Stress Corrosion Cracking Susceptibility of 316LN Grade Stainless Steel Weld Joint in Boiling Magnesium Chloride Hexahydrate Environment

被引:6
|
作者
Rajasekaran, R. [1 ]
Lakshminarayanan, A. K. [2 ]
Vasudevan, M. [3 ]
Raja, P. Vasantha [4 ]
机构
[1] Sri Sivasubramaniya Nadar Coll Engn, Dept Mech Engn, Chennai 603103, Tamil Nadu, India
[2] Sri Sivasubramaniya Nadar Coll Engn, Dept Mech Engn, Chennai 603110, Tamil Nadu, India
[3] Indira Gandhi Ctr Atom Res IGCAR, Mat Dev & Technol Div, Chennai 603102, Tamil Nadu, India
[4] Indira Gandhi Ctr Atom Res IGCAR, Adv Welding & Modelling Sect, Chennai 603102, Tamil Nadu, India
关键词
Stress corrosion cracking; 316LN austenitic stainless steel; Boiling MgCl(2 center dot)6H(2)O; Corrosion elongation curve; Transmission Electron Microscopy; Fractography; Dissolution of delta-ferrite; ALLOY; 600; PITTING CORROSION; FAILURE ANALYSIS; STRAIN-RATE; BEHAVIOR; 304-STAINLESS-STEEL; RESISTANCE; HYDROGEN; MICROSTRUCTURE;
D O I
10.1007/s12540-021-01162-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 316LN Stainless Steel (SS) weld joints were fabricated using Tungsten Inert Gas (TIG) Welding and Activated Flux Tungsten Inert Gas (A-TIG) Welding techniques with suitable process parameters. Initially, basic mechanical properties were evaluated across weld joints. Further microstructural study of the base metal, TIG, and A-TIG joints were accomplished using Optical Microscopy (OM), Transmission Electron Microscopy (TEM), and Scanning Electron Microscopy (SEM) techniques. The microstructural characterization revealed higher grain size variations at the fusion zone of the A-TIG joint due to the slow cooling rate and reversed Marangoni convection effect. The Stress Corrosion Cracking (SCC) susceptibility of the TIG and A-TIG welded joints was assessed using five different loading/Stress conditions. The constant load boiling 45 wt% Magnesium Chloride Hexahydrate (MgCl(2 center dot)6H(2)O) solution as per ASTM G36-94 standard was used to evaluate the SCC susceptibility of the welded joints. The SCC (crack initiation and propagation) of the base metal and welded joints occurred by the anodic dissolution and Hydrogen Induced Cracking mechanisms. For the welded joints additionally, the dissolution of the delta-ferrite increased the crack growth rate. The A-TIG joint exhibited lesser SCC resistance than the TIG joint for the following major reasons: (i) Formation of the large dendrites (ii) Presence of the higher grain size variations at the fusion zone. Moreover, both welded joints showed lesser SCC resistance than the base metal due to the dissolution of the delta-ferrite and the residual stress formation. The fractographic studies for the base metal, TIG, and A-TIG joints revealed the brittle nature of transgranular SCC failure.
引用
收藏
页码:2778 / 2797
页数:20
相关论文
共 50 条
  • [31] Effect of welding processes on the residual stress and distortion in type 316LN stainless steel weld joints
    Vasantharaja, P.
    Vasudevan, M.
    Palanichamy, P.
    JOURNAL OF MANUFACTURING PROCESSES, 2015, 19 : 187 - 193
  • [32] STRESS-CORROSION CRACKING SUSCEPTIBILITY OF AISI-316-NG AND 316 STAINLESS-STEEL IN AN IMPURITY ENVIRONMENT
    MAIYA, PS
    SHACK, WJ
    CORROSION, 1985, 41 (11) : 630 - 634
  • [33] Cracking initiation mechanism of 316LN stainless steel in the process of the hot deformation
    Zhang, Xiuzhi
    Zhang, Yishuai
    Li, Yingjie
    Liu, Jiansheng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 559 : 301 - 306
  • [34] Stress corrosion cracking mechanism of AISI 316LN stainless steel rebars in chloride contaminated concrete pore solution using the slow strain rate technique
    Martin, U.
    Ress, J.
    Bosch, J.
    Bastidas, D. M.
    ELECTROCHIMICA ACTA, 2020, 335
  • [35] Localized creep characterization of 316LN stainless steel weld joint using Small Punch Creep test
    Kumar, J. Ganesh
    Laha, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 705 : 72 - 78
  • [36] Isothermal and thermomechanical fatigue behaviour of type 316LN austenitic stainless steel base metal and weld joint
    Kumar, T. Suresh
    Yadav, S. D.
    Nagesha, A.
    Kannan, R.
    Reddy, G. V. Prasad
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 772
  • [37] Effects of thiosulfate on susceptibility of type 316 stainless steel to stress corrosion cracking in 3.5% aqueous sodium chloride
    Ashour, EA
    Meguid, EAA
    Ateya, BG
    CORROSION, 1997, 53 (08) : 612 - 616
  • [38] Clustering and ordering of nitrogen in nuclear grade 316LN austenitic stainless steel
    Shankar, P
    Sundararaman, D
    Ranganathan, S
    JOURNAL OF NUCLEAR MATERIALS, 1998, 254 (01) : 1 - 8
  • [39] The stress corrosion cracking behavior of austenitic stainless steels in boiling magnesium chloride solutions
    Alyousif, Osama M.
    Nishimura, Rokuro
    CORROSION SCIENCE, 2007, 49 (07) : 3040 - 3051
  • [40] DYNAMIC AND POSTDEFORMATION RECRYSTALLIZATION OF NUCLEAR-GRADE 316LN STAINLESS STEEL
    Zhang, R. H.
    Wang, Z. H.
    Shi, Z. P.
    Wang, B.
    Fu, W. T.
    STRENGTH OF MATERIALS, 2015, 47 (01) : 94 - 99