Onset of Hot Tearing in Ternary Mg-Al-Sr Alloy Castings

被引:0
|
作者
G. Cao
I. Haygood
S. Kou
机构
[1] University of Wisconsin–Madison,Department of Materials Science and Engineering
[2] University of Wisconsin–Madison,Department of Engineering Physics
[3] University of Wisconsin–Madison,Department of Materials Science and Engineering
关键词
Mold; Mold Wall; Load Curve; Thermal Arrest; Scheil Model;
D O I
暂无
中图分类号
学科分类号
摘要
Ternary Mg-Al-Sr alloys are the base of a few new creep-resistant, lightweight Mg alloys for automobiles. Hot tearing of Mg-Al-Sr alloys was studied by constrained rod casting (CRC) in a steel mold equipped with a load cell and a thermocouple. The alloys investigated included, in order of decreasing hot tearing susceptibility, Mg-4Al-1.5Sr, Mg-6Al-1.5Sr, Mg-8Al-1.5Sr, and Mg-8Al-3Sr. Two different molds were used, one for 8.7-mm-diameter rods and the other 7.9 mm. The cooling rate was varied by varying mold preheating from 523 K (250 °C) to 658 K (385 °C) and mold insulation. The load curve showed a clear peak when hot tearing occurred in all but Mg-8Al-3Sr due to its high resistance to hot tearing. From the peak and the cooling curve, the temperature at which hot tearing occurred was determined and found to decrease with increasing Al content from 4 to 8 pct. For a specific alloy, the hot tearing onset temperature did not change significantly with the rod diameter or mold preheating, at least within the experimental conditions used. The Scheil solidification model was used to estimate the fraction solid at the onset of hot tearing. It was found that hot tearing occurred near the end of primary solidification L → α (Mg) and that the fraction solid at which hot tearing occurred decreased with increasing Al content. The validity of the Scheil model was discussed.
引用
收藏
页码:2139 / 2150
页数:11
相关论文
共 50 条
  • [1] Onset of Hot Tearing in Ternary Mg-Al-Sr Alloy Castings
    Cao, G.
    Haygood, I.
    Kou, S.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (08): : 2139 - 2150
  • [2] Hot-Tearing Susceptibility of Ternary Mg-Al-Sr Alloy Castings
    G. Cao
    C. Zhang
    H. Cao
    Y.A. Chang
    S. Kou
    Metallurgical and Materials Transactions A, 2010, 41 : 706 - 716
  • [3] Hot-Tearing Susceptibility of Ternary Mg-Al-Sr Alloy Castings
    Cao, G.
    Zhang, C.
    Cao, H.
    Chang, Y. A.
    Kou, S.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2010, 41A (03): : 706 - 716
  • [4] Hot tearing of ternary Mg−Al−Ca alloy castings
    G. Cao
    S. Kou
    Metallurgical and Materials Transactions A, 2006, 37 : 3647 - 3663
  • [5] Hot tearing of ternary Mg-Al-Ca alloy castings
    Cao, G.
    Kou, S.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (12): : 3647 - 3663
  • [6] Effect of Sr/Al Ratio on Microstructure and Properties of Mg-Al-Sr Alloy
    Fan Jinping
    Xu Bingshe
    Wang Shebin
    Liu Lu
    Feng Zhiyong
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 (10) : 1721 - 1724
  • [7] Research on Corrosion Resistance of Mg-Al-Sr Alloy
    Wu, Tong
    Peng, Xiaodong
    Wang, Dongya
    Xie, Weidong
    MATERIALS RESEARCH, PTS 1 AND 2, 2009, 610-613 : 964 - 967
  • [8] A Research on the influence of Sr/Al ratio on microstructure of Mg-Al-Sr alloy
    Fan Jinping
    Wang Shebin
    Guo Duanyang
    Xu Bingshe
    ADVANCED MATERIALS, PTS 1-4, 2011, 239-242 : 2201 - +
  • [9] Effect of Sr/Al ratio on microstructure and properties of Mg-Al-Sr alloy
    Fan, Jinping
    Xu, Bingshe
    Wang, Shebin
    Liu, Lu
    Feng, Zhiyong
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2012, 41 (10): : 1721 - 1724
  • [10] Hot tearing susceptibility of binary Mg-Y alloy castings
    Wang, Zhi
    Huang, Yuanding
    Srinivasan, Amirthalingam
    Liu, Zheng
    Beckmann, Felix
    Kainer, Karl Ulrich
    Hort, Norbert
    MATERIALS & DESIGN, 2013, 47 : 90 - 100