Optical Microspectroscopy Study of the Mechanical Stability of Empty and Filled Carbon Nanotubes under Hydrostatic Pressure

被引:12
|
作者
Anis, Badawi [1 ]
Boerrnert, F. [2 ,3 ]
Ruemmeli, M. H. [2 ]
Kuntscher, C. A. [1 ]
机构
[1] Univ Augsburg, D-86159 Augsburg, Germany
[2] IFW Dresden, D-01171 Dresden, Germany
[3] Tech Univ Dresden, Speziallab Triebenberg, D-01062 Dresden, Germany
来源
JOURNAL OF PHYSICAL CHEMISTRY C | 2014年 / 118卷 / 46期
关键词
RADIAL-BREATHING MODE; ELECTRONIC-PROPERTIES; RAMAN-SCATTERING; ELASTIC PROPERTIES; PHASE-TRANSITION; FULLERENE C-70; BUNDLES; IODINE; PEAPODS; C-60;
D O I
10.1021/jp506922s
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
We present a high-pressure optical and infrared spectroscopy study on the mechanical stability of single-walled carbon nanotubes (SWCNTs) filled with C-60 and C-70 fullerene molecules (C-60- and C-70-peapods), double-walled carbon nanotubes (DWCNTs) derived from the C-60- and C-70-peapods (DWCNTs/C-60 and DWCNTs/C-70), and iodine-filled SWCNTs (I-SWCNTs). High-resolution transmission electron microscopy, Raman, and optical spectroscopy were used to characterize all prepared samples. For the C-60- and C-70-peapods, we find an anomaly in the pressure-induced shifts of the optical transitions at the critical pressures P-c1 approximate to 6.5 and 7.0 GPa, respectively, compared to P-c1 approximate to 3 GPa in the case of empty SWCNTs. The shift of the anomaly to higher pressure signals the stabilization of the nanotubes by the C-60 and C-70 filling. The value of P-c1 is in good agreement with theoretical predictions of the pressure-induced deformation for highly filled peapods with similar average diameter. In comparison to SWCNTs, the pressure-induced red shifts of the optical transitions in DWCNTs/C-60 are extremely small below similar to 10 GPa, demonstrating the enhanced mechanical stability due to the inner tube. The anomaly at the critical pressure P-d approximate to 12 GPa in DWCNTs/C-60 signals the onset of the pressure-induced deformation of the tubular cross sections or the collapse of the DWCNTs. For the DWCNTs/C70, the anomaly in the pressure-induced shift is lowered to P-d approximate to 9 GPa compared to 12 GPa in the case of DWCNTs/C-60. This behavior signals that the stabilization of the outer tube by the inner tube in DWCNTs/C-70 is lower compared to the DWCNTs/C-60. Interestingly, the iodine filling shows a stabilization for the outer tubes up to 10 GPa in contrast with the previously published Raman results. For all samples, except I-SWCNTs, the low energy absorbance decreases rapidly with increasing pressure, suggesting the destruction of the SWCNT electronic band structure and hence an increasing carrier localization. In the I-SWCNTs the pressure-induced free carriers localization is partially compensated by the metallization of the iodine chains under pressure.
引用
收藏
页码:27048 / 27062
页数:15
相关论文
共 50 条
  • [31] Elastic properties of carbon nanotubes under hydrostatic pressure -: art. no. 153407
    Reich, S
    Thomsen, C
    Ordejón, P
    PHYSICAL REVIEW B, 2002, 65 (15) : 1 - 4
  • [32] Electrophysical properties of composite films based on multiwalled carbon nanotubes under hydrostatic pressure
    Arslanov T.R.
    Babaev A.A.
    Arslanov R.K.
    Khokhlachev P.P.
    Terukov E.I.
    Filippov A.K.
    Bulletin of the Russian Academy of Sciences: Physics, 2015, 79 (6) : 755 - 758
  • [33] Tensile strength of single-walled carbon nanotubes with defects under hydrostatic pressure
    Xia, YY
    Zhao, MW
    Ma, YC
    Ying, MJ
    Liu, XD
    Liu, PJ
    Mei, LM
    PHYSICAL REVIEW B, 2002, 65 (15) : 1 - 7
  • [34] Double-walled carbon nanotubes under hydrostatic pressure: Raman experiments and simulations
    Gadagkar, Vikram
    Saha, Surajit
    Muthu, D. V. S.
    Maiti, Prabal K.
    Lansac, Yves
    Jagota, A.
    Moravsky, Alexander
    Loutfy, R. O.
    Sood, A. K.
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2007, 7 (06) : 1753 - 1759
  • [35] Influence of filling atoms on radial collapse and elasticity of carbon nanotubes under hydrostatic pressure
    Han, Zhi-De
    Ling, Cui-Cui
    Guo, Qi-Kai
    Lu, Hai-Peng
    Sui, Hong-Guang
    Yin, Jiao-Jian
    Deng, Long-Jiang
    SCIENCE BULLETIN, 2015, 60 (17) : 1509 - 1516
  • [36] Photoluminescence study of aqueous-surfactant-wrapped single-walled carbon nanotubes under hydrostatic pressure
    Deacon, R. S.
    Chuang, K. -C.
    Doig, J.
    Mortimer, I. B.
    Nicholas, R. J.
    PHYSICAL REVIEW B, 2006, 74 (20):
  • [37] Theoretical modeling relating to temperature and cap/end for carbon nanotubes under hydrostatic pressure
    Gao, Ming
    Bian, Lichun
    ZAMM-ZEITSCHRIFT FUR ANGEWANDTE MATHEMATIK UND MECHANIK, 2020, 100 (04):
  • [38] Effect of functional groups on the radial collapse and elasticity of carbon nanotubes under hydrostatic pressure
    Ling, Cuicui
    Xue, Qingzhong
    Jing, Nuannuan
    Xia, Dan
    NANOSCALE, 2012, 4 (13) : 3894 - 3900
  • [39] Influence of filling atoms on radial collapse and elasticity of carbon nanotubes under hydrostatic pressure
    Zhi-De Han
    Cui-Cui Ling
    Qi-Kai Guo
    Hai-Peng Lu
    Hong-Guang Sui
    Jiao-Jian Yin
    Long-Jiang Deng
    ScienceBulletin, 2015, 60 (17) : 1509 - 1516
  • [40] The tunable mechanical property of water-filled carbon nanotubes under an electric field
    Ye, Hongfei
    Zhang, Zhongqiang
    Zhang, Hongwu
    Chen, Zhen
    Zong, Zhi
    Zheng, Yonggang
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2014, 47 (12)