Washout resistance of self-protected underwater concrete in freshwater and seawater

被引:24
|
作者
Nasr, Ahmed A. [1 ]
Chen, Songgui [2 ]
Jin, Feng [1 ]
机构
[1] Tsinghua Univ, State Key Lab Hydrosci & Engn, Beijing 100084, Peoples R China
[2] Tianjin Res Inst Water & Transport Engn, Xingang 2nd Rd, Tianjin, Peoples R China
基金
中国国家自然科学基金;
关键词
Self-protected underwater concrete (SPUC); Underwater protective agent (UPA); Washout; pH value test; Freshwater & Seawater; Aggregate segregation; COMPACTING CONCRETE; RHEOLOGICAL PROPERTIES; BOND STRENGTH; SLUMP FLOW; SUPERPLASTICIZER; PERFORMANCE; DOSAGE; TIME;
D O I
10.1016/j.conbuildmat.2021.123186
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this paper, the washout resistance of an innovative self-protected underwater concrete (SPUC) was tested under the influence of an underwater protective agent (UPA) in freshwater and seawater during the static case of water flow. The pervious methods of underwater concrete have been carried performed by incorporating the anti-washout admixtures (AWAs) into the proportions of concrete mix in order to make the mixture coherent during the placing of underwater concrete, but the UPA technique depends on changing the characteristics of the water to make it suitable for receiving fresh self-compacted concrete (SCC) without leakage into water. An experimental program consisted of 20 mixes was conducted by using 4 tests: non-dispersion test (US Army Corp CRD C61), slump, and slump flow (SF), and pH value test to investigate the behavior of concrete during placing the concrete underwater. These experiments were implemented based on five parameters: UPA concentration, W/C ratio, superplasticizer (SP) content, fine aggregate (FA) ratio, and water environment. Test results showed that the washout was decreased by increasing the UPA concentration. Mass losses also were increased by increasing the W/C ratio or SP and decreased by increasing the fine aggregate ratio. Besides, seawater showed higher resistance to washout than freshwater. On the other hand, the pH test was shown to be compatible with the results of the CRD C61 test. However, freshwater specimens achieved higher pH values than seawater because freshwater was more alkaline. Furthermore, the relationship between D loss of mass and D pH tests was induced between UPA and UPA-free. Finally, it was concluded that the recommendations relating to the SPUC proportions should be concluded in the technical guideline on SPUC. (c) 2021 Elsevier Ltd. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Self-protected Scheme for Wavelength Reusable WDM Passive Optical Networks
    Fan, Peng
    Chen, Hongwei
    Chen, Minghua
    Xie, Shizhong
    2011 OPTICAL FIBER COMMUNICATION CONFERENCE AND EXPOSITION (OFC/NFOEC) AND THE NATIONAL FIBER OPTIC ENGINEERS CONFERENCE, 2011,
  • [42] Application of factorial models to predict the effect of anti-washout admixture, superplasticizer and cement on slump, flow time and washout resistance of underwater concrete
    ACM Advanced Concrete and Masonry Centre, Department of Civil, Structural and Environmental Engineering, University of Paisley, United Kingdom
    Materials and Structures/Materiaux et Constructions, 2000, 33 (05): : 317 - 323
  • [43] Application of factorial models to predict the effect of anti-washout admixture, superplasticizer and cement on slump, flow time and washout resistance of underwater concrete
    Sonebi, M
    Tamimi, AK
    Bartos, PJM
    MATERIALS AND STRUCTURES, 2000, 33 (229) : 317 - 323
  • [44] Application of factorial models to predict the effect of anti-washout admixture, superplasticizer and cement on slump, flow time and washout resistance of underwater concrete
    M. Sonebi
    A. K. Tamimi
    P. J. M. Bartos
    Materials and Structures, 2000, 33 : 317 - 323
  • [45] Experimental Studies on the Seismic Performance of Underwater Concrete Piers Strengthened by Self-Stressed Anti-Washout Concrete and Segments
    Sun, Yu
    Xu, Wansong
    Shen, Sheng
    APPLIED SCIENCES-BASEL, 2023, 13 (21):
  • [46] Self-protected high-temperature superconducting demonstrator magnet for particle detectors
    Van den Eijnden, Joep L.
    Vaskuri, Anna K.
    Cure, Benoit
    Dudarev, Alexey
    Mentink, Matthias
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2024, 37 (01):
  • [47] ICeGaNTM technology: The easy-to-use and self-protected GaN power IC
    Longobardi G.
    Efthymiou L.
    Findlay J.
    Bricconi A.
    Comiskey P.
    Arnold M.
    Miller D.
    Udrea F.
    Power Electronic Devices and Components, 2023, 4
  • [48] A self-protected architecture for wavelength-division-multiplexed passive optical networks
    Chan, TJ
    Chan, CK
    Chen, LK
    Tong, F
    IEEE PHOTONICS TECHNOLOGY LETTERS, 2003, 15 (11) : 1660 - 1662
  • [49] Robust ESD Self-Protected LDNMOSFET by an Enhanced Displacement-Current Triggering
    Kao, Tzu-Cheng
    Lien, Chen-Hsin
    Chiu, Chien-Wei
    Lee, Jian-Hsing
    Lo, Yen-Hsiang
    Hung, Chung-Yu
    Huang, Tsung-Yi
    Su, Hung-Der
    2015 IEEE INTERNATIONAL RELIABILITY PHYSICS SYMPOSIUM (IRPS), 2015,
  • [50] The Mix Ratio Study of Self-Stressed Anti-Washout Underwater Concrete Used in Nondrainage Strengthening
    Wu, Shaofeng
    Jiang, Shao-Fei
    Shen, Sheng
    Wu, Zhaoqi
    MATERIALS, 2019, 12 (02)