High-Temperature Oxidation and Wear Behavior of (Fe,Cr)Al Intermetallic Compound and (Fe,Cr)Al-Al2O3 Nanocomposites

被引:0
|
作者
F. Sourani
M. H. Enayati
M. Taghipour
机构
[1] Isfahan University of Technology,Department of Materials Engineering
关键词
(Fe,Cr)Al-Al2O3 nanocomposites; intermetallics; nanocomposite; nano-scratch; oxidation resistance; wear behavior;
D O I
暂无
中图分类号
学科分类号
摘要
In the current study, oxidation and wear resistance of FeAl and (Fe,Cr)Al intermetallic compounds as well as (Fe,Cr)Al-5%vol Al2O3 and (Fe,Cr)Al-10%vol Al2O3 nanocomposites were investigated. Ball-milled powders were hot-pressed at 5.5 GPa and 1600 °C for 15 min in order to produce the bulk samples. The cyclic oxidation test was performed at 1100 °C for 100h. High-temperature wear tests were conducted at 400 °C with loads of 20 N in sliding speed and sliding distance of 0.1 m/s and 500 m, respectively. Furthermore, the nano-scratch tests were performed in single-direction as well as pass and return modes with a maximum load of 20 mN. Results showed that the (Fe,Cr)Al intermetallic compound had superior oxidation resistance with the lowest kp value at the same oxidation time. The improved oxidation performance of (Fe,Cr)Al intermetallic compound compared to (Fe,Cr)Al-Al2O3 composites can be due to the presence of more Al in (Fe,Cr)Al sample. According to the nano-scratch test, (Fe,Cr)Al-10%vol Al2O3 nanocomposite (with H/E ratio of 0.036) had the best wear resistance. On the other hand, nanocomposites containing 5% and 10% of Al2O3 had the lowest friction coefficient (≈ 0.6 and 0.3, respectively). The main wear mechanism for the FeAl compound was adhesive wear, while, delamination was the main mechanism for samples containing Al2O3 nanoparticles. Although the formation of Al2O3 reinforcement nanoparticles somewhat decreases the oxidation resistance, it also resulted in significant overall improvement in the wear behavior.
引用
收藏
页码:3654 / 3669
页数:15
相关论文
共 50 条
  • [21] On the oxidation behavior of cathodic arc evaporated Al-Cr-Fe and Al-Cr-Fe-O coatings. I
    Koller, Christian Martin
    Kirnbauer, Alexander
    Dalbauer, Valentin
    Kolozsvari, Szilard
    Ramm, Juergen
    Mayrhofert, Paul-Heinz
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2019, 37 (04):
  • [22] Systematic investigation of the oxidation behavior of Fe-Cr-Al cladding alloys in high-temperature steam
    Wang, Peng
    Qi, Wen
    Yang, Kun
    Qiao, Yingjie
    Wang, Xiaodong
    Zheng, Ting
    Bai, Chengying
    Liu, Zhen
    Zhang, Xiaohong
    CORROSION SCIENCE, 2022, 207
  • [23] High-temperature oxidation behavior of as-cast Ni-Cr-Al-Fe based alloys
    Han, Chao
    Liu, Yong
    Wang, Yan
    Li, Wei-Jie
    Tang, Hui-Ping
    Fenmo Yejin Cailiao Kexue yu Gongcheng/Materials Science and Engineering of Powder Metallurgy, 2011, 16 (06): : 806 - 814
  • [24] COMPARISON OF OXIDATION BEHAVIOR OF FE-CR-AL, NI-CR-AL, AND CO-CR-AL ALLOYS
    STOTT, FH
    WOOD, GC
    HOBBY, MG
    OXIDATION OF METALS, 1971, 3 (02): : 103 - &
  • [25] High-temperature oxidation behavior of ODS-Fe3Al
    Wright, IG
    Pint, BA
    Tortorelli, PF
    OXIDATION OF METALS, 2001, 55 (3-4): : 333 - 357
  • [26] High-Temperature Oxidation Behavior of ODS–Fe3Al
    I. G. Wright
    B. A. Pint
    P. F. Tortorelli
    Oxidation of Metals, 2001, 55 : 333 - 357
  • [27] OXIDATION RESISTANCE OF RAPIDLY SOLIDIFIED FE-CR-AL RIBBONS AT HIGH-TEMPERATURE
    OKABE, S
    KOHNO, M
    ISHII, K
    YUKUMOTO, M
    NOZAKI, T
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1994, 181 : 1104 - 1108
  • [28] HIGH-TEMPERATURE OXIDATION OF FE-CR-(AL) AND FE-CR-NI ALLOYS UNDER TENSILE-STRESS
    IKEDA, Y
    NII, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1983, 47 (03) : 191 - 197
  • [29] Wear behavior of Al-Al2O3 reinforced composites
    Sahin, Y.
    ADVANCED DESIGN TECHNOLOGY, PTS 1-3, 2011, 308-310 : 1577 - 1581
  • [30] High-Temperature Oxidation of Fe3Al and Fe3Al-Zr Intermetallics
    Chevalier, S.
    Juzon, P.
    Borchardt, G.
    Galerie, A.
    Przybylski, K.
    Larpin, J. P.
    OXIDATION OF METALS, 2010, 73 (1-2): : 43 - 64