Leaching of Spent Ni-Mo Hydrodesulphurization (HDS) Catalyst in Oxalic Acid Solutions

被引:5
|
作者
Ilhan, Sedat [1 ]
机构
[1] Istanbul Univ, Fac Engn, Dept Met & Mat Engn, TR-34320 Istanbul, Turkey
关键词
Leaching; Hydrodesulphurization catalyst; Mo recovery; Ni recovery; MOLYBDENUM; RECOVERY; EXTRACTION; ALUMINUM; COBALT;
D O I
10.1007/978-3-319-52132-9_56
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
In this work, the effect of crushing, temperature, oxalic acid concentration and stirring speed on the leaching of spent Ni-Mo HDS catalyst was investigated. Spent Ni-Mo HDS catalyst was roasted at 500 degrees C under dynamic air atmosphere for 4 h prior to leaching experiments. It was found that roasted spent Ni-Mo HDS catalyst included mainly Al2O3, MoO3, NiMoO4 and AlPO4. Leaching experiments were performed using 5 g of uncrushed roasted Ni-Mo HDS catalyst, 1 L of 0.25, 0.50, 0.75 and 1 M H2C2O4 solutions, 25, 40, 55 and 70 degrees C temperatures and 200, 250 and 300 rpm stirring speeds. Leaching behavior of Mo, Al, P and Ni was determined. It is seen that H2C2O4 can be used successfully for the leaching of roasted HDS catalyst. More than 90% of the molybdenum and 80% of Nickel is extracted from the experiments carried out using 300 rpm stirring speed, 1 M H2C2O4 and 40 degrees C.
引用
收藏
页码:557 / 564
页数:8
相关论文
共 50 条
  • [21] Metal recovery from spent Ni-Mo-V hydrodesulphurisation catalyst in oxalic acid media by mechanochemical treatment
    Zoraga, Mert
    CANADIAN METALLURGICAL QUARTERLY, 2024, 63 (03) : 882 - 891
  • [22] Extraction of Molybdenum from Spent HDS Catalyst by Pressure Alkaline Leaching
    Shijie Zhao
    Zhiqin Liao
    Yu Xie
    Xisong Li
    Yanyang Dai
    Zhirong Li
    Mingyu Wang
    Journal of Sustainable Metallurgy, 2021, 7 : 773 - 782
  • [23] Extraction of Molybdenum from Spent HDS Catalyst by Pressure Alkaline Leaching
    Zhao, Shijie
    Liao, Zhiqin
    Xie, Yu
    Li, Xisong
    Dai, Yanyang
    Li, Zhirong
    Wang, Mingyu
    JOURNAL OF SUSTAINABLE METALLURGY, 2021, 7 (03) : 773 - 782
  • [24] Recovery of Mo, V and Ni from spent catalyst using leaching and solvent extraction
    Pradhan, Debabrata
    Pattanaik, Archana
    Samal, D. P. Krishna
    Sukla, Lala Behari
    Kim, Dong Jin
    MATERIALS TODAY-PROCEEDINGS, 2020, 30 : 322 - 325
  • [25] Selective Leaching of Valuable Metals from Spent Fluid Catalytic Cracking Catalyst with Oxalic Acid
    Zheng, Dalong
    Zhang, Yimin
    Liu, Tao
    Huang, Jing
    Cai, Zhenlei
    Zhang, Ruobing
    MINERALS, 2022, 12 (06)
  • [26] Platinum Recovery from Spent CCR Platforming Catalyst with Oxalic Acid and Aqua Regia Leaching
    Yuliusman
    Prawira, L. P. D., I
    Nafisah, A. R.
    Amananti, K. S.
    Ayu, M. P.
    Isa, M.
    3RD INTERNATIONAL CONFERENCE ON ENGINEERING TECHNOLOGY FOR SUSTAINABLE DEVELOPMENT (ICET4SD), 2020, 722
  • [27] Recovery of lanthanum from acid leaching solutions of spent cracking catalyst
    Martsul', V. N.
    Kozlowskaya, I. Yu.
    RUSSIAN JOURNAL OF APPLIED CHEMISTRY, 2015, 88 (10) : 1589 - 1593
  • [28] Recovery of lanthanum from acid leaching solutions of spent cracking catalyst
    V. N. Martsul’
    I. Yu. Kozlowskaya
    Russian Journal of Applied Chemistry, 2015, 88 : 1589 - 1593
  • [29] REACTIVITY AND MORPHOLOGY OF Ni, Mo, AND Ni-Mo OXIDE CLUSTERS SUPPORTED ON MCM-48 TOWARD THIOPHENE HYDRODESULPHURIZATION
    Bartholomew, Catherine
    Chakradhar, Ashish
    Burghaus, Uwe
    Wu, Chia-Ming
    Peng, Rui
    Mishra, Srujan
    Koodali, Ranjit T.
    SURFACE REVIEW AND LETTERS, 2014, 21 (05)
  • [30] Ni-Mo catalyst synthesized by mechanical alloying
    Sosa, M
    Estrada-Guel, I
    Alonso, G
    Ornelas, C
    De la Torre, SD
    Martínez-Sánchez, R
    METASTABLE, MECHANICALLY ALLOYED AND NANOCRYSTALLINE MATERIALS, 2003, : 745 - 750