Onset of Hot Tearing in Ternary Mg-Al-Sr Alloy Castings

被引:0
|
作者
G. Cao
I. Haygood
S. Kou
机构
[1] University of Wisconsin–Madison,Department of Materials Science and Engineering
[2] University of Wisconsin–Madison,Department of Engineering Physics
[3] University of Wisconsin–Madison,Department of Materials Science and Engineering
关键词
Mold; Mold Wall; Load Curve; Thermal Arrest; Scheil Model;
D O I
暂无
中图分类号
学科分类号
摘要
Ternary Mg-Al-Sr alloys are the base of a few new creep-resistant, lightweight Mg alloys for automobiles. Hot tearing of Mg-Al-Sr alloys was studied by constrained rod casting (CRC) in a steel mold equipped with a load cell and a thermocouple. The alloys investigated included, in order of decreasing hot tearing susceptibility, Mg-4Al-1.5Sr, Mg-6Al-1.5Sr, Mg-8Al-1.5Sr, and Mg-8Al-3Sr. Two different molds were used, one for 8.7-mm-diameter rods and the other 7.9 mm. The cooling rate was varied by varying mold preheating from 523 K (250 °C) to 658 K (385 °C) and mold insulation. The load curve showed a clear peak when hot tearing occurred in all but Mg-8Al-3Sr due to its high resistance to hot tearing. From the peak and the cooling curve, the temperature at which hot tearing occurred was determined and found to decrease with increasing Al content from 4 to 8 pct. For a specific alloy, the hot tearing onset temperature did not change significantly with the rod diameter or mold preheating, at least within the experimental conditions used. The Scheil solidification model was used to estimate the fraction solid at the onset of hot tearing. It was found that hot tearing occurred near the end of primary solidification L → α (Mg) and that the fraction solid at which hot tearing occurred decreased with increasing Al content. The validity of the Scheil model was discussed.
引用
收藏
页码:2139 / 2150
页数:11
相关论文
共 50 条
  • [31] Effect of pressure levels on tensile properties of squeeze cast Mg-Al-Sr alloy
    Wang, Shuping
    Sun, Zhizhong
    Hu, Henry
    MAGNESIUM TECHNOLOGY 2008, 2008, : 421 - 425
  • [32] Effect of strontium content on porosity and tensile properties of squeeze cast Mg-Al-Sr alloy
    Zhang, Q.
    Wang, S. P.
    Hu, H.
    MATERIALS TECHNOLOGY, 2009, 24 (03) : 166 - 169
  • [33] Diecastability and properties of Mg-Al-Sr based alloys
    Argo, D
    Pekguleryuz, M
    Labelle, P
    Dierks, M
    Sparks, T
    Waltemate, T
    MAGNESIUM TECHNOLOGY 2001, 2001, : 131 - 136
  • [34] New developments in assessing hot tearing in magnesium alloy castings
    Bichler, L.
    Ravindran, C.
    MATERIALS & DESIGN, 2010, 31 : S17 - S23
  • [35] Hot-tearing susceptibility of Mg-9Al-xZn alloy
    Wang, YS
    Wang, QD
    Wu, GH
    Zhu, YP
    Ding, WJ
    MATERIALS LETTERS, 2002, 57 (04) : 929 - 934
  • [36] The Thermal Diffusivity of Mg-Al-Sr and Mg-Al-Ca-Sr Sand Casting Magnesium Alloys
    Kielbus, Andrzej
    Rzychon, Tomasz
    Moskal, Grzegorz
    DIFFUSION IN SOLIDS AND LIQUIDS VII, 2012, 326-328 : 249 - +
  • [37] Acoustic emission study of Mg-Al-Sr alloy reinforced with short Saffil® fibers deformed in compression
    Mathis, Kristian
    Farkas, Gergely
    Janecek, Milos
    Choe, Heeman
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 575 : 1 - 5
  • [38] Hot tearing behavior testing of Mg alloy
    Wang, Y.S.
    Zhang, Y.B.
    Ding, W.J.
    Wang, Q.D.
    Tezhong Zhuzao Ji Youse Hejin/Special Casting & Nonferrous Alloys, 2001, (03):
  • [39] Effect of Ca/Al ratio on hot tearing susceptibility of Mg-Al-Ca alloy
    Du, Xudong
    Wang, Feng
    Wang, Zhi
    Zhou, Le
    Wei, Ziqi
    Liu, Zheng
    Mao, Pingli
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 911
  • [40] Effect of extrusion on microstructures, and mechanical and creep properties of Mg-Al-Sr and Mg-Al-Sr-Ca alloys
    Jing, Bai
    Yangshan, Sun
    Feng, Xue
    Shan, Xue
    Jing, Qiang
    Tao Weijian
    SCRIPTA MATERIALIA, 2006, 55 (12) : 1163 - 1166