Phase transformation during surface ablation of cobalt-cemented tungsten carbide with pulsed UV laser

被引:0
|
作者
T. Li
Q. Lou
J. Dong
Y. Wei
J. Liu
机构
[1] Shanghai Institute of Optics and Fine Mechanics,
[2] Chinese Academy of Sciences,undefined
[3] P.O. Box 800-211,undefined
[4] Shanghai,undefined
[5] 201800,undefined
[6] China,undefined
[7] Northwest Institute of Nuclear Technology,undefined
[8] P.O. Box 69-13,undefined
[9] Xi’an,undefined
[10] 710024,undefined
[11] China,undefined
来源
Applied Physics A | 2001年 / 73卷
关键词
PACS: 81.05.Bx; 81.65.Cf;
D O I
暂无
中图分类号
学科分类号
摘要
Surface ablation of cobalt-cemented tungsten carbide hard metal has been carried out in this work using a 308 nm, 20 ns XeCl excimer laser. Surface microphotography and XRD, as well as an electron probe have been used to investigate the transformation of phase and microstructure as a function of the pulse-number of laser shots at a laser fluence of 2.5 J/cm2. The experimental results show that the microstructure of cemented tungsten carbide is transformed from the original polygonal grains of size 3 μm to interlaced large, long grains with an increase in the number of laser shots up to 300, and finally to gross grains of size 10 μm with clear grain boundaries after 700 shots of laser irradiation. The crystalline structure of the irradiated area is partly transformed from the original WC to βWC1-x, then to αW2C and CW3, and finally to W crystal. It is suggested that the undulating ‘hill–valley’ morphology may be the result of selective removal of cobalt binder from the surface layer of the hard metal. The formation of non-stoichiometric tungsten carbide may result from the escape of elemental carbon due to accumulated heating of the surface by pulsed laser irradiation.
引用
收藏
页码:391 / 397
页数:6
相关论文
共 50 条
  • [21] In situ diagnosis of pulsed UV laser surface ablation of tungsten carbide hardmetal by using laser-induced optical emission spectroscopy
    Li, TJ
    Lou, QH
    Wei, YR
    Huang, F
    Dong, JX
    Liu, JR
    APPLIED SURFACE SCIENCE, 2001, 185 (1-2) : 114 - 122
  • [22] ROLE OF THE BINDER PHASE IN CEMENTED TUNGSTEN CARBIDE-COBALT ALLOYS
    GURLAND, J
    NORTON, JT
    JOURNAL OF METALS, 1952, 4 (10): : 1051 - 1056
  • [23] ROLE OF THE BINDER PHASE IN CEMENTED TUNGSTEN CARBIDE-COBALT ALLOYS
    GURLAND, J
    NORTON, JT
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1952, 194 (10): : 1051 - 1056
  • [24] Study of laser surface phase transition hardening quenching for high cobalt cemented carbide
    Wang, Sahngzhi
    Sun, Jing
    Tian, Nailiang
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 1998, 8 (01): : 89 - 94
  • [25] Nanosecond UV laser induced subsurface damage mechanics of cemented tungsten carbide
    Zhang, Quanli
    Chu, Chenglong
    Zhang, Zhen
    Zhu, Yandan
    CERAMICS INTERNATIONAL, 2021, 47 (23) : 32927 - 32937
  • [26] ROLE OF THE BINDER PHASE IN CEMENTED TUNGSTEN CARBIDE-COBALT ALLOYS - DISCUSSION
    FISCHER, RB
    GURLAND, J
    NORTON, JT
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1953, 197 (05): : 746 - 746
  • [27] Thin films deposited by femtosecond pulsed laser ablation of tungsten carbide
    De Bonis, A.
    Teghil, R.
    Santagata, A.
    Galasso, A.
    Rau, J. V.
    APPLIED SURFACE SCIENCE, 2012, 258 (23) : 9198 - 9201
  • [28] Nanosecond Laser Ablation Assisted Precision Grinding of WC/Co Cemented Tungsten Carbide
    Deng, Shibo
    Xia, Yongqi
    Wu, Mingtao
    Lei, Dajiang
    Zhang, Quanli
    INTERNATIONAL JOURNAL OF PRECISION ENGINEERING AND MANUFACTURING, 2025, 26 (02) : 283 - 294
  • [29] Artificial neural networks for surface modification of cobalt based tungsten cemented carbide deposits
    Jean, M. -D.
    Lin, B. -T.
    Wu, C. -S.
    SURFACE ENGINEERING, 2009, 25 (01) : 59 - 69
  • [30] Experimental and analytical investigation of cemented tungsten carbide ultra-short pulse laser ablation
    Urbina, J. P. Calderon
    Daniel, C.
    Emmelmann, C.
    LASERS IN MANUFACTURING (LIM 2013), 2013, 41 : 745 - 751