Influence of surface treatments on bond strength of metal and ceramic brackets to a novel CAD/CAM hybrid ceramic material

被引:43
|
作者
Elsaka, Shaymaa E. [1 ,2 ]
机构
[1] Mansoura Univ, Fac Dent, Dept Dent Biomat, Mansoura 35516, Egypt
[2] Al Farabi Coll Dent & Nursing, Dept Restorat Dent Sci, Jeddah, Saudi Arabia
关键词
Hybrid ceramic; Orthodontic brackets; Shear bond strength; Surface treatments; ORTHODONTIC BRACKETS; CONDITIONING METHODS; PORCELAIN SURFACES; DENTAL CERAMICS; STAINLESS-STEEL; IN-VITRO; CEMENT; ENAMEL;
D O I
10.1007/s10266-014-0188-8
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This study evaluated the effect of four different surface treatments methods on the shear bond strength (SBS) of ceramic and metal brackets to Vita Enamic (VE) CAD/CAM hybrid ceramic. A total of 240 plates (10 mm x 10 mm x 3 mm) were cut from VE ceramic blocks and divided into two groups. In each group, four subgroups were prepared by hydrofluoric acid (HF); phosphoric acid (H3PO4); diamond ceramic grinding bur; and silica coating using CoJet system (CJ). Maxillary central incisor metal (Victory Series) and ceramic (Clarity) brackets were bonded with light-cure composite and then stored in artificial saliva for 1 week and thermocycled. The SBS test was performed, and the failure types were classified with adhesive remnant index scores. Surface morphology of the ceramic was characterized after treatment using a scanning electron microscope. Data were analyzed using two-way ANOVA, Tukey HSD test, and Weibull analysis. SBS was significantly affected by the type of bracket and by type of treatment (P < 0.001). Specimens treated with CJ presented with significantly higher SBS compared to other groups (P < 0.05). Improvements in SBS values (MPa) were found in the following order: CJ > HF > Bur > H3PO4. Ceramic bracket showed higher SBS compared to metal bracket. Adhesive failures between the ceramic and composite resin were the predominant mode of failure in all groups. Surface treatment of VE CAD/CAM hybrid ceramic with silica coating enhanced the adhesion with ceramic and metal brackets.
引用
收藏
页码:68 / 76
页数:9
相关论文
共 50 条
  • [31] Bond strength of ceramic or resin CAD-CAM laminate veneers
    Bakir, Metin
    Bakir, Sehmus
    Bahsi, Emrullah
    AMERICAN JOURNAL OF DENTISTRY, 2020, 33 (06): : 287 - 290
  • [32] Effect of surface treatments on the bond strength of resin-repaired resin matrix CAD-CAM ceramic: A scoping review
    Albergardi, Ana Beatriz de Souza
    Limirio, Joao Pedro Justino de Oliveira
    Gomes, Jessica Marcela de Luna
    Pesqueira, Aldieris Alves
    Pellizzer, Eduardo Piza
    JOURNAL OF DENTISTRY, 2025, 154
  • [33] Effect of Different Surface Treatments on the Bond Strength of the Hybrid Ceramic Characterization Layer
    Vieira Grangeiro, Manasses Tercio
    Rossi, Natalia Rivoli
    Lopes Barreto, Larissa Araujo
    Bottino, Marco Antonio
    Mendes Tribst, Joao Paulo
    JOURNAL OF ADHESIVE DENTISTRY, 2021, 23 (05): : 429 - 435
  • [34] Effects of different etching methods and bonding procedures on shear bond strength of orthodontic metal brackets applied to different CAD/CAM ceramic materials
    Buyuk, S. Kutalmis
    Kucukekenci, Ahmet Serkan
    ANGLE ORTHODONTIST, 2018, 88 (02) : 221 - 226
  • [35] The Effects of Er,Cr:YSGG laser on shear bond strength of orthodontic lingual brackets to CAD/CAM ceramic systems
    Kaygisiz, Emine
    Egilmez, Ferhan
    Ergun, Guelfem
    Yuksel, Sema
    Nagas, Isil Cekic
    EUROPEAN ORAL RESEARCH, 2023, 57 (03) : 122 - 127
  • [36] Effect of a single-component ceramic conditioner on shear bond strength of precoated brackets to different CAD/CAM materials
    Gonzalez-Serrano, Carlos
    Phark, Jin-Ho
    Fuentes, Maria Victoria
    Albaladejo, Alberto
    Sanchez-Monescillo, Andres
    Duarte, Sillas, Jr.
    Ceballos, Laura
    CLINICAL ORAL INVESTIGATIONS, 2021, 25 (04) : 1953 - 1965
  • [37] Effect of a single-component ceramic conditioner on shear bond strength of precoated brackets to different CAD/CAM materials
    Carlos González-Serrano
    Jin-Ho Phark
    María Victoria Fuentes
    Alberto Albaladejo
    Andrés Sánchez-Monescillo
    Sillas Duarte
    Laura Ceballos
    Clinical Oral Investigations, 2021, 25 : 1953 - 1965
  • [38] Factors affecting the shear bond strength of metal and ceramic brackets bonded to different ceramic surfaces
    Abu Alhaija, Elham S. J.
    Abu AlReesh, Issam A.
    AlWahadni, Ahed M. S.
    EUROPEAN JOURNAL OF ORTHODONTICS, 2010, 32 (03) : 274 - 280
  • [39] The Influence of Ceramic Surface Treatments on the Microtensile Bond Strength of Resin Cements to Y-TZP Ceramic
    朴美姬
    朴珠美
    Seung-Geun Ahn
    Kwang-Yeob Song
    Tae-Sung Bae
    Jae-Youn Jung
    Journal of Wuhan University of Technology(Materials Science), 2010, 25 (06) : 996 - 1000
  • [40] The influence of ceramic surface treatments on the microtensile bond strength of resin cements to Y-TZP ceramic
    Park Mi-Hee
    Ju-Mi Park
    Seung-Geun Ahn
    Kwang-Yeob Song
    Tae-Sung Bae
    Jae-Youn Jung
    Wang Xinyu
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2010, 25 : 996 - 1000