Hydroxyapatite coating effect on the bond strength between CAD/CAM materials and a resin cement

被引:0
|
作者
Omer Sagsoz
Nurdan Polat Sagsoz
Mustafa Tolga Yurtcan
Niyazi Ozcelik
机构
[1] Ataturk University,Department of Restorative Treatment, Faculty of Dentistry
[2] Ataturk University,Department of Prosthodontics, Faculty of Dentistry
[3] Atatürk University,Department of Nanoscience and Nanoengineering, Graduate School of Natural and Applied Sciences
[4] Atatürk University,Department of Mathematics and Science Education, Kazim Karabekir Education Faculty
[5] Hacettepe University,Department of Chemistry, Faculty of Science
来源
Odontology | 2019年 / 107卷
关键词
Hydroxyapatite; PLD; Surface treatment; CAD/CAM; Resin cements;
D O I
暂无
中图分类号
学科分类号
摘要
The purpose of this study was to evaluate the bond strength between CAD/CAM materials and a resin cement using hydroxyapatite coating as a surface treatment method. Different surface treatments (Control, no treatment-C; Sandblasting-SB; Hydrofluoric acid etching-HF; applying tooth desensitizer-TeM; applying topical crème-ToM, HAp coating with Pulse Laser Deposition technique-PLD) were applied to three different CAD/CAM materials (LAVA Ultimate, VITA Enamic, and Cerec Blocs). After surface treatments, a universal adhesive (Single Bond Universal, 3M ESPE) was applied and adhesive resin (Rely X Ultimate, 3M ESPE) were cemented on each material surface using plastic tubes (4 mm in diameter). The shear bond strength values were measured using a universal testing machine. Scanning electron microscope analysis were performed to evaluate failure modes and effects of surface treatments. Obtained data were statistically analyzed using two-way ANOVA and Tukey’s post hoc test (p = 0.05). The bond strength of PLD groups were significantly higher than other groups in resin-ceramics (p < 0.05). In Cerec Blocs, HF resulted significantly higher bond strength than other groups (p < 0.05). SEM analysis of surface treatment methods (except TeM and ToM) revealed an increase in surface alterations compared to control groups. Failure modes were dominantly adhesive in groups C, TeM, and ToM, whereas mostly mix or cohesive failures were observed in PLD, HF, and SB. Hydroxyapatite coating with PLD technique exhibited promising bond strength results for CAD/CAM resin-ceramics. HAp coating can be used as a replacement for hydrofluoric acid etching and sandblasting in CAD/CAM resin-ceramic materials to obtain better bond strength values.
引用
收藏
页码:491 / 499
页数:8
相关论文
共 50 条
  • [41] Bond Strength of Different Composite Resin Materials and CAD/CAM Restorative Materials to Each Other and Dentin Tissue
    Saridag, Serkan
    Tekce, Neslihan
    Alper, Seval Baspinar
    Inan, Burcu Dereli
    BEZMIALEM SCIENCE, 2022, 10 (06): : 786 - 795
  • [42] Bond strength of ceramic or resin CAD-CAM laminate veneers
    Bakir, Metin
    Bakir, Sehmus
    Bahsi, Emrullah
    AMERICAN JOURNAL OF DENTISTRY, 2020, 33 (06): : 287 - 290
  • [43] Cement bond strength to millable composite for CAD/CAM restorations.
    Sturdevant, JR
    Swift, EJ
    Bayne, SC
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 453 - 453
  • [44] Microtensile Bond Strength of CAD-CAM Restorative Dental Material Blocks to Resin Cement: An In Vitro Study
    Gonzalez-Angulo, Eva
    Fernandez-Estevan, Lucia
    Casas-Terron, Javier
    Senent-Vicente, Gisela
    Fons-Badal, Carla
    Bonmati, Fernando Garcia-Sala
    Agustin-Panadero, Ruben
    Roman-Rodriguez, Juan Luis
    MATERIALS, 2023, 16 (13)
  • [45] Adhesion of a new adhesive resin cement to CAD/CAM materials.
    Rusin, R. P.
    Cummings, K. M.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B337 - B337
  • [46] Evaluation of shear bond strength of zirconia-based monolithic CAD-CAM materials to resin cement after different surface treatments
    Altan, B.
    Cinar, S.
    Tuncelli, B.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2019, 22 (11) : 1475 - 1482
  • [47] Bond strength of resin cement to polyglass and ceramic materials
    O'Keefe, KL
    Li, DF
    Noaman, K
    Powers, JM
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 815 - 815
  • [48] Microtensile Bond Strength of Composite Cement to Novel CAD/CAM Materials as a Function of Surface Treatment and Aging
    Lise, D. P.
    Van Ende, A.
    De Munck, J.
    Vieira, L. C. C.
    Baratieri, L. N.
    Van Meerbeek, B.
    OPERATIVE DENTISTRY, 2017, 42 (01) : 73 - 81
  • [49] Effect of ceramic primers with different chemical contents on the shear bond strength of CAD/CAM ceramics with resin cement after thermal ageing
    Mehmet Uğur
    İdris Kavut
    Özgür Ozan Tanrıkut
    Önder Cengiz
    BMC Oral Health, 23
  • [50] Effect of ceramic primers with different chemical contents on the shear bond strength of CAD/CAM ceramics with resin cement after thermal ageing
    Ugur, Mehmet
    Kavut, Idris
    Tanrikut, Ozgur Ozan
    Cengiz, Onder
    BMC ORAL HEALTH, 2023, 23 (01)