Interactions at the head-tape interface of a linear tape system

被引:7
|
作者
Hempstock, MS [1 ]
Wild, MA [1 ]
Sullivan, JL [1 ]
机构
[1] Aston Univ, Sch Engn & Appl Sci, Surface Sci Res Grp, Birmingham B4 7ET, W Midlands, England
关键词
linear; media; tribology;
D O I
10.1016/S0301-679X(00)00059-1
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Ln this study, tape cycling experiments were performed using two different experimental metal particle media in combination with a Travan(TM) linear tape system. The aim was to investigate the effect of head/tape contact on the tribological properties and signal performance of the system. A combination of cycling at extreme environmental conditions, use of experimental media, and cycling beyond the normal limit of operation ensured a worst-case scenario for the head-tape interactions. Auger electron spectroscopy (AES) and atomic force microscopy (AFM) were used to characterize the chemical and physical surface changes that occurred on and in the head surfaces. X-ray photoelectron spectroscopy (XPS) was used to identify the chemical changes that occurred at the media surface and these changes were correlated to variation in signal dropout rate. Measurements were made as functions of number of cycles. The cycling experiments for the two different tapes were performed at conditions of 32 degrees C, 80% RH and 5 degrees C, 10% RH and transfer of material from the media to the head was observed at each condition for both tape types. The degree of material transfer was influenced by the environmental operating conditions, but was governed by localized heating effects, such as those originating from active magnetoresistive (MR) elements and frictional interactions between the head and media. XPS analyses of the surface of the media revealed a reduction of nitrogen with increasing number of cycles indicating binder depletion, Significant differences in elemental concentrations were also detected between areas corresponding to regions directly under the cartridge belt compared to those off belt. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:391 / 399
页数:9
相关论文
共 50 条
  • [41] HEAD/TAPE INTERFACE PRESSURE CONTROL USING VACUUM.
    Clurman, Stanley Paul
    Herzog, Donald George
    RCA technical notes, 1983, (1323):
  • [42] Durability studies of metal evaporated tapes in a linear tape drive: Role of head contour and tape tension
    Anton V. Goldade
    B. Bhushan
    Microsystem Technologies, 2005, 11 : 32 - 47
  • [43] Head/tape spacing measurements for digital linear tape drives using three-color interferometry
    Tan, SW
    Garrettson, B
    Talke, FE
    Kneeburg, D
    Judge, J
    TRIBOLOGY TRANSACTIONS, 2000, 43 (01) : 144 - 150
  • [44] TAPE HEAD AMPLIFIER
    不详
    ELECTRONICS WORLD & WIRELESS WORLD, 1990, 96 (1649): : 250 - 250
  • [45] CAPACITANCE PROBE STUDY OF ROTATING-HEAD-TAPE INTERFACE
    FELISS, NA
    TALKE, FE
    IBM JOURNAL OF RESEARCH AND DEVELOPMENT, 1977, 21 (03) : 289 - 293
  • [46] Algorithms for extraction of spacing information from a head/tape interface
    Swain, R
    Baugh, E
    Talke, F
    OPTICS AND LASERS IN ENGINEERING, 1997, 27 (03) : 309 - 320
  • [47] Advanced Magnetic Tape Technology for Linear Tape Systems
    Shimizu, Osamu
    Harasawa, Takeshi
    Noguchi, Hitoshi
    2014 30TH SYMPOSIUM ON MASSIVE STORAGE SYSTEMS AND TECHNOLOGIES (MSST), 2014,
  • [48] Finite element analysis of tape-head interface phenomena of VCR
    Matsushita Electric Industrial Co, Ltd, Osaka, Japan
    JSME Int J Ser C, 3 (609-616):
  • [49] Wear mechanisms at the metal evaporated magnetic tape-head interface
    Berar, P
    Kato, K
    Osaki, H
    Terazono, T
    Kapsa, P
    JOURNAL OF TRIBOLOGY-TRANSACTIONS OF THE ASME, 1999, 121 (02): : 408 - 415
  • [50] Measurement and origin of tape edge damage in a linear tape drive
    Goldade, AV
    Bhushan, B
    TRIBOLOGY LETTERS, 2003, 14 (03) : 167 - 180