Effect of heat treatments on Charpy impact properties of 15Cr12MoVWN ferritic/martensitic steel

被引:0
|
作者
Ting-wei Ma
Xian-chao Hao
Ping Wang
机构
[1] Northeastern University,Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education
[2] Yingkou Institute of Technology,CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research
[3] Chinese Academy of Sciences,undefined
来源
Journal of Iron and Steel Research International | 2022年 / 29卷
关键词
15Cr12MoVWN steel; Ductile-to-brittle transition temperature; Prior austenite grain size; M; C; MX;
D O I
暂无
中图分类号
学科分类号
摘要
The Charpy impact properties of 15Cr12MoVWN ferritic/martensitic steel for sodium-cooled reactors with variation in heat treatment factors and parameters are reported. The results show that the ductile-to-brittle transition temperature (DBTT) increased and the upper shelf energy (USE) decreased with increase in normalizing temperature. However, the variation tendency of DBTT and USE was the opposite with increase in tempering temperature. The tempering temperature showed a greater influence on USE than the normalizing temperature, and normalizing and tempering temperatures had the equally significant effects on DBTT, but the cooling method was not a significant factor for DBTT and USE. The prior austenite grain and M23C6 size were the main influences on DBTT, and the dislocation density was the main factor affecting the variation of USE. The heat-treatment regime recommended for 15Cr12MoVWN steel was composed of normalizing at 1000–1050 °C for 0.5 h followed by water quenching or air cooling and tempering at 760 °C for 1.5 h.
引用
收藏
页码:512 / 518
页数:6
相关论文
共 50 条
  • [21] Tensile and Charpy impact properties of an ODS ferritic/martensitic steel 9Cr-1.8W-0.5Ti-0.35Y2O3
    Zhang, Guangming
    Zhou, Zhangjian
    Wang, Man
    Li, Shaofu
    Zou, Lei
    Zhang, Liwei
    FUSION ENGINEERING AND DESIGN, 2014, 89 (04) : 280 - 283
  • [22] Microstructure and Charpy impact properties of 12-14Cr oxide dispersion-strengthened ferritic steels
    Oksiuta, Z.
    Baluc, N.
    JOURNAL OF NUCLEAR MATERIALS, 2008, 374 (1-2) : 178 - 184
  • [23] Charpy impact properties of martensitic 10.6% Cr steel (MANET-I) before and after neutron exposure
    Kernforschungszentrum Karlsruhe, G.m.b.H., Karlsruhe, Germany
    Fusion Eng Des, pt C (365-370):
  • [24] Environmental effect of steam on crack closure mechanisms of a 9-12% Cr ferritic/martensitic steel
    Fischer, T.
    Kuhn, B.
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 132
  • [25] Effect of Carbon Content on Microstructure and Mechanical Properties of 9 to 12 pct Cr Ferritic/Martensitic Heat-Resistant Steels
    Yin, Feng-Shi
    Tian, Li-Qian
    Xue, Bing
    Jiang, Xue-Bo
    Zhou, Li
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (07): : 2203 - 2209
  • [26] Effect of Carbon Content on Microstructure and Mechanical Properties of 9 to 12 pct Cr Ferritic/Martensitic Heat-Resistant Steels
    Feng-Shi Yin
    Li-Qian Tian
    Bing Xue
    Xue-Bo Jiang
    Li Zhou
    Metallurgical and Materials Transactions A, 2012, 43 : 2203 - 2209
  • [27] STRUCTURE EVOLUTION DURING HEAT-TREATMENTS OF 12-PERCENT CR MARTENSITIC STEEL FOR NET
    COPPOLA, R
    GONDI, P
    MONTANARI, R
    VENIALI, F
    JOURNAL OF NUCLEAR MATERIALS, 1988, 155 (616-619) : 616 - 619
  • [28] Impact of Thermomechanical Fatigue on Microstructure Evolution of a Ferritic-Martensitic 9 Cr and a Ferritic, Stainless 22 Cr Steel
    Kuhn, Bernd
    Lopez Barrilao, Jennifer
    Fischer, Torsten
    APPLIED SCIENCES-BASEL, 2020, 10 (18):
  • [29] Microstructure and Mechanical Properties of Heat-Resistant 12% Cr Ferritic-Martensitic Steel EK-181 after Thermomechanical Treatment
    Polekhina, N. A.
    Litovehenko, I. Yu.
    Tyurnentsev, A. N.
    Astafurova, E. G.
    Chernov, V. M.
    Leontyeva-Smirnova, M. V.
    INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS WITH HIERARCHICAL STRUCTURE FOR NEW TECHNOLOGIES AND RELIABLE STRUCTURES 2015, 2015, 1683
  • [30] Effect of isothermal heat treatment on microstructure and mechanical properties of Reduced Activation Ferritic Martensitic steel
    Chandravathi, K. S.
    Sasmal, C. S.
    Laha, K.
    Parameswaran, P.
    Nandagopal, M.
    Vijayanand, V. D.
    Mathew, M. D.
    Jayakumar, T.
    Kumar, E. Rajendra
    JOURNAL OF NUCLEAR MATERIALS, 2013, 435 (1-3) : 128 - 136