Impact of preheating on the mechanical performance of different MgO-C bricks?Intermediate temperature range

被引:13
|
作者
Gass, Sebastian E. [1 ]
Galliano, Pablo G. [2 ]
Tomba Martinez, Analia G. [1 ]
机构
[1] UNMdP, CONICET, Fac Ingn, Inst Invest Ciencia & Tecnol Mat INTEMA, Av JB Juste 4302, RA-7600 Mar Del Plata, Argentina
[2] Tenaris Siderca, Dr Simini 250, RA-2804 Campana, Argentina
关键词
MgO-C refractories; Mechanical behavior; Thermal treatment; Intermediate temperature; MAGNESIA-GRAPHITE REFRACTORIES; THERMAL-SHOCK RESISTANCE; CHEMICAL-REACTIONS; BEHAVIOR; MICROSTRUCTURE; BRICKS;
D O I
10.1016/j.jeurceramsoc.2021.01.025
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This work analyses the mechanical behavior of MgO-C refractories at an intermediate temperature of 1000 ?C. Conditions similar to those occurring during the in-service pre-heating of steelmaking ladles are simulated by thermal treatment before the mechanical testing. Stress-strain curves were determined under compressive loading at RT and 1000 ?C. The impact of the thermally activated physicochemical transformations on the mechanical response of the materials was evaluated in terms of parameters such as strength, fracture deformation, secant modulus and yield strength. The presence of Al seems to be deleterious when longer soaking times at 1000 ?C were applied, which was attributed to the progressive damage related to in situ phase formation. On the other hand, when heating these types of refractories simultaneously with the application of a low compressive load, the closure of previously formed microcracks (self-healing) was considered to be mainly responsible for their mechanical behavior.
引用
收藏
页码:3769 / 3781
页数:13
相关论文
共 50 条
  • [31] The effect of B4C and CaB6 additions in MgO-C bricks
    Hunold, K
    Ollig, M
    Potschke, J
    Rymon-Lipinski, T
    UNIFIED INTERNATIONAL TECHNICAL CONFERENCE ON REFRACTORIES (UNITECR 97), VOL 1 - 3: 5TH BIENNIAL WORLDWIDE CONGRESS - REFRACTORIES, A WORLDWIDE TECHNOLOGY, 1997, : 789 - 797
  • [32] Synthesis of chemically bonded porous ceramics from MgO-C refractory bricks waste
    Luza, A. L.
    Simao, L.
    Acordi, J.
    Raupp-Pereira, F.
    Innocentini, M. D. M.
    Montedo, O. R. K.
    CERAMICS INTERNATIONAL, 2022, 48 (03) : 3426 - 3434
  • [33] Degradation Kinetics of MgO-C Refractory at High Temperature
    Juhun Lee
    Jaewoo Myung
    Yongsug Chung
    Metallurgical and Materials Transactions B, 2021, 52 : 1179 - 1185
  • [34] INFLUENCE OF HEAT-TREATMENT CONDITIONS ON THE PROPERTIES OF MGO-C BRICKS CONTAINING ALUMINUM
    HAYASHI, S
    TAKAHASHI, H
    WATANABE, A
    OSAKA, A
    MIURA, Y
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1994, 102 (05): : 476 - 481
  • [35] Effects of resin and graphite content on density and oxidation behavior of MgO-C refractory bricks
    Hashemi, B
    Nemati, ZA
    Faghihi-Sani, MA
    CERAMICS INTERNATIONAL, 2006, 32 (03) : 313 - 319
  • [36] Resin-bonded MgO-C bricks for the refractory lining of metallurgical vessels.
    Bartha, P
    Weibel, G
    STAHL UND EISEN, 1997, 117 (01): : 75 - +
  • [37] Phase formation in MgO-C refractories with different antioxidants
    Atzenhofer, C.
    Harmuth, H.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (14) : 7330 - 7338
  • [38] Degradation Kinetics of MgO-C Refractory at High Temperature
    Lee, Juhun
    Myung, Jaewoo
    Chung, Yongsug
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2021, 52 (03): : 1179 - 1185
  • [39] Oxidation behaviors of MgO-C refractories with different Si/SiC ratio in the 1100-1500 °C range
    Xiao, Junli
    Chen, Junfeng
    Wei, Yaowu
    Zhang, Yu
    Zhang, Shaowei
    Li, Nan
    CERAMICS INTERNATIONAL, 2019, 45 (17) : 21099 - 21107
  • [40] Change of physical properties of unburned MgO-C bricks under various heating conditions
    Uchida, Shigeki
    Ichikawa, Kenji
    Yamamura, Takashi
    Nakamura, Ryosuke
    Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan, 1996, 104 (1212): : 723 - 728