Decarburization as a tool to explore parallels between solid-solid and liquid-solid transformations: Fe-C-Mn-Si steels

被引:0
|
作者
Brij K. Dhindaw
Deba Prakash Guru
Gary Purdy
Hatem S. Zurob
机构
[1] Indian Institute of Technolgy,
[2] Bharat Heavy Electricals Limited,undefined
[3] McMaster University,undefined
关键词
planar Interface; morphological instability; solidification; decarburization;
D O I
暂无
中图分类号
学科分类号
摘要
The study of single-interface transformations under controlled conditions offers insights into the similarities and distinctions between solidification and solid-solid transformations. In this contribution, we consider some parallels between the formation of a layer of ferrite on an originally austenitic steel bar and the growth of the columnar zone in the solidification of an alloy ingot. The necessary conditions for solid-solid interfacial breakdown of a decarburization front are explored and the evidence to date reviewed. The response of some Fe-C-Mn-Si steels to controlled decarburization is considered, and we present a first report of the morphological instability of a ferrite/austenite decarburization interface, and compare it with the interfacial breakdown in the solid-liquid interface. The instability is tentatively ascribed to the effects of grain-boundary nucleation and/or grain-boundary diffusion of alloying elements in austenite. Other similarities (and differences) between the growth of a ferrite layer on an alloy steel and the development of the columnar zone of an ingot are discussed.
引用
收藏
页码:255 / 260
页数:5
相关论文
共 50 条
  • [21] NOTE ON GRAIN-BOUNDARY PENETRATION OF CU AND MN IN GAMMA-FE AT 1100 DEGREESC DURING LIQUID-SOLID POWDER ALLOYING
    LARSSON, LE
    MATERIALS SCIENCE AND ENGINEERING, 1975, 19 (02): : 241 - 244
  • [22] Low Temperature (-300°C) Epitaxial Growth of SiGe by Liquid-solid Coexisting Annealing of A-GeSn/Si(100) Structure
    Chikita, Hironori
    Matsumura, Ryo
    Sadoh, T.
    Miyao, M.
    QUANTUM, NANO, MICRO TECHNOLOGIES AND APPLIED RESEARCHES, 2014, 481 : 137 - 140
  • [23] Phase field simulation of liquid-solid-eutectoid multiple phase transformations of a Fe-C binary alloy
    Li Feng
    Jun-he Zhong
    Chang-sheng Zhu
    Jun Wang
    Guo-sheng An
    Rong-zhen Xiao
    China Foundry, 2020, (04) : 301 - 307
  • [24] Phase field simulation of liquid-solid-eutectoid multiple phase transformations of a Fe-C binary alloy
    Li Feng
    Jun-he Zhong
    Chang-sheng Zhu
    Jun Wang
    Guo-sheng An
    Rong-zhen Xiao
    China Foundry, 2020, 17 : 301 - 307
  • [25] Phase field simulation of liquid-solid-eutectoid multiple phase transformations of a Fe-C binary alloy
    Feng, Li
    Zhong, Jun-he
    Zhu, Chang-sheng
    Wang, Jun
    An, Guo-sheng
    Xiao, Rong-zhen
    CHINA FOUNDRY, 2020, 17 (04) : 301 - 307
  • [26] Phase field simulation of liquid-solid-eutectoid multiple phase transformations of a Fe-C binary alloy
    Li Feng
    Junhe Zhong
    Changsheng Zhu
    Jun Wang
    Guosheng An
    Rongzhen Xiao
    ChinaFoundry, 2020, 17 (04) : 301 - 307
  • [27] Non-Contact Measurement of Thermophysical Properties of Fe, Fe-C, and Fe-C-Mn Alloys in Solid, Supercooled, and Stable Liquid Phases
    Jeon, Sangho
    Kang, Dong-Hee
    Kang, Shin Hwan
    Kang, Shin Eon
    Okada, Junpei T.
    Ishikawa, Takehiko
    Lee, Sooheyong
    Lee, Geun Woo
    ISIJ INTERNATIONAL, 2016, 56 (04) : 719 - 722
  • [29] Diffusion Behavior of Mn and Si Between Liquid Oxide Inclusions and Solid Iron-Based Alloy at 1473 K
    Kim, Sun-Joong
    Tago, Hanae
    Kim, Kyung-Ho
    Kitamura, Shin-Ya
    Shibata, Hiroyuki
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2018, 49 (03): : 977 - 987
  • [30] Diffusion Behavior of Mn and Si Between Liquid Oxide Inclusions and Solid Iron-Based Alloy at 1473 K
    Sun-Joong Kim
    Hanae Tago
    Kyung-Ho Kim
    Shin-ya Kitamura
    Hiroyuki Shibata
    Metallurgical and Materials Transactions B, 2018, 49 : 977 - 987