Ultrafine Ductile and Austempered Ductile Irons by Solidification in Ultrasonic Field

被引:2
|
作者
Ahmed, M. [1 ,2 ]
Riedel, E. [1 ]
Baehr, R.
Kovalko, M. [3 ]
Volochko, A. [3 ]
Nofal, A. [2 ]
机构
[1] Otto von Guericke Univ, Inst Mfg Technol & Qual Management, Univ Pl 2, D-39106 Magdeburg, Germany
[2] Cent Met Res & Dev Inst, Dept Foundry Technol, Cairo 11421, Egypt
[3] Natl Acad Sci, Phys Tech Inst, Kuprevich Str 10, Minsk 220141, BELARUS
关键词
ultrasonic melt treatment UST; spheroidal graphite iron; austempered ductile iron; dual-phase ADI alloys; CFD simulation; extremely fine graphite; ultrafine ausferrite structure; nodularity and nodule count; GRAPHITE NODULE COUNT; MECHANICAL-PROPERTIES; CAST-IRON; MICROSTRUCTURE; NODULARITY; KINETICS; MOLTEN;
D O I
10.1007/s40962-021-00683-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this research, ultrasonic melt treatment (UST) was used to produce a new ultrafine grade of spheroidal graphite cast iron (SG iron) and austempered ductile iron (ADI) alloys. Ultrasonic treatment was numerically simulated and evaluated based on acoustic wave streaming. The simulation results revealed that the streaming of the acoustic waves propagated as a stream jet in the molten SG iron along the centerline of the ultrasonic source (sonotrode) with a maximum speed of 0.7 m/s and gradually decreased to zero at the bottom of the mold. The metallographic analysis of the newly developed SG iron alloy showed an extremely ultrafine graphite structure. The graphite nodules' diameter ranging between 6 and 9 mu m with total nodule count ranging between 900 to more than 2000 nodules per mm(2), this nodule count has never been mentioned in the literature for castings of the same diameter, i.e., 40 mm. In addition, fully ferritic matrix was observed in all UST SG irons. Further austempering heat treatments were performed to produce different austempered ductile iron (ADI) grades with different ausferrite morphologies. The dilatometry studies for the developed ADI alloys showed that the time required for the completion of the ausferrite formation in UST alloys was four times shorter than that required for statically solidified SG irons. SEM micrographs for the ADI alloys showed an extremely fine and short ausferrite structure together with small austenite blocks in the matrix. A dual-phase intercritically austempered ductile iron (IADI) alloy was also produced by applying partial austenitization heat treatment in the intercritical temperature range, where austenite + ferrite + graphite phases coexist. In dual-phase IADI alloy, it was established that introducing free ferrite in the matrix would provide additional refinement for the ausferrite.
引用
收藏
页码:1463 / 1477
页数:15
相关论文
共 50 条
  • [41] Microstructural Evolutions and Properties of Partially Austenitizing and Austempered Ductile Irons
    Chen, Jhewn-Kuang
    Chen, Bi-Ting
    Tsai, Jui-Shen
    STEEL RESEARCH INTERNATIONAL, 2016, 87 (02) : 191 - 198
  • [42] Microstructural characteristics of Al-alloyed austempered ductile irons
    Kiani-Rashid, A. R.
    Edmonds, D. V.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 477 (1-2) : 391 - 398
  • [43] Machinability of martensitic and austempered ductile irons with dual matrix structure
    Sabzalipour, Mohsen
    Rashidi, A. M.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 6928 - 6941
  • [44] Influence of austenization temperature on the erosion behavior of austempered ductile irons
    Chang, L. C.
    Hsui, I. C.
    Chen, L. H.
    Lui, S. T.
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2008, 15 (01): : 29 - 33
  • [45] Cavitation erosion behavior of austempered ductile irons of increasing hardness
    Abreu, Marcio
    Elfsberg, Jessica
    Jonsson, Stefan
    WEAR, 2021, 484
  • [46] SOLIDIFICATION SEGREGATION AND ITS INFLUENCE ON AUSTEMPERED DUCTILE IRON
    GUNDLACH, RB
    JOURNAL OF METALS, 1987, 39 (07): : A61 - A61
  • [47] The solidification and corrosion behaviour of austempered chilled ductile iron
    Hemanth, J
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2000, 101 (1-3) : 159 - 166
  • [48] Solidification, Macrostructure and Shrinkage Formation of Ductile and Compacted Irons
    Boeri, Roberto E.
    Lopez, Marcos G.
    Tenaglia, Nicolas E.
    Massone, Juan M.
    INTERNATIONAL JOURNAL OF METALCASTING, 2020, 14 (04) : 1172 - 1182
  • [49] Solidification, Macrostructure and Shrinkage Formation of Ductile and Compacted Irons
    Roberto E. Boeri
    Marcos G. López
    Nicolás E. Tenaglia
    Juan M. Massone
    International Journal of Metalcasting, 2020, 14 : 1172 - 1182
  • [50] Comparison of High-Temperature Properties and Thermal Shock Resistance of Austempered Ductile Irons (ADI) with Those of Pearlitic Ductile Cast Irons
    Ajabshiri, Mehrdad
    Sharafi, Shahriar
    Moeini, Alireza
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2012, 43A (01): : 56 - 60