys. A common remedy for hot cracking is the use of an appropriate filler wire with a high Si content. In the present study, three different approaches for improving the hot cracking susceptibility of AA2198 laser beam welded without any filler material are presented. For this purpose, pre-heating of the weld samples to elevated temperatures, pre-loading of the weld samples perpendicular to the welding direction, or an optimization of the laser-beam welding parameters were conducted. The autogenously welded samples were assessed with regard to the resulting total crack length and their mechanical properties. It was demonstrated that all of the presented approaches led to a reduction of hot cracking. However, the largest effect was observed for the use of low levels of laser power and welding velocity. The mechanical properties of the optimised autogenously welded samples are only marginally inferior as for the samples laser welded with the Al-Si filler wire AA4047.
引用
收藏
页码:299 / 310
页数:11
相关论文
共 50 条
  • [31] A Weldability Study of Al-Cu-Li 2198 Alloy
    Calogero, V.
    Costanza, G.
    Missori, S.
    Sili, A.
    Tata, M. E.
    METALLURGIST, 2014, 57 (11-12) : 1134 - 1141
  • [32] Characterization of Localized Corrosion in an Al-Cu-Li Alloy
    Chen Luo
    Xinxin Zhang
    Xiaorong Zhou
    Zhihua Sun
    Xiaoyun Zhang
    Zhihui Tang
    Feng Lu
    George E. Thompson
    Journal of Materials Engineering and Performance, 2016, 25 : 1811 - 1819
  • [33] A new ultrahigh strength Al-Cu-Li alloy
    Zhong, Jifa
    Zheng, Ziqiao
    Luo, Xianfu
    Aluminium Alloys 2014 - ICAA14, 2014, 794-796 : 1050 - 1056
  • [34] Ageing response of a Al-Cu-Li 2198 alloy
    Zhang, Sai-fei
    Zeng, Wei-dong
    Yang, Wen-hua
    Shi, Chun-ling
    Wang, Hao-jun
    MATERIALS & DESIGN, 2014, 63 : 368 - 374
  • [35] Superplastic behavior of Al-Cu-Li based alloy
    Du Yu-xuan
    Zhang Xin-ming
    Ye Ling-ying
    Luo Zhi-hui
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1379 - S1382
  • [36] TB-PRECIPITATES IN AN AL-CU-LI ALLOY
    LUDWICZAK, EA
    RIOJA, RJ
    SCRIPTA METALLURGICA ET MATERIALIA, 1991, 25 (06): : 1415 - 1419
  • [37] The propagation of localized corrosion in Al-Cu-Li alloy
    Zhang, X.
    Zhou, X.
    Ma, Y.
    Thompson, G. E.
    Luo, C.
    Sun, Z.
    Zhang, X.
    Tang, Z.
    SURFACE AND INTERFACE ANALYSIS, 2016, 48 (08) : 745 - 749
  • [38] Investigation of welding parameters on microstructure and mechanical properties of laser beam-welded joint of 2060 Al-Cu-Li alloy
    Gu, Cheng
    Wei, Yanhong
    Zhan, Xiaohong
    Zhang, Dan
    Ren, Shuai
    Liu, Hongbing
    Li, Hao
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 91 (1-4): : 771 - 780
  • [39] Study of the structure and phase composition of laser welded joints of Al-Cu-Li alloy under different heat treatment conditions
    Malikov, Alexandr
    Bulina, Natalia
    Sharafutdinov, Marat
    Orishich, Anatoliy
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 104 (9-12): : 4313 - 4324
  • [40] Study of the structure and phase composition of laser welded joints of Al-Cu-Li alloy under different heat treatment conditions
    Alexandr Malikov
    Natalia Bulina
    Marat Sharafutdinov
    Anatoliy Orishich
    The International Journal of Advanced Manufacturing Technology, 2019, 104 : 4313 - 4324