Crystal Structure of Silicides in a Ti – 0.7 WT.% Si Nanostructured Alloy

被引:0
|
作者
M. B. Ivanov
S. S. Manokhin
A. Yu. Kolobova
机构
[1] Belgorod State National Research University,
[2] Institute for Problems of Chemical Physics of the Russian Academy of Sciences,undefined
来源
Russian Physics Journal | 2017年 / 60卷
关键词
titanium; titanium silicide; incoherent inclusions; nanostructured state;
D O I
暂无
中图分类号
学科分类号
摘要
Using warm, lengthwise grooved-roll processing of the Ti – 0.7 wt.% Si alloy, a nanostructured state is formed in it at 873 K with the grain-subgrain elements measuring about 280 nm. The titanium silicides precipitating during the dynamic strain-induced aging of the alloy are investigated by the methods of high-resolution scanning electron microscopy. It is found that the shape of the silicides is close to spherical, they have an FCClattice and an incoherent interface with the matrix.
引用
收藏
页码:855 / 861
页数:6
相关论文
共 50 条
  • [41] Mechanical and corrosion resistances of a Sn-0.7 wt.%Cu lead-free solder alloy
    Freitas, Emmanuelle S.
    Osorio, Wislei R.
    Spinelli, Jose E.
    Garcia, Amauri
    MICROELECTRONICS RELIABILITY, 2014, 54 (6-7) : 1392 - 1400
  • [42] The effect of flow localization and shear bands development on the structure and mechanical behavior of Cu-4.98 wt.% Ti alloy
    Hameda, AA
    Blaz, L
    JOURNAL DE PHYSIQUE IV, 1998, 8 (P8): : 189 - 195
  • [43] Flow softening during hot compression of Cu-3.45 wt.% Ti alloy
    Hameda, AA
    Blaz, L
    SCRIPTA MATERIALIA, 1997, 37 (12) : 1987 - 1993
  • [44] Grain Characteristics and Mechanical Properties of Bioinert Ti-40 wt. % Nb Alloy
    Zhu, Qifang
    Sharkeev, Yurii
    Eroshenk, Anna
    Sun Zeming
    Zhang, Hongju
    Han, Xiaole
    Glukhov, Ivan
    Mairambekova, Aikol
    Khimch, Margarita
    PROCEEDINGS OF THE INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS WITH HIERARCHICAL STRUCTURE FOR NEW TECHNOLOGIES AND RELIABLE STRUCTURES 2019, 2019, 2167
  • [45] Characterization and Calculation of the Dynamic Recrystallization Texture in Fe-3.0 Wt.% Si Alloy
    Shao, Guangshuai
    Sha, Yuhui
    Chen, Xi
    Chang, Songtao
    Zhang, Fang
    Zuo, Liang
    MATERIALS, 2022, 15 (02)
  • [46] Microstructure and mechanical properties of rapidly quenched Fe-6.5 wt.% Si alloy
    Liang, Y. F.
    Lin, J. P.
    Ye, F.
    Li, Y. J.
    Wang, Y. L.
    Chen, G. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 504 : S476 - S479
  • [47] Ultra-mild wear of a hypereutectic Al-18.5 wt.% Si alloy
    Chen, M.
    Alpas, A. T.
    WEAR, 2008, 265 (1-2) : 186 - 195
  • [48] Improvement of magnetic properties of an Fe-6.5 wt.% Si alloy by directional solidification
    Fu, Huadong
    Zhang, Zhihao
    Jiang, Yanbin
    Xie, Jianxin
    MATERIALS LETTERS, 2011, 65 (09) : 1416 - 1419
  • [49] Improvement of magnetic properties of an Fe-6.5 wt. % Si alloy by directional recrystallization
    Zhang, Z. W.
    Chen, G.
    Bei, H.
    Ye, F.
    Chen, G. L.
    Liu, C. T.
    APPLIED PHYSICS LETTERS, 2008, 93 (19)
  • [50] Cooling rate and microstructure of rapidly solidified Al-20 wt.% Si alloy
    Xu, CL
    Wang, HY
    Qiu, F
    Yang, YF
    Jiang, QC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 417 (1-2): : 275 - 280