Influence of Er;Cr:YSGG Laser on Shear Bond Strength and Color Stability of Lithium Disilicate Ceramics: An In Vitro Study

被引:35
|
作者
Vohra, Fahim [1 ]
Labban, Nawaf [2 ]
Al-Hussaini, Abeer [3 ]
Al-Jarboua, Maha [3 ]
Zawawi, Rahaf [3 ]
Alrahlah, Ali [4 ]
Naseem, Mustafa [5 ]
机构
[1] King Saud Univ, Dept Prosthet Dent Sci, Coll Dent, Eng Abdullah Bugshan Res Chair Dent & Oral Rehabi, Riyadh 11545, Saudi Arabia
[2] King Saud Univ, Dept Prosthet Dent Sci, Coll Dent, Riyadh, Saudi Arabia
[3] King Saud Univ, Coll Dent, Riyadh, Saudi Arabia
[4] King Saud Univ, Coll Dent, Dept Restorat Dent Sci, Eng Abdullah Bugshan Res Chair Dent & Oral Rehabi, Riyadh, Saudi Arabia
[5] Dar Al Uloom Univ, Dept Prevent Dent Sci, Riyadh, Saudi Arabia
关键词
Er; Cr:YSGG laser; lithium disilicate; ceramic; shear bond strength; color stability; ER; CR-YSGG LASER; COMPOSITE; ACID; RESTORATIONS; RESISTANCE; ADHESIVE; CEMENT;
D O I
10.1089/photob.2018.4582
中图分类号
R61 [外科手术学];
学科分类号
摘要
Objective: The aim of this study was to assess the effect of Er;Cr:YSGG laser parameters (power and frequency) on the bond strength and color stability of lithium disilicate (LD) ceramics. Materials and methods: One hundred ten specimens of LD ceramic were fabricated following heat pressed technique. Fifty disks were randomly distributed into five groups according to types of surface treatment [hydrofluoric (HF) acid, L1S L2S, L1D, and L2D]. For all laser-treated groups, bond preparation settings were used with a gold hand piece using a MZ10 tip (Er;Cr:YSGG, water lase I plus; Biolase). After surface treatment, adhesive bond was applied, and after photopolymerization, a composite buildup was performed. To evaluate shear bond strength, a controlled force was applied until failure using a universal testing machine. Color stability was assessed for six groups (HF, L1S L2S, L1D, L2D, and control) of LD ceramic (shade A1, LT translucency) through the CIE L*a*b* system. Three specimens from each of the six groups were selected randomly for assessment of surface topography using scanning electron microscopy. Means and standard deviations were compared using analysis of variance and Tukey's post hoc test (p<0.05). Results: The maximum and minimum mean bond strength were shown by the L2D group 19.951.014 and L1S group specimens 14.68 +/- 0.863, respectively. Highest mean Delta E was found in L2S group 8.17 +/- 2.10 and the lowest mean Delta E was found in control group (no treatment) 0.11 +/- 0.05. Conclusions: LD specimens lased (Er;Cr:YSGG) with 3.75 W power and 15Hz frequency for 4min showed bond strength comparable with HF acid samples, and color changes within acceptable range (Delta E 1.17). Laser treatment (Er;Cr:YSGG) at 3.75 W power and 15Hz frequency for 4min of LD ceramics appears to be clinically efficient, showing acceptable bond strength and color stability.
引用
收藏
页码:483 / 488
页数:6
相关论文
共 50 条
  • [41] Acid-etch interval and shear bond strength of Er,Cr:YSGG laser-prepared enamel and dentin
    Ali Obeidi
    Perng-Ru Liu
    Lance C. Ramp
    Preston Beck
    Norbert Gutknecht
    Lasers in Medical Science, 2010, 25 : 363 - 369
  • [42] Acid-etch interval and shear bond strength of Er,Cr:YSGG laser-prepared enamel and dentin
    Obeidi, Ali
    Liu, Perng-Ru
    Ramp, Lance C.
    Beck, Preston
    Gutknecht, Norbert
    LASERS IN MEDICAL SCIENCE, 2010, 25 (03) : 363 - 369
  • [43] CORRELATION OF ROUGHNESS AND MICROSHEAR BOND STRENGTH OF Er,Cr:YSGG LASER IRRADIATION ON ZIRCONIA
    Oliveira, Pedro
    Zeidan, Leonardo
    Barroso, Juliana
    Rodrigues, Jose
    Roulet, Jean
    Cassoni, Alessandra
    LASERS IN SURGERY AND MEDICINE, 2016, 48 (04) : 431 - 431
  • [44] Shear bond strength of metallic brackets bonded to enamel pretreated with Er,Cr:YSGG LASER and CPP-ACP
    Yomna A. Nabawy
    Tarek N. Yousry
    Nadia M. El-Harouni
    BMC Oral Health, 21
  • [45] Shear bond strength of composite resin to dentin after Er, Cr: YSGG laser irradiation or phosphoric acid etching
    Saja Qasim Salman
    Basima Mohammed Ali Hussein
    Lasers in Dental Science, 8 (1)
  • [46] Bond strength of porcelain to acid or er,cr:ysgg laser etched enamel.
    Usumez, A
    Aykent, F
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : 476 - 476
  • [47] Effects of Er,Cr:YSGG Laser Parameters on Dentin Bond Strength and Interface Morphology
    Ayar, Muhammet Kerim
    Yildirim, Tahsin
    Yesilyurt, Cemel
    MICROSCOPY RESEARCH AND TECHNIQUE, 2015, 78 (12) : 1104 - 1111
  • [48] Effect of acid etching, Er, Cr: YSGG laser conditioning and combining on shear bond strength of orthodontic metal bracket
    Roshan A.
    Hosseini N.
    Lasers in Dental Science, 2019, 3 (4) : 235 - 239
  • [49] The effects of disinfection with Er, Cr:YSGG laser, application of CPP-ACP and sodium hypochlorite on shear bond strength
    Ersan, Z.
    Yazicioglu, I
    Serin, A.
    Dogan, M.
    NIGERIAN JOURNAL OF CLINICAL PRACTICE, 2022, 25 (12) : 1949 - 1954
  • [50] Bond strength of composite resin to enamel and dentin prepared with Er,Cr:YSGG laser
    Takada, Mayo
    Shinkai, Koichi
    Kato, Chikage
    Suzuki, Masaya
    DENTAL MATERIALS JOURNAL, 2015, 34 (06) : 863 - 871