IMPROVEMENT OF WELD METAL TOUGHNESS IN HIGH HEAT INPUT ELECTRO-SLAG WELDING OF LOW CARBON STEEL

被引:8
|
作者
Kitani, Y. [1 ]
Ikeda, R. [1 ]
Ono, M. [1 ]
Ikeuchi, K. [2 ]
机构
[1] JFE Steel Corp, Joining & Strength Res Dept, Steel Res Lab, Chiba, Japan
[2] Osaka Univ, JWRI, Ibaraki, Japan
关键词
Boron; Defects; Electroslag welding; Ferrite; Fluxes; Gases; Grain boundaries; Inclusions; Mechanical properties; Oxygen; Reference lists; Toughness; Weld metal; Welding fluxes; C-MN STEEL; ACICULAR FERRITE; NUCLEATION; INCLUSIONS; BORON;
D O I
10.1007/BF03266704
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In recent years, important steel structures of high-rise buildings such as the box columns required high toughness of welded joints considering the shockproof against the large-scale earthquake. In Japan, there are some specifications that demand Charpy impact energy more than 70 J at 0 degrees C in any welded joints. However in high heat input electro-slag welding, the microstructure of the weld metal becomes very coarse and weld metal toughness is remarkably deteriorated. In this paper, authors tried to form fully acicular ferrite microstructure in the weld metal of high heat input electro-slag welding to improve the weld metal toughness. High heat input (approximately 100 kJ/mm) electro-slag welding was carried out in the 60 mm thickness steel plate joint. Applying high Ti bearing welding wire and low basicity welding flux provided the weld metal with acicular ferrite microstructure, because large amounts of Ti containing oxide inclusions which were known as effective nucleation sites for acicular ferrite formations were dispersed in the weld metal. B addition to the weld metal suppressed the formation of coarse grain boundary ferrite when B/N ratio in the weld metal ranged between 0.5 and 0.8. When B/N ratio in the weld metal exceeded 0.8, the weld metal toughness was deteriorated due to an increase of M-A constituent. Consequently it was possible that fully acicular ferrite microstructure was formed in the weld metal of high heat input electro-slag welding and achieved the excellent weld metal toughness (vE(0) > 100 J).
引用
收藏
页码:R57 / R63
页数:7
相关论文
共 50 条
  • [21] Improvement of Heat-Affected Zone Toughness of Steel Plates for High Heat Input Welding by Inclusion Control with Ca Deoxidation
    Wang, Ruizhi
    Yang, Jian
    Xu, Longyun
    METALS, 2018, 8 (11)
  • [22] STUDY ON IMPROVEMENT OF HAZ TOUGHNESS OF STEEL FOR LOW-TEMPERATURE SERVICE .1. BASIC PRINCIPLE OF IMPROVEMENT OF HAZ TOUGHNESS OF STEEL FOR LOW-TEMPERATURE SERVICE UNDER HIGH HEAT INPUT WELDING CONDITION
    KAWASHIMA, Y
    MATSUDA, S
    ONO, Y
    OKAMURA, Y
    SATO, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1982, 22 (12) : B400 - B400
  • [23] INCREASE IN THE TOUGHNESS OF THE WELD METAL ZONE IN THE ARC-WELDING OF A HEAT-TREATED STEEL
    TITOV, NY
    WELDING PRODUCTION, 1978, 25 (11): : 30 - 32
  • [24] Effect of heat input on the microstructure and impact toughness of submerged arc weld metal for high-performance weathering steel
    Li, Fangmin
    Li, Jinjian
    Hu, Bing
    Yi, Yuzhu
    Wang, Qiuming
    Wang, Qingfeng
    MATERIALS RESEARCH EXPRESS, 2023, 10 (09)
  • [25] IMPROVEMENT OF TOUGHNESS OF Cr-Mo STEEL WELD METAL AT LOW TEMPERATURE.
    Yamamoto, Shigeaki
    Natsume, Syogo
    Welding and Metal Fabrication, 1986, 54 (03): : 110 - 111
  • [26] Microstructure and corrosion characterization of weld metal in stainless steel and low carbon steel joint under different heat input
    Huang, Yanqin
    Huang, Jankang
    Zhang, Jianxiao
    Yu, Xiaoquan
    Li, Qi
    Wang, Zhen
    Fan, Ding
    MATERIALS TODAY COMMUNICATIONS, 2021, 29
  • [27] Evaluation of the AISI 904L Alloy Weld Overlays Obtained by GMAW and Electro-Slag Welding Processes
    Jorge, Jorge C. F.
    Meira, O. G.
    Madalena, F. C. A.
    de Souza, L. F. G.
    Araujo, L. S.
    Mendes, M. C.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (05) : 2204 - 2212
  • [28] Evaluation of the AISI 904L Alloy Weld Overlays Obtained by GMAW and Electro-Slag Welding Processes
    Jorge C. F. Jorge
    O. G. Meira
    F. C. A. Madalena
    L. F. G. de Souza
    L. S. Araujo
    M. C. Mendes
    Journal of Materials Engineering and Performance, 2017, 26 : 2204 - 2212
  • [29] Effect of heat input on weld microstructure and toughness of laser-arc hybrid welding of martensitic stainless steel
    Hao, Kangda
    Zhang, Chen
    Zeng, Xiaoyan
    Gao, Ming
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2017, 245 : 7 - 14
  • [30] Effect of Heat Input on Geometry of Austenitic Stainless Steel Weld Bead on Low Carbon Steel
    Saha M.K.
    Hazra R.
    Mondal A.
    Das S.
    Journal of The Institution of Engineers (India): Series C, 2019, 100 (04) : 607 - 615