Influence of Work Hardening on Tensile and Fatigue Behavior of Resistance Spot-Welded Dual-Phase Steel

被引:0
|
作者
Gorti Janardhan
Krishna Dutta
Goutam Mukhopadhyay
机构
[1] GMR Institute of Technology,Department of Mechanical Engineering
[2] National Institute of Technology of Rourkela,Department of Metallurgical and Materials Engineering
[3] R & D,undefined
关键词
dislocation density; DP600 steel; fatigue; load carrying ability; prestrain; spot-welds;
D O I
暂无
中图分类号
学科分类号
摘要
In the current study, 1.4 mm thick dual-phase (DP600) steel sheets were prestrained at 0, 5, 10, and 15% prestrain levels followed by spot-welding in lap-shear configuration. The load carrying ability and fatigue properties of the joints were studied. Besides, the dislocation density of the deformed specimens was estimated by x-ray diffraction (XRD) as well as transmission electron microscopy (TEM). Additionally, in-depth examinations were carried out in terms of microstructure, hardness profiles, as well as fractography. The results indicated that the load carrying ability of joints increased with attendant reduction in energy absorption, with increase in prestrain level. The prestraining of sheets has insignificant influence on the high-cycle fatigue strength of the joints. In case of tensile–shear loading, the initiation of crack occurred at the base metal, while under cyclic loading, crack initiation took place from the heat-affected zone (HAZ). The majority of the dislocations produced owing to the prestraining are annihilated at HAZ during joining process, so there is no noteworthy influence of prestrain on the high-cycle fatigue strength of spot-welds.
引用
收藏
页码:624 / 637
页数:13
相关论文
共 50 条
  • [31] Fatigue Crack Propagation Behavior in Dual-Phase Steel
    PAEC, Dera Ghazi Khan, Pakistan
    不详
    J Mater Eng Perform, 2 (245-251):
  • [32] Influence of in situ postweld heat treatment on microstructure and failure behavior of dual-phase steel resistance spot weld
    Imtiaz Ali Soomro
    Srinivasa Rao Pedapati
    Mokhtar Awang
    The International Journal of Advanced Manufacturing Technology, 2021, 114 : 3739 - 3750
  • [33] The effect of coatings on the resistance spot welding behavior of 780 MPa dual-phase steel
    Tumuluru, M.
    WELDING JOURNAL, 2007, 86 (06) : 161S - 169S
  • [34] Fatigue crack propagation behavior in dual-phase steel
    Sarwar, M
    Priestner, R
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 1999, 8 (02) : 245 - 251
  • [35] Fatigue crack propagation behavior in dual-phase steel
    M. Sarwar
    R. Priestner
    Journal of Materials Engineering and Performance, 1999, 8 : 245 - 251
  • [36] Influence of in situ postweld heat treatment on microstructure and failure behavior of dual-phase steel resistance spot weld
    Soomro, Imtiaz Ali
    Pedapati, Srinivasa Rao
    Awang, Mokhtar
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 114 (11-12): : 3739 - 3750
  • [37] LOAD CARRYING CAPACITY AND MICROSTRUCTURE OF RESISTANCE SPOT WELDED DUAL-PHASE (DP600) STEEL
    Ataya, Sabbah
    CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS 2014, 2014, : 297 - 304
  • [38] Magnetically Assisted Resistance Spot Welding of Dual-Phase Steel
    Li, Y. B.
    Li, Y. T.
    Shen, Q.
    Lin, Z. Q.
    WELDING JOURNAL, 2013, 92 (04) : 124S - 132S
  • [39] FATIGUE OF A DUAL-PHASE STEEL
    SHERMAN, AM
    DAVIES, RG
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (07): : 929 - 933
  • [40] Overload failure curve and fatigue behavior of spot-welded specimens
    Lee, H
    Kim, N
    Lee, TS
    ENGINEERING FRACTURE MECHANICS, 2005, 72 (08) : 1203 - 1221