Microstructure and deformability of Sn-Zn-Bi alloys

被引:0
|
作者
Zhou Jian [1 ]
Li Peipei [1 ]
Xiao Yingying [1 ]
Fu xiaoqing [1 ]
机构
[1] Southeast Univ, Dept Mat Sci & Engn, Nanjing 210096, Peoples R China
关键词
D O I
暂无
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
With addition of Bi, wettability of Sn-Zn alloys can be obviously improved. As a low melting point alloy, it is expected that Sn-Zn-Bi alloy come to being one of commercial solders. But, there is an unfavorable effect on plasticity of Sn-Zn-Bi alloys by adding Bi, so Bi concentration is usually required below 5mass% to maintain the alloys enough elongation. This alloying method can not match with the demand for satisfactory wettability. For example, wettabilty of typical Sn-8Zn-3Bi alloy is not good enough for air condition. This solder usually needs nitrogen atmosphere help it wet on substrate. Embrittlement of Sn-Zn-Bi alloy must be solved before it can be deformed into solder wire. In this paper, effect of microstructure evolution on elongation of Sn-Zn-Bi alloys has been investigated. Adding Bi into Sn-9Zn, primary Zn phase dispersed in eutectic matrix. With addition of Bi, quantity and size of the coarse plate Zn phase in those alloys have increased, and then elongation of the alloys has decreased. Adding 4mass% Bi into Sn-9Zn, elongation of the alloy is below 8%. Fracture analysis shows that intergranular crack is liable to occur along with the interface between primary Zn and matrix. The weak cohesion between primary Zn and matrix cause decrease of elongation. To restrain primary Zn phase from forming, Zn concentration of Sn-Zn-Bi alloys has been deduce. Results display that Sn-Zn-Bi alloys without primary Zn phase obtain higher deformability.. Elongation of Sn-6Zn-6Bi alloy is above 8%.
引用
收藏
页码:311 / +
页数:2
相关论文
共 50 条
  • [21] Microstructure of Rapidly Solidified Alloys of the Sn-Zn-Bi-In System
    Gusakova, O. V.
    Shepelevich, V. G.
    PHYSICS OF METALS AND METALLOGRAPHY, 2018, 119 (05): : 482 - 490
  • [22] Effect of interfacial microstructure on joint strength between Sn-Ag-Cu and Sn-Zn-Bi solders and Cu substrate
    Hirose, A
    Yanagawa, H
    Ide, E
    Kobayashi, KF
    Electronics Goes Green 2004 (Plus): Driving Forces for Future Electronics, Proceedings, 2004, : 363 - 368
  • [23] WETTING PROPERTIES OF Sn-Pb, Sn-Zn AND Sn-Zn-Bi LEAD-FREE SOLDERS
    Mayappan, Ramani
    Ismail, Ahmad Badri
    Ahmad, Zainal Arifin
    Ariga, Tadashi
    Hussain, Luay Bakir
    JURNAL TEKNOLOGI, 2007, 46
  • [24] Effect of Bi contents on joint strength between Sn-Pb plating and Sn-Zn-Bi solder
    Tsujiguchi, Masato
    Tanigawa, Masanobu
    Mimatsu, Takaaki
    Yamada, Takayuki
    Shapu Giho/Sharp Technical Journal, 2006, (94): : 62 - 67
  • [25] ON THE CHARACTERIZATION OF THE MATERIAL AND THE DEFORMABILITY OF SN-ZN ALLOYS
    SCHLEGEL, J
    HENNIG, W
    HENSGER, KE
    NEUE HUTTE, 1985, 30 (04): : 146 - 150
  • [26] Fatigue reliability evaluation for Sn-Zn-Bi and Sn-Zn lead-free solder joints
    Yu, Q
    Jin, JC
    Kim, DS
    Shiratori, M
    MATERIALS TRANSACTIONS, 2005, 46 (11) : 2316 - 2321
  • [27] Correlation between interfacial microstructure and shear behavior of Sn-Ag-Cu solder ball joined with Sn-Zn-Bi paste
    Shih, Po-Cheng
    Lin, Kwang-Lung
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (08) : 2574 - 2581
  • [28] Sn-Zn-Bi无铅钎料的研究现状
    赵东升
    焊接, 2014, (01) : 47 - 53+70
  • [29] Sn-Zn-Bi无铅钎料成分设计
    吴文云
    邱小明
    孙大谦
    刘卫红
    李明高
    不详
    吉林大学学报(工学版) , 2004, (04) : 538 - 543
  • [30] Retardation of spalling by the addition of Ag in Sn-Zn-Bi solder with the Au/Ni metallization
    Sharif, A.
    Chan, Y. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 445 : 686 - 690