Wafer-level plasma activated bonding: new technology for MEMS fabrication

被引:0
|
作者
Viorel Dragoi
Gerald Mittendorfer
Christine Thanner
Paul Lindner
机构
[1] EV Group,
来源
Microsystem Technologies | 2008年 / 14卷
关键词
Chemical Mechanical Polishing; Wafer Bonding; Chemical Mechanical Polishing Process; Bare Silicon Wafer; Wafer Bonding Process;
D O I
暂无
中图分类号
学科分类号
摘要
Manufacturing and integration of MEMS devices by wafer bonding often lead to problems generated by thermal properties of materials. These include alignment shifts, substrate warping and thin film stress. By limiting the thermal processing temperatures, thermal expansion differences between materials can be minimized in order to achieve stress-free, aligned substrates without warpage. Achieving wafer level bonding at low temperature employs a little magic and requires new technology development. The cornerstone of low temperature bonding is plasma activation. The plasma is chosen to compliment existing interface conditions and can result in conductive or insulating interfaces. A wide range of materials including semiconductors, glasses, quartz and even plastics respond favorably to plasma activated bonding. The annealing temperatures required to create permanent bonds are typically ranging from room temperature to 400°C for process times ranging from 15–30 min and up to 2–3 h. This new technique enables integration of various materials combinations coming from different production lines.
引用
收藏
页码:509 / 515
页数:6
相关论文
共 50 条
  • [41] A Test IC for Wafer-Level Characterization of an IntraCMOS-MEMS Fabrication Process
    Linares Aranda, M.
    Hernandez Martinez, L.
    de la Hidalga Wade, F. J.
    IEEE LATIN AMERICA TRANSACTIONS, 2022, 20 (01) : 108 - 116
  • [42] Fabrication and Characterization of a Novel Wafer-level Chip Scale Package for MEMS Devices
    Cao, Yuhan
    Luo, Le
    2009 INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY & HIGH DENSITY PACKAGING (ICEPT-HDP 2009), 2009, : 5 - 8
  • [43] Adhesive wafer bonding using a molded thick benzocyclobutene layer for wafer-level integration of MEMS and LSI
    Makihata, M.
    Tanaka, S.
    Muroyama, M.
    Matsuzaki, S.
    Yamada, H.
    Nakayama, T.
    Yamaguchi, U.
    Mima, K.
    Nonomura, Y.
    Fujiyoshi, M.
    Esashi, M.
    JOURNAL OF MICROMECHANICS AND MICROENGINEERING, 2011, 21 (08)
  • [44] WAFER-LEVEL HERMETIC PACKAGING TECHNOLOGY FOR MEMS USING ANODICALLY-BONDABLE LTCC WAFER
    Tanaka, Shuji
    Matsuzaki, Sakae
    Mohri, Mamoru
    Okada, Atsushi
    Fukushi, Hideyuki
    Esashi, Masayoshi
    2011 IEEE 24TH INTERNATIONAL CONFERENCE ON MICRO ELECTRO MECHANICAL SYSTEMS (MEMS), 2011, : 376 - 379
  • [45] RF-MEMS wafer-level packaging using through-wafer via technology
    Tian, J.
    Iannacci, J.
    Sosin, S.
    Gaddi, R.
    Bartek, M.
    EPTC 2006: 8TH ELECTRONIC PACKAGING TECHNOLOGY CONFERENCE, VOLS 1 AND 2, 2006, : 441 - 447
  • [46] 3-D wafer-level packaging of MEMS using surface activated bonding and through-Si vias
    Takegawa, Yoshiyuki
    Kamakura, Masanao
    Baba, Toru
    Okudo, Takafumi
    Taura, Takumi
    Tomoida, Ryo
    Shiroishi, Hisanori
    Tone, Kaoru
    Saijo, Takashi
    IDW '07: PROCEEDINGS OF THE 14TH INTERNATIONAL DISPLAY WORKSHOPS, VOLS 1-3, 2007, : 1411 - 1414
  • [47] Wafer-level bonding/stacking technology for 3D integration
    Ko, Cheng-Ta
    Chen, Kuan-Neng
    MICROELECTRONICS RELIABILITY, 2010, 50 (04) : 481 - 488
  • [48] An innovative approach to wafer-level MEMS packaging
    Teomim, D
    Badihi, A
    Zilber, G
    SOLID STATE TECHNOLOGY, 2002, 45 (01) : 57 - +
  • [49] One micron precision, wafer-level aligned bonding for interconnect, MEMS and packaging applications
    Mirza, AR
    50TH ELECTRONIC COMPONENTS & TECHNOLOGY CONFERENCE - 2000 PROCEEDINGS, 2000, : 676 - 680
  • [50] Warpage Modeling and Characterization to Simulate the Fabrication Process of Wafer-Level Adhesive Bonding
    Lim, Ji-hyuk
    Ham, Suk-jin
    Jeong, Byung-gil
    32ND IEEE/CPMT INTERNATIONAL ELECTRONIC MANUFACTURING TECHNOLOGY SYMPOSIUM, 2007, : 186 - 190