Studies on Stress Corrosion Cracking of Super 304H Austenitic Stainless Steel

被引:0
|
作者
B. Prabha
P. Sundaramoorthy
S. Suresh
S. Manimozhi
B. Ravishankar
机构
[1] NIT,
[2] WRI-BHEL,undefined
关键词
austenitic stainless steel Super 304H; chloride solution; EDAX; macrostructure; microstructure; SEM; strain;
D O I
暂无
中图分类号
学科分类号
摘要
Stress corrosion cracking (SCC) is a common mode of failure encountered in boiler components especially in austenitic stainless steel tubes at high temperature and in chloride-rich water environment. Recently, a new type of austenitic stainless steels called Super304H stainless steel, containing 3% copper is being adopted for super critical boiler applications. The SCC behavior of this Super 304H stainless steel has not been widely reported in the literature. Many researchers have studied the SCC behavior of steels as per various standards. Among them, the ASTM standard G36 has been widely used for evaluation of SCC behavior of stainless steels. In this present work, the SCC behavior of austenitic Fe-Cr-Mn-Cu-N stainless steel, subjected to chloride environments at varying strain conditions as per ASTM standard G36 has been studied. The environments employed boiling solution of 45 wt.% of MgCl2 at 155 °C, for various strain conditions. The study reveals that the crack width increases with increase in strain level in Super 304H stainless steels.
引用
收藏
页码:1294 / 1299
页数:5
相关论文
共 50 条
  • [31] Investigation of Stress Corrosion Cracking Initiation in Machined 304 Austenitic Stainless Steel in Magnesium Chloride Environment
    Zhang, Wenqian
    Wu, Huanchun
    Wang, Siyang
    Hu, Yujin
    Fang, Kewei
    Wang, Xuelin
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (01) : 191 - 204
  • [32] Investigation of Stress Corrosion Cracking Initiation in Machined 304 Austenitic Stainless Steel in Magnesium Chloride Environment
    Wenqian Zhang
    Huanchun Wu
    Siyang Wang
    Yujin Hu
    Kewei Fang
    Xuelin Wang
    Journal of Materials Engineering and Performance, 2020, 29 : 191 - 204
  • [33] Stress Corrosion Cracking of 304 Austenitic Stainless Steel in H2SO4/NaCl Media at Room Temperature
    Alshamsi, Ahmed S.
    CORROSION, 2024, 80 (09) : 910 - 921
  • [34] Carbon formation on stainless steel 304H in convection section of ethane cracking plant
    Ramezanipour, F.
    Singh, A.
    Paulson, S.
    Farag, H.
    Birss, V. I.
    Thangadurai, V.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2015, 50 (04) : 303 - 310
  • [35] The corrosion of austenitic 304 stainless steel in biodiesel
    Gallina, Andre Lazarin
    Stroparo, Erivelton Cesar
    da Cunha, Maico Taras
    Pinto Rodrigues, Paulo Rogerio
    REM-REVISTA ESCOLA DE MINAS, 2010, 63 (01) : 71 - 75
  • [36] Effect of Temperature on Reheat Cracking Susceptibility of Super304H Austenitic Stainless Steel Weld Metal
    Xiao Xiaopeng
    Dong Wenchao
    Li Dianzhong
    Li Yiyi
    Lu Shanping
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (07) : 2444 - 2452
  • [37] Effect of Temperature on Reheat Cracking Susceptibility of Super304H Austenitic Stainless Steel Weld Metal
    Xiao, Xiaopeng
    Dong, Wenchao
    Li, Dianzhong
    Li, Yiyi
    Lu, Shanping
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2023, 52 (07): : 2444 - 2454
  • [38] Stress corrosion cracking behaviour of gas tungsten arc welded super austenitic stainless steel joints
    Kumar, M. Vinoth
    Balasubramanian, V.
    Rajakumar, S.
    Albert, Shaju K.
    DEFENCE TECHNOLOGY, 2015, 11 (03): : 282 - 291
  • [39] Stress corrosion cracking behaviour of gas tungsten arc welded super austenitic stainless steel joints
    M.VINOTH KUMAR
    V.BALASUBRAMANIAN
    S.RAJAKUMAR
    SHAJU K.ALBERT
    Defence Technology, 2015, 11 (03) : 282 - 291
  • [40] Effect of surface machining on intergranular stress corrosion cracking (IGSCC) in sensitised type 304 austenitic stainless steel
    Rahimi, S.
    Mehrez, K.
    Marrow, T. J.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2016, 51 (05) : 383 - 391