Effect of Laves Phase on High-Temperature Deformation and Microstructure Evolution in an 18Cr-2Mo-0.5Nb Ferritic Stainless Steel

被引:0
|
作者
Ken-ichi Ikeda
Nana Kwame Gyan Yamoah
William T. Reynolds
Jun-ichi Hamada
Mitsuhiro Murayama
机构
[1] Kyushu University,Faculty of Engineering Sciences
[2] Hokkaido University,Faculty of Engineering
[3] Virginia Tech,Department of Materials Science and Engineering
[4] North Carolina A&T State University,Department of Mechanical Engineering
[5] Hikari,Nippon Steel & Sumikin Stainless Steel Corporation
关键词
Flow Stress; Lave Phase; Ferritic Stainless Steel; Orowan Strengthen; Precipitate Volume Fraction;
D O I
暂无
中图分类号
学科分类号
摘要
Niobium-containing ferritic stainless steels are finding new applications in automotive exhaust components because of their oxidation resistance, thermal fatigue resistance, and high-temperature strength. The mechanical behavior of Nb-containing ferritic steels at service temperatures of 973 K (700 °C) and higher results from the convolution of dynamic microstructural changes including precipitation, precipitate coarsening, strain hardening, recovery, and recrystallization. The relative contributions of these competing processes have yet to be clarified. In this study, the high-temperature flow strength of an 18Cr-2Mo-0.5Nb ferritic stainless steel (SUS 444) was correlated with microstructure under different strain and initial precipitate distributions to clarify the relative role of the strengthening and softening processes. High-temperature tensile tests at 1023 K (750 °C) of un-aged (initial microstructure is precipitate-free) and pre-aged (initial microstructure contains precipitates) samples were carried out and transmission electron microscopy was used to assess dislocation distributions and precipitate morphology. The difference in the stress–strain curves between un-aged and pre-aged samples was drastic; the yield strength of the un-aged sample was twice that of the pre-aged sample, and the un-aged sample exhibits a noticeable yield drop. Transmission electron microscopy revealed a Laves phase nucleated and grew during the high-temperature tensile test in the un-aged sample and the majority of the precipitates in the pre-aged sample were the same Laves phase. Furthermore, a strain effect on precipitate growth was recognized in un-aged and pre-aged conditions by comparing grip (no strain) and gage (strained) sections of tensile samples. The dominant strengthening contribution in un-aged samples is initially the precipitate shearing mechanism and it changes to Orowan strengthening beyond the ultimate tensile strength, whereas the dominant contribution in the pre-aged samples appears to be Orowan strengthening throughout the stress–strain curve.
引用
收藏
页码:3460 / 3469
页数:9
相关论文
共 50 条
  • [41] A novel precipitation mechanism of Laves phase in Fe-30Cr-2Mo super ferritic stainless steel: In-situ phase transformation
    Zhu, Yangyang
    Ning, Likui
    Liu, Enze
    Zhou, Yangtao
    Tan, Zheng
    Tong, Jian
    Li, Haiying
    Zheng, Zhi
    MATERIALS LETTERS, 2023, 338
  • [43] Microstructure and mechanical properties of friction stir welded 18Cr-2Mo ferritic stainless steel thick plate
    Han, Jian
    Li, Huijun
    Zhu, Zhixiong
    Barbaro, Frank
    Jiang, Laizhu
    Xu, Haigang
    Ma, Li
    MATERIALS & DESIGN, 2014, 63 : 238 - 246
  • [44] Microstructure and mechanical properties of friction stir welded 18Cr-2Mo ferritic stainless steel thick plate
    Han, Jian
    Li, Huijun
    Zhu, Zhixiong
    Barbaro, Frank
    Jiang, Laizhu
    Xu, Haigang
    Ma, Li
    Materials and Design, 2014, 63 : 238 - 246
  • [45] Effects of W on microstructure and high-temperature oxidation behavior of ferritic stainless steel weldment
    Ji, Yijie
    Xie, Yuye
    Zhu, Shuangchun
    Yan, Biao
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2017, 31 (16-19):
  • [46] MICROSTRUCTURE EVOLUTION OF LAVES PHASE Cr2Nb/Cr ALLOYS PREPARED BY ARC MELTING
    Li Kewei
    Li Shuangming
    Fu Hengzhi
    ACTA METALLURGICA SINICA, 2011, 47 (06) : 663 - 670
  • [47] The effect of deformation temperature in metastable austenite zone on microstructure evolution, mechanical and corrosion properties of high Cr ferritic-martensitic steel
    Wang, Wanjun
    Wang, Xuan
    Lv, Yinghui
    Wu, Yingkun
    Chen, Jianguo
    KOVOVE MATERIALY-METALLIC MATERIALS, 2024, 62 (01): : 21 - 30
  • [48] HIGH-TEMPERATURE OXIDATION OF 1.25CR-0.5MO STEEL IN SO2
    WONGMORENO, AD
    LUISILLO, AB
    OXIDATION OF METALS, 1991, 35 (3-4): : 245 - 258
  • [49] A comprehensive study on the effect of high-temperature deformation level on microstructure development of austenitic stainless steel
    Rout, Matruprasad
    Ranjan, Ravi
    Anand, Kumar Aniket
    MATERIALS AT HIGH TEMPERATURES, 2025, 42 (01) : 25 - 38
  • [50] High-temperature Laves precipitation and its effects on recrystallisation behaviour and Luders deformation in super ferritic stainless steels
    Lu, Hui-Hu
    Guo, Hong-Kui
    Liang, Wei
    Li, Jian-Chun
    Zhang, Gang-Wang
    Li, Tao-Tao
    MATERIALS & DESIGN, 2020, 188