摘要
Si3N4 ceramic was joined to itself using a filler alloy of (CuZn)85Ti15 at 1123–1323 K for 15 min. TEM observation showed that a reaction zone of TiN and/or Ti2N exists at the interface between the ceramic and filler alloy, and the center of the joint is composed of Cu-Zn solid solution in which there are Cu2TiZn and Ti5Si3 reaction phases. With increasing brazing temperature, both the thickness of the reaction zone and the amount and size of the Ti5Si3 phase increase, while the amount and size of the Cu2TiZn phase decrease. When the brazing temperature reached 1323 K, the Cu2TiZn phase disappeared. When the brazing temperature is lower than 1223 K, the interfacial reaction zone is mainly composed of Ti2N, which has a cylindrical shape and orientates randomly in the zone. There is a crystal orientation relationship between the Ti2N in the reaction zone and the Cu in the Cu-Zn solid solution, which is: {110}Ti2N//{420}Cu, 〈001〉Ti2N//〈001〉Cu. When the brazing temperature is higher than 1223 K, the interfacial zone is composed of TiN, which has a plate shape crossing each other.
引用
收藏
页码:4587 / 4591
页数:4
相关论文
共 50 条
  • [21] Effect of Si3N4-particles addition in Ag-Cu-Ti filler alloy on Si3N4/TiAl brazed joint
    Song, X. G.
    Cao, J.
    Wang, Y. F.
    Feng, J. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (15): : 5135 - 5140
  • [22] EFFECT OF ACTIVE METAL ON BONDING CHARACTERISTICS AND INTERFACIAL STRUCTURE OF THE SI3N4/SI3N4 JOINTS BRAZED BY AG-CU FILLER METAL
    MORIZONO, Y
    NAKATA, T
    NISHIDA, M
    CHIBA, A
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1995, 103 (08) : 810 - 815
  • [23] Interfacial microstructure of Si3N4/Si3N4 joint brazed using Au-Ni-V filler alloy
    Zhang, J.
    Sun, Y.
    Liu, C. F.
    Zhang, H. W.
    JOURNAL OF MATERIALS SCIENCE, 2010, 45 (08) : 2188 - 2193
  • [24] Effect of brazing temperature on microstructure and mechanical properties of Si3N4/Si3N4 joints brazed with Ag–Cu–Ti + Mo composite filler
    Y. M. He
    J. Zhang
    X. Wang
    Y. Sun
    Journal of Materials Science, 2011, 46 : 2796 - 2804
  • [25] Microstructure and mechanical properties of an Si3N4/Si3N4 joint brazed with Au-Ni-Pd-V filler alloy
    Sun, Y.
    Zhang, J.
    Geng, Y. P.
    Ikeuchi, K.
    Shibayanagi, T.
    SCRIPTA MATERIALIA, 2011, 64 (05) : 414 - 417
  • [26] Effect of Ti Content on Microstructure and Mechanical Properties of Si3N4/Si3N4 Joints Brazed with Ag-Cu-Ti plus Mo Composite Filler
    Zhang, Jie
    He, Yanming
    PRICM 7, PTS 1-3, 2010, 654-656 : 2018 - 2021
  • [27] Microstructural and mechanical characterization of the Si3N4/Si3N4 joint brazed using Au-Ni-V filler alloys
    Zhang, J.
    Sun, Y.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (03) : 751 - 757
  • [28] Interfacial structure and strength of Si3N4 ceramics joint brazed with amorphous filler metal and Cu layer
    Zou, Jiasheng
    Zeng, Peng
    Xu, Xiangping
    Hanjie Xuebao/Transactions of the China Welding Institution, 2012, 33 (11): : 47 - 50
  • [29] Microstructure and properties of the Si3N4/Si3N4 brazing joint
    Zhang, J
    Naka, N
    Zhou, Y
    Lei, TQ
    MECHANICS AND MATERIAL ENGINEERING FOR SCIENCE AND EXPERIMENTS, 2001, : 222 - 225
  • [30] Study on interfacial structure and strength of Si3N4/Ti/Cu/Ti/Si3N4 PTLP bonding
    邹家生
    蒋志国
    许志荣
    陈广
    China Welding, 2006, (01) : 11 - 15