Magnetic domains and coercivity in SmCo 2:17 type magnets

被引:8
|
作者
Gutfleisch, O. [1 ]
Mueller, K. -H. [1 ]
Wolf, M. [1 ]
Khlopkov, K. [1 ]
Yan, A. [1 ]
Schaefer, R. [1 ]
Gemming, T. [1 ]
Schultz, L. [1 ]
机构
[1] IFW Dresden, Inst Met Mat, D-01171 Dresden, Germany
关键词
SmCo alloy; permanent magnet; coercivity; magnetic interaction domain; magnetic force microscopy;
D O I
10.1016/S1006-706X(08)60160-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The coercivity of SmCo 2:17-type magnets is known to be very sensitive to details of the processing procedure. In this study we have found that the same is true with respect to the domain structure of these magnets. Thus in optimally processed high temperature Sm(Co0.784Fe0.1Cu0.088Zr0.028)(7.19) magnets, the typical domain width is less than 1 mu m, but significantly larger than the typical size of 2:17R cells of about 100 nm. On the other hand, quenching straight from the aging temperature of 850 degrees C, i.e. omitting slow cooling, leads to a much coarser domain structure (domain width similar to 10 mu m) and a small coercivity (< 0.1 T). The fine domain structure of the optimally processed bulk magnet can be considered as interaction domains - an alternative phenomenon compared to the zigzag shaped domain walls known for thinned specimen.
引用
收藏
页码:48 / 59
页数:12
相关论文
共 50 条
  • [11] Influence of exchange coupling interaction on coercivity in 2:17-type SmCo-based high temperature permanent magnets
    Xu, Hao
    Wang, Hui
    Xi, Longlong
    Liu, Bingjie
    Du, Kangzhe
    Gao, Hao
    Liu, Jinghua
    Zhang, Tianli
    Jiang, Chengbao
    SCRIPTA MATERIALIA, 2023, 222
  • [12] Coercivity and magnetic anisotropy of sintered Sm2Co17-type permanent magnets
    TellezBlanco, JC
    Kou, XC
    Grossinger, R
    EstevezRams, E
    Fidler, J
    Ma, BM
    JOURNAL OF APPLIED PHYSICS, 1997, 82 (08) : 3928 - 3933
  • [13] Effect of solution temperature on the microstructure of 2:17 type SmCo magnets
    Zhang, Chen
    Ren, Shaoqing
    Lv, Ke
    Zhao, Mingjing
    Li, Yan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1003
  • [14] Modeling the coercivity of 2:17 magnets
    Kronmüller, H
    RARE EARTH MAGNETS AND THEIR APPLICATIONS, 2002, : 804 - 813
  • [15] Review of research on 2:17 type SmCo rare earth permanent magnets
    Yi, JH
    Peng, YD
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (04) : 337 - 342
  • [16] Chemical composition and coercivity of SmCo5 magnets
    de Campos, MF
    Landgraf, FJG
    Saito, NH
    Romero, SA
    Neiva, AC
    Missell, FP
    de Morais, E
    Gama, S
    Obrucheva, EV
    Jalnin, BV
    JOURNAL OF APPLIED PHYSICS, 1998, 84 (01) : 368 - 373
  • [17] Magnetic texture and coercivity of anisotropic nanocrystalline SmCo6.1Si0.9 magnets
    An, Shizhong
    Zhang, Tianli
    Jiang, Chengbao
    JOURNAL OF APPLIED PHYSICS, 2014, 115 (17)
  • [19] Coercivity of 2:17 based permanent magnets
    Kronmueller, H.
    Goll, D.
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2006, 13 : 39 - 47
  • [20] Kinetic studies of hydrogen desorption in SmCo 2/17-type sintered magnets
    Zakotnik, M.
    Prosperi, D.
    Williams, A. J.
    THERMOCHIMICA ACTA, 2009, 486 (1-2) : 41 - 45