PROPERTY OF 9CR-3W-3CO-ND-B HEAT-RESISTANT STEEL SAVE12AD WELDED JOINT

被引:0
|
作者
Kurihara, Shinnosuke [1 ]
Osuki, Takahiro [1 ]
Hamaguchi, Tomoaki [1 ]
Semba, Hiroyuki [1 ]
Okada, Hirokazu [1 ]
Hirata, Hiroyuki [2 ]
Yoshizawa, Mitsuru [3 ]
机构
[1] Nippon Steel & Sumitomo Met Corp, Amagasaki, Hyogo, Japan
[2] Nippon Steel & Sumitomo Met Corp, Futtsu, Chiba, Japan
[3] Nippon Steel & Sumitomo Met Corp, Dusseldorf, Germany
来源
ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE EIGHTH INTERNATIONAL CONFERENCE, 2016 | 2016年
关键词
CREEP DEFORMATION; MOD.9CR-1MO STEEL;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Developed 9Cr-3W-3Co-Nd-B heat-resistant steel SAVE12AD (Recently designated as ASME Grade 93) pipes and tubes have higher creep strength in both base metal and welded joints than conventional high Cr ferritic steels such as ASME Grades 91, 92 and 122. The welded joints of SAVEI2AD tubes with commercial filler wire for W62-10CMWV-Co (Gr. 92) or Ni base filler wire ERNiCr-3 (Alloy82) also have much better creep rupture strength than those of conventional steels because of suppression of refining in the Heat-Affected-Zone (HAZ). However, the creep rupture strength of weld metal of W62-10CMWV-Co was marginal. Additionally, the hot cracking susceptibility of weld metal using Ni base filler wire ERNiCr-3 was occasionally below the required level. Similar welding consumable for SAVE12AD has been developed to solve these problems. Optimization of nickel, neodymium and boron contents on similar welding consumable enables to obtain both the good long-term creep rupture strength and low enough hot cracking susceptibility of weld metal. Consequently, SAVEI2AD welded joint is expected to be applied of piping and tubing above 600 degrees C in USC power plants because of its good properties with similar welding consumable.
引用
收藏
页码:931 / 938
页数:8
相关论文
共 50 条
  • [41] On Laves phase in a 9Cr3W3CoB martensitic heat resistant steel when aged at high temperatures
    Liang, Ye
    Yan, Wei
    Shi, Xianbo
    Li, Yanfen
    Shi, Quanqiang
    Wang, Wei
    Shan, Yiyin
    Yang, Ke
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 85 : 129 - 140
  • [42] Air and wet air oxidation of 9Cr-3Co-3W creep resistant ferritic steel at 650 °C
    Tang, S.
    Tang, X.
    Xiang, Z. D.
    ADVANCES IN CHEMICAL, MATERIAL AND METALLURGICAL ENGINEERING, PTS 1-5, 2013, 634-638 : 1685 - 1689
  • [43] Precipitates and Particles Coarsening of 9Cr–1.7W–0.4Mo–Co Ferritic Heat-Resistant Steel after Isothermal Aging
    Qiuzhi Gao
    Yanan Zhang
    Hailian Zhang
    Huijun Li
    Fu Qu
    Jian Han
    Cheng Lu
    Bintao Wu
    Yao Lu
    Yan Ma
    Scientific Reports, 7
  • [44] Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions
    Yan, Peng
    Liu, Zhengdong
    Bao, Hansheng
    Weng, Yuqing
    Liu, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 588 : 22 - 28
  • [45] Effect of aging temperature on the microstructures and mechanical properties of ZG12Cr9Mo1Co1NiVNbNB ferritic heat-resistant steel
    Xue Yang
    Lan Sun
    Ji Xiong
    Ping Zhou
    Hong-yuan Fan
    Jian-yong Liu
    InternationalJournalofMineralsMetallurgyandMaterials, 2016, 23 (02) : 168 - 175
  • [46] Effect of aging temperature on the microstructures and mechanical properties of ZG12Cr9Mo1Co1NiVNbNB ferritic heat-resistant steel
    Xue Yang
    Lan Sun
    Ji Xiong
    Ping Zhou
    Hong-yuan Fan
    Jian-yong Liu
    International Journal of Minerals, Metallurgy, and Materials, 2016, 23 : 168 - 175
  • [47] Effect of aging temperature on the microstructures and mechanical properties of ZG12Cr9Mo1Co1NiVNbNB ferritic heat-resistant steel
    Yang, Xue
    Sun, Lan
    Xiong, Ji
    Zhou, Ping
    Fan, Hong-yuan
    Liu, Jian-yong
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2016, 23 (02) : 168 - 175
  • [48] 650°C Long-Term Structure Stability Study on 18Cr-9Ni-3CuNbN Heat-Resistant Steel
    Yu, Hongyao
    Dong, Jianxin
    Xie, Xishan
    PRICM 7, PTS 1-3, 2010, 654-656 : 118 - +
  • [49] Study of early corrosion behavior for 12Cr1MoV heat-resistant steel in solution with NaHCO3 by electrochemical noise
    Tian, Zhi-Qiang
    Kong, Xiao-Dong
    Wu, Gang
    Wang, Yuan-Sheng
    Cailiao Gongcheng/Journal of Materials Engineering, 2011, (08): : 8 - 13
  • [50] Field studies of steam oxidation behavior of austenitic heat-resistant steel 10Cr18Ni9Cu3NbN
    Liang, Zhiyuan
    Zhao, Qinxin
    Singh, Preet M.
    Wang, Yungang
    Li, Yuxin
    Wang, Yushu
    ENGINEERING FAILURE ANALYSIS, 2015, 53 : 132 - 137